Background: Poly-ether-ether-ketone(PEEK) has been introduced to many dental fields. Recently it was tested as a retainer wire‎ following orthodontic treatment. This study aimed to investigate the effect of changing the bonding spot size and location on the performance of PEEK retainer wires. Methods: A biomechanical study involving four three-dimensional finite element models was performed. The basic model was with a 0.8 mm cylindrical cross-section PEEK wire, bonded at the center of the lingual surface of the mandibular incisors with 4 mm in diameter composite spots. Two other models were designed with 3 mm and 5 mm composite sizes. The last model was created with the composite bonding spot of the canine away from the center of the crown, closer to the lateral incisor. The linear displacement of the teeth, strains of the periodontal ligament, and stresses in PEEK wire and composite were evaluated. The data was numerically produced with color coded display by the software. Selected values were tabulated and compared among models. Results: The amount of linear displacement and strain was very low. Stresses in the wire and composite were affected by the size and position of the composite bonding spot. The safe limits were identified at 235 MPa for PEEK and 100 MPa for composite. The basic model had a von Mises stress in the PEEK wire of 122.09 MPa, and a maximum principal stress in the composite of 99.779 MPa. Both stresses were within the safe limits, which means a lower risk of failure in PEEK and composite. All other models had stresses that exceeded the safe limit of the composite. The 3 mm composite model was the only one that developed stresses in the wire more than the safe limits of PEEK. Conclusions: Within the limitations of this study, bonding PEEK wires with 4 mm bonding spots to the clinical crown center provided the best mechanical performance of the wires and spots; otherwise, the mechanical properties of the wire and composite would be affected and, therefore, might affect the retention process. Keywords: Retention, PEEK, Finite element analysis
The experiment was conducted at the Faculty of Agriculture University of Ain Shams-Egypt, from January to March 2008, to study the effect of different levels of chromium yeast (Cr-yeast) on broiler chickens performance, carcass quality and enzyme activity through 35 days of experimental periods. A total of 450 one-day old unsexed chickens (Cobb) strain were used. The birds were randomly allocated to five treatments with 3 replicates each. The treatments were control (T1) without supplementation and T2, T3, T4 and T5 which were supplemented with 0.5, 1, 1.5 and 2 mg Cr-yeast /kg diet, respectively. Live body weight and weight gain were significantly (p<0.05) higher when Cr-yeast were supplemented at 1 (T3), 1.5 (T4) and 2 (T5) mg/kg diet. Fe
... Show MoreThis paper is devoted to investigate the effect of internal curing technique on the properties of self-compacting concrete. In this study, self-compacting concrete is produced by using limestone powder as partial replacement by weight of cement with percentage of (5%), sand is partially replaced by volume with saturated fine lightweight aggregate which is thermostone aggregate as internal curing material in three percentages of (5%, 10%, 15%) for self-compacting concrete, and the use of two external curing conditions which are water and air. The experimental work was divided into three parts: in the first part, the workability tests of fresh self-compacting concrete were conducted. The second part included conducting compressive str
... Show Morethe shear strength parameters of the treated and untreated gypsum soil under the effect of four soaking and drying cycles has studied in this paper, moreover examined the effect of wetting and drying cycles on the collapse potential of the soil and comparing between the behavior of the treated and untreated gypsum soil under the effect of the two conditions. Gypsum soil sample brought from Sawa lake in Al Muthana governorate with the content of gypsum 65.5%, the polyurethane polymer (PP) was used with different percentages 3, 6, and 10% to enhance the mechanical properties of gypsum soil, model was prepared to achieve four soaking and drying cycle to the samples before testing, this model consists of an Aluminum plate base with dimensions 7
... Show MoreBackground: One of the most important complications of fixed orthodontic treatment is formation of white spots, which are initial carious lesions. Addition of antimicrobial agents into orthodontic adhesive material might be wise solution for prevention of white spots formation. The aim of this study was to evaluate the antibacterial properties of orthodontic adhesive primer against S. Mutans after adding the three different types of nanoparticles (Ag, ZnO, or TiO2). Materials and methods: Discs were prepared using empty insulin syringe approximately 2 mm×2 mm rounded in shape specimens (40 discs) were divided into four groups (ten discs for each group): The first group was the control (made from primer only), the second group (10 dis
... Show MoreAbstract:
Purpose\The researcher paper aims to determine the impact of information technology on the job performance, for Iraq private ban as through the use of technology dimensions of job performance.
The aim of this research: this study aims to discuss the importance of information technology and its role in achieving job performance and its impact on the Iraq banking sector design/ methodology/ approach used entrance design/methodology/approach- pilot, the questionnaire was used to collect data in order to develop a model to measure reliably and correctly to the variables of information technology and job performance, and hypotheses were tested through the use of some statisti
... Show MoreIron-Epoxy composite samples were prepared by added
different weight percentages (0, 5, 10, 15, and 20 wt %) from Iron
particles in the range of (30-40μm) as a particle size. The contents
were mixed carefully, and placed a circular dies with a diameter of
2.5 cm. Different mechanical tests (Shore D Hardness, Tensile
strength, and Impact strength ) were carried out for all samples. The
samples were immersed in water for ten weeks, and after two weeks
the samples were take-out and drying to conducting all mechanical
tests were repeated for all samples. The hardness values increased
when the Iron particle concentration increased while the Impact
strength is not affected by the increasing of Iron particles