Background: Alginate impression material is the irreversible hydrocolloid material that is widely used in dentistry. The contact time between alginate and gypsum cast could have a detrimental effect on the properties of the gypsum cast. The objective of this study is to evaluate the impact of various contact time intervals of Alginate impressions & type III dental stone on surface properties of stone cast. Materials and Methods: Time intervals tested were 1hour, 6 hours and 9 hours. Surface properties of stone cast evaluated were surface detail reproduction, hardness and roughness. Surface detail reproduction was determined using cylindrical brass test block in accordance with ISO 1563. Surface roughness was measured by profilometer and hardness was measured by Durometer (Shore D). Results: The detail reproduction showed significant difference (P<0.05), at 6 hr., and 9 hr. showed better results. While surface roughness significantly decreased (p<0.01) with prolonged contact time. However, surface hardness increased significantly (p<0.01) with increased contact time. Conclusions: Surface detail reproduction increased with increasing the contact time and this was noticed at (6, 9 hours). However, 1hour time interval showed decreased surface detailed reproduction. Roughness decreased when the contact time was increased between type III dental stone and alginate impression whereas, hardness was improved significantly with increasing contact time.
In this paper, we used two monomers, 3,3',4,4'-benzophenone tetracarboxylic dianhydride (BTDA) and m,m'-diaminobenzophenone (m, m’-DABP), to produce polyamide acid and then converted it to polyimide (PI). The effects of phosphoric acid (H3PO4) molarity (1, 2, and 3 M) on the structural, thermal, mechanical, and electrical characteristics of the polyimides/polyaniline (PI/PANI) nanocomposites were studied. Two sharp reflection peaks were developed by the addition of PANI to PI. When 3 M H3PO4 is added, the crystalline sharp peak loses some of its intensity. The complex formation of PI/PANI-H3PO4 was confi
... Show MoreA polycrystalline PbxS1-x alloys with various Pb content ( 0.54 and 0.55) has been prepared successfully. The structure and composition of alloys are determined by X-ray diffraction (XRD), atomic absorption spectroscopy (AAS) and X-ray fluorescence (XRF) respectively. The X-ray diffraction results shows that the structure is polycrystalline with cubic structure, and there are strong peaks at the direction (200) and (111), the grain size varies between 20 and 82 nm. From AAS and XRF result, the concentrations of Pb content for these alloys were determined. The results show high accuracy and very close to the theoretical values. A photoconductive detector as a bulk has been fabricated by taking pieces of prepared alloys and polished chemic
... Show MoreThis study was conducted on the effect of the sedimentary source (the sediments coming from both the Iraqi-Iranian borderline and the Tigris river) on the optical and textural features, especially sphericity and roundness of feldspar minerals (potassium and plagioclase types) in soils of the southern part of the alluvial plain. Eight pedons were selected to represent the study area, five of them represented sediments coming from the borderline, which included pedons of (Badra, Taj Al-Din, Al-Shihabi, Jassan, and Galati), while two of them represent the sediments of the Tigris River (Essaouira, Al-Dabouni), the pedon of Ali Al-Gharbi was represented the mixing area of sediments of all the floods coming from the borderline and the sediments o
... Show MoreThe aim of this study is to identify the effect of particle size and to increase the concentration of Iraqi bentonite on rheological properties in order to evaluate its performance and to know if it can be used as drilling fluid without additives or not. In this study, Iraqi bentonite was carried out by mineral composition (XRD), chemical composition (XRF) and Particle size distribution (PSD), and its rheological properties were measured at different particle size and concentration. The results showed that when the particle size of Iraqi bentonite decreased, and the rheological properties were increased with increased concentration of Iraqi bentonite. Also, Iraqi bentonite was unable to use as drilling fluid without certain additives.
... Show MoreIn this study many specimen s were prepared from 2024-T3 Aluminum alloy for corrosion test by the dimensions of (15*15*3) mm according to ASTM G71-31 and then subjected to shot peening process at different time (15, 30, 45) minutes using steel ball having a diameter of 2.75 mm and Rockwell Hardness of 55RC to induce compressive residual stress which were measured using X-Ray diffraction method, surface roughness and hardness were tested before and after peening. Electrochemical corrosion test by Tafel extrapolation method was carried out in an environment of 3 .5% NaCl solutions (sea water) where Corrosion rate calculated using Tafle equation.
The obtained results show a favorable influence of SP treatment
... Show MoreBackground:Periodontal diseases and dental caries are the most common oral diseases, but they can be adequately prevented by adopting a specific health behavior and plaque control.The study was carried out to determine and compare oral health status; it included both caries experience, gingival health and oral hygiene behavior betweenfirst and fifth yearsof Al-Mustansiriyahdental students. Materials and methods: Total sample of the study consisted of 50 students at first year (25 males, 25 females)and 60 students at fifth year (30 males, 30 females). Plaque andgingival indices,dental caries indices (DMFS and DMFT) wererecorded to evaluateoral health status for each student. Further questionnaires were given to evaluate different oral hyg
... Show MoreObjectives: Maxillofacial silicone is used to restore abnormalities due to congenital or acquired causes. However, the quality of silicone is far from ideal. This study was aimed at assessing the influence of the addition of cellulose nanofibers (CNFs; several nanometers wide and 2-5 micro m long) on the physical and mechanical characteristics of maxillofacial silicone elastomers. Methods: Two CNF weight percentages (0.5% and 1%) were tested, and 180 specimens were divided into one control and two experimental groups. Each group was subdivided into six subgroups. In each subgroup, ten specimens subjected to each of the following tests: tearing strength, Shore-A hardness, tensile strength, elongation percentage, surface roughness, and color
... Show More