Background: White spot lesion is the first visible sign of dental caries that is characterized by demineralized lesion underneath an intact surface. Several studies demonstrated that they could be treated using noninvasive techniques like the use of fluoride or casein phospho-peptide and amorphous calcium phosphate. Improvement in aesthetic outcomes by covering the demineralized enamel is one of the advantages of the use of resin infiltration and opal-ustre microabrasion, which are two new techniques that had been used for treatment of white spot lesion. The purpose of this study was to evaluate the impact of resin infiltration and microabrasion in the microhardness of the artificial white spot lesions at various depths. Material and method: Forty-eight artificially white spot lesions were divided into three groups (n=16) according to the depth of the lesion (shallow enamel, deep enamel, shallow dentine). Then, each of the main groups was divided into two subgroups (n = 8), the first group was treated with resin infiltration, while the second one was treated with Opalustre microabrasion. Assessment of the microhardness was done using Vickers hardness at the baseline, after demineralization (formation of the white spot lesion) and after the treatment with the resin infiltration and the microabrasion. Results: There was a significant difference in the microhardness of all the layers after demineralization. Although the hardness values that found among the icon group in the inner enamel and the outer dentine were higher than that of the opalustre, statistically there was no significant difference between the two mate-rials in all the layers of the white spot lesion. Conclusion: Microhardness values decrease as the depth of the white spot lesion increase. There was an increase in the microhardness values after the treatment with the resin infiltration and the microabrasion.
Background: This study was conducted to assess the effects of various beverages on the shear bond strength of light-cured orthodontic composite used to bond stainless steel orthodontic brackets on human teeth and to determine the site of bonding failure of this material. Materials and Methods: Fifty extracted human premolars were selected and randomly divided into five equal groups each with 10 teeth according to the beverage type (Control, One Tiger, Milk, Green tea and Coffee). After bonding, the teeth were immersed in specific beverages for 5 minutes twice daily with equal intervening intervals then washed and stored in distilled water at 37º C for the reminder of the day. The process was carried out for 30 days. The samples were then
... Show MoreBackground: The Initial (primary) stability is one of the factors that play an important role in the success of the dental implants. The purpose of this study was to evaluate the initial stability of dental implant with horizontal plate by using five analytical tests: insertion torque, removal torque, resonance frequency analysis, push-in test and pull-out test. Materials and methods: Two different lengths of dental implants (5mm and 10mm) were tested in this study; each dental implant was 4mm in diameter with a square threads shape of 1mm pitch and 0.5mm depth. The crestal area was 4.2mm diameter contained a right angle margin circumferential ring while the apical area was tapered with two self-tapping grooves. In this study, the initial s
... Show MoreBackground: This in vitro study was carried out to evaluate the effect of various endodontic irrigants (sodium hypochlorite, ethylene diaminetetracetic acid and normal saline) on sealing ability of (Biodentine, mineral trioxide aggregate, and amalgam) used to repair furcal perforations. Material and methods: One hundred and twenty extracted human molars with divergent roots were used in this study. A standard root canal access cavity was prepared in each tooth and furcal perforation was made and was standardized by using k file size 100 instrument to get a perforation of (1.32mm) in diameter .The teeth were randomly divided in to three groups of 40 teeth according to the type of material used to repair the perforations (Group A: The furcal
... Show MoreIntroduction: Articaine was developed in 1969, with reported advantages which are increased potency, increased duration of its anesthetic effect and superior diffusion through bony tissue. The effectiveness of using 4% articaine infiltration for extraction of mandibular molar teeth in comparison to 2% lidocaine inferior alveolar nerve block is not settled yet. Aim: The aim of this study was to evaluate the effectiveness of using 4% articaine infiltration for extraction of mandibular molars by comparing it to the use of 2% lidocaine inferior alveolar nerve block in terms of success, the volume of local anesthetic agents and the pain experienced during the procedure. Materials and methods: A prospective randomized controlled study included
... Show MoreBackground: Poly-ether-ether-ketone(PEEK) has been introduced to many dental fields. Recently it was tested as a retainer wire‎ following orthodontic treatment. This study aimed to investigate the effect of changing the bonding spot size and location on the performance of PEEK retainer wires. Methods: A biomechanical study involving four three-dimensional finite element models was performed. The basic model was with a 0.8 mm cylindrical cross-section PEEK wire, bonded at the center of the lingual surface of the mandibular incisors with 4 mm in diameter composite spots. Two other models were designed with 3 mm and 5 mm composite sizes. The last model was created with the composite bonding spot of the canine away from the center of t
... Show MoreBackground: Poly-ether-ether-ketone(PEEK) has been introduced to many dental fields. Recently it was tested as a retainer wire‎ following orthodontic treatment. This study aimed to investigate the effect of changing the bonding spot size and location on the performance of PEEK retainer wires. Methods: A biomechanical study involving four three-dimensional finite element models was performed. The basic model was with a 0.8 mm cylindrical cross-section PEEK wire, bonded at the center of the lingual surface of the mandibular incisors with 4 mm in diameter composite spots. Two other models were designed with 3 mm and 5 mm composite sizes. The last model was created with the composite bonding spot of the canine away from the center
... Show MoreThis research aims to clarify the importance of an accounting information system that uses artificial intelligence to detect earnings manipulation. The research problem stems from the widespread manipulation of earning in economic entities, especially at the local level, exacerbated by the high financial and administrative corruption rates in Iraq due to fraudulent accounting practices. Since earning manipulation involves intentional fraudulent acts, it is necessary to implement preventive measures to detect and deter such practices. The main hypothesis of the research assumes that an accounting information system based on artificial intelligence cannot effectively detect the manipulation of profits in Iraqi economic entities. The researche
... Show MoreA hand lay-up method was used to prepare Epoxy/ metal composites. Epoxy resin (EP) was used as a matrix with metal particles (Al, Cu, and Fe) as fillers.
The preparation method includes preparing square panels of composites with different weight percentage of fillers (10, 20, 30, 40, and 50%). Standard specimens (88mm in diameter) for thermal conductivity tests were prepared to measure thermal conductivity kexp.The result of experimental thermal conductivity kexp, for EP/metal composites show that, kexp increase with increasing weight percentage, For EP/ Al and EP/Cu composites, and it have have maximum values of 0.33 and 0.35 W/m.K, respectively. While kexp for EP/ Fe composite show slight increase with maximum value of 0.186 W/m.K.
EP/ metal composites were prepared as adhesives between two steel rods. Epoxy resin (EP) was used as a matrix with metal as fillers (Al, Cu, Fe,).
The preparation method for tensile adhesion tests includes two steel rods with adhesive composites between the rods to measure adhesion strength Sad and adhesion toughness Gad.
Results of tensile adhesion tests show that EP/ metals composite have maximum strength Sad for certain weight percentage of metals 2.95 and 9MPa at 10% for EP/Al and EP/Cu composite and 8.2MPa at 40% for EP/Fe composites