Background: This clinical trial aims to evaluate the color changes of direct resin composite veneer (DCV) restorations based on spectrophotometric analysis of 4 different types of resin composites between the baseline immediately after polishing and after one year of follow-up. Materials and methods: 28 patients were assessed for eligibility for participation, aged between 18 and 38 years old, who indicated for DCV restorations in anterior maxillary teeth were considered for participation in this study. In total, 25 patients who met the inclusion criteria were selected (6 males and 19 females, mean age: 20.9 at the time of restoration placement), and 3 patients were excluded. Participants were divided into four groups based on the type of composite resin used for restorations. Group 1 nanohybrid Ips Empress direct (Ivoclar Vivadent)](IPS) (13 restorations/6 patients), group 2 microfilled [Essentia (GC cooperation Japan)](ES) (14 restorations / 7 patients), group 3 supra-nano filled [ Estelite ∑ Quick (Tokuyama, Tokyo, Japan)](EQ) (17 restorations / 7 patients) and group 4 nanofill [Filtek Ultimate (3M ESPE)](FU) (13 restorations / 5 patients). Baseline Color measurements were performed with a spectrophotometer immediately after finishing and polishing (baseline), and after one year of recall, color change (ΔE) from baseline values and after one year of follow-up of DCVs were calculated according to CIELab color coordinates. For this, a silicone mold was fabricated for each patient and used as a guide for each measurement to standardize the site of the readings. Statistical analysis of the data was applied using the Kruskal-Wallis test with Dunn-Bonferroni posthoc test after controlling the distribution of data in terms of normality with the Shapiro Wilk test. Results: At the end of one year,25 participants(57restorations) were followed up. The mean ΔE of IPS, EQ, and FU composites were higher than the ES composite resin, but there was no statically significant difference between all types of composites (P> 0.05). There was no statistically significant difference in the mean ΔL* between any types of composite resin (p> 0.05). There was a significant change in Δa* and Δb* after a one-year recall for all the types of DCV restorations (p < 0.05). Conclusion: After one year of follow-up, the spectrophotometer measurements of direct resin composite veneer restorations, it was concluded no difference between the mean ΔE of ES, IPS, FU, and EQ resin composite. ES (Microfilled hybrid) showed a lower mean ΔE value compared to the other groups. All groups of resin composite showed color changes within clinically acceptable levels after a one-year follow-up.
Origanum majorana (Majorana hortensis), an evergreen herbaceous plant belonging to the Lamiaceae family, has been well known for being used for gastrointestinal, cardiac, respiratory, rheumatologic and many other illnesses, but in wounds management hasn’t been qualified scientifically yet. The goal of the study was to evaluate the wound healing properties of sterols in n-hexane and phenols in ethyl acetate extract fractions of the Iraqi Origanum majorana L aerial parts by contrasting their wound healing abilities with those of commercially available MEBO ointment in a rat excised wound repair model. At various periods, the size of the wounds was measured and skin tissue samples were taken for histopathology. When compared to positive and
... Show More98 samples were collected from various clinical sources included (Burns, wounds, urines, sputums, blood) From the city of Baghdad, After performing the biochemical and microscopic examination, 52 isolates were obtained for Pseudomonas aeruginosa, 17 (32.7%) isolates from burn infection, 12 (23%) isolates from Wound infection 11 (21.2%) isolates from urine infection, 7 (13.5%) isolates of sputum and 5 (9.6%) isolates from blood. Bacteria susceptibility to form biofilm has been detectedby microtiter plate method, The results showed that 80% of the bacterial isolates were produced the biofilm with different proportions, alg D gene (alginate production) has been detected by polymerase chain reaction (PCR) Which plays an essential role in the fo
... Show MoreThe nanostructured Manganese dioxide/Carbon fiber (CF) composite electrode was prepared galvanostatically using a facile method of anodic electrodeposition by varying the reaction time and MnSO4 concentration of the electrochemical solution. The effects of these parameters on the structures and properties of the prepared electrode were evaluated. For determining the crystal characteristics, morphologies, and topographies of the deposited MnO2 films onto the surfaces of carbon fibers, the X-ray diffraction (XRD), field emission scanning electron microscopy (FESEM), and atomic force microscopy (AFM) techniques were used, respectively. It found that the carbon fibers were coated with γ-MnO2 with a density that increased with increasing the de
... Show MoreComposite steel-concrete sections have a broad benefit through increasing structural strength as well as minimizing the self-loads. All past researches were concerned with pre-installed shear connectors (PRSC) in the manufacturing of composite sections. A new fabrication technique for steel-concrete-steel composite sections were presented in the current study by the post-installation shear connectors (POSC) passed-through an embedded polymerizing vinyl chloride (PVC) pipes. The performance of normal strength concrete prisms with a specified strength of 32 MPa connected to square steel tubes (SST) was investigated. Six specimens were fabricated in both methodologies, PRSC and POSC were experimentally tested by Push-out test. The spac
... Show MoreCalcium-Montmorillonite (bentonite) [Ca-MMT] has been prepared via cation exchange reaction using benzalkonium chloride [quaternary ammonium] as a surfactant to produce organoclay which is used to prepare polymer composites. Functionalization of this filler surface is very important factor for achieving good interaction between filler and polymer matrix. Basal spacing and functional groups identification of this organoclay were characterized using X-Ray Diffraction (XRD) and Fourier Transform Infrared (FTIR) spectroscopy respectively. The (XRD) results showed that the basal spacing of the treated clay (organoclay) with the benzalkonium chloride increased to 15.17213 0A, this represents an increment of about 77.9% in the
... Show MorePVC/Kaolinite composites were prepared by the melt intercalation method. Mechanical properties, thermal properties, flammability and water absorption percentage of prepared samples were tested. Mechanical characteristic such as tensile strength, elongation at break; hardness and impact strength (charpy type) were measured for all samples. It was found that the tensile strength and elongation at break of PVC composites decreased with increasing kaolinite loading. Also, the hardness of the composites increases with increase in filler content .The impact strength of the composites at the beginning increases at lower kaolinite loadings is due to the lack of kaolin adhesion to the matrix. However, at higher kaolin loadings. This severe agglom
... Show MoreLaser etching may be an alternative to acid etching of enamel and dentin. Several characteristics of irradiated dental hard tissues have been considered advantageous, microscopically rough surfaces without demineralization, open dentinal tubules without smear layer production and dentin surface sterilization. The aim of this study is to determine and compare histology the microleakage in class V cavity restored with a light cured composite after conditioning the samples(tooth surface) with 1-acid etching, 2-Q-switched Nd:YAG Laser etching and finally 3- acid and laser etching. Materials and methods: Twenty four non carious human extracted teeth were used in this study. The samples were equally grouped into four groups of six teeth each.
... Show More