Background: This in vitro study evaluated the fracture resistance of weakened endodontically treated premolars with class II MOD cavities restored with different composite restorations (Low-shrinkage Filtek P90, nanohybrid Filtek Z250 XT and SDR bulk fill). The type and mode of fracture were also assessed for all the experimental groups. Materials and Method: Fifty human adult maxillary premolar teeth were selected for this study. Standardized extensive class II MOD cavities with endodontic treatment were prepared for all teeth, except those that were saved as intact control. The teeth were divided into five groups of ten teeth each (n=10): (Group 1) intact control group, (Group 2) unrestored teeth with endodontic treatment, (Group 3) restored with (Filtek Z250 XT), (Group 4) restored with SDR bulk-fill flowable composite and (Group 5) restored with Filtek P90 composite. All specimens were subjected to compressive axial loading until fracture in a universal testing machine. The data were statistically analyzed using one-way ANOVA test and LSD test. Macroscopic fracture type were observed and classified into favorable and unfavorable. Specimens in group 3, 4 and 5 were examined by stereomicroscope at a magnification of 20× to evaluate the mode of failure into adhesive, cohesive or mixed. Results: The mean fracture load was (1.123 Kn) for group 1, (0.545 Kn) for group 2, (0.687 Kn) for group 3, (0.799 Kn) for group 4 and (0.672 Kn) for group 5. Using one way ANOVA test a highly significant difference (P < 0.01) were found among all groups. The use of bulk-fill flowable composite improved the fracture resistance significantly in comparison to silorane and non-significantly to Filtek Z250 XT. Filtek Z250 XT showed better improvement in fracture resistance but with no significant differences in comparison to Filtek P90 composite restorations. The type of failure was unfavorable for all the restored groups. Conclusion:All experimental composite restorations showed significant improvement in the resistance to cuspal fracture in comparison to unrestored one. However, under the conditions of this study, direct composite restorations should be considered as a valid interim restoration for weakened endodontically treated teeth before cuspal coverage can be provided.
Background: The Initial (primary) stability is one of the factors that play an important role in the success of the dental implants. The purpose of this study was to evaluate the initial stability of dental implant with horizontal plate by using five analytical tests: insertion torque, removal torque, resonance frequency analysis, push-in test and pull-out test. Materials and methods: Two different lengths of dental implants (5mm and 10mm) were tested in this study; each dental implant was 4mm in diameter with a square threads shape of 1mm pitch and 0.5mm depth. The crestal area was 4.2mm diameter contained a right angle margin circumferential ring while the apical area was tapered with two self-tapping grooves. In this study, the initial s
... Show MoreBackground: The bond strength of the root canal sealers to dentin seems to be a very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate the shear bond strength of four different obturation systems using push-out test. Materials and methods: Forty straight palatal roots of the maxillary first molars teeth were used in this study, these roots were instrumented using crown down technique and ProTaper system, instrumentation were done with copious irrigation of 2.5% sodium hypochlorite and 17% buffered solution of EDTA was used as final irrigant followed by distilled water, roots were randomly divided into four groups according to the obturation system (ten teeth for each g
... Show MoreBackground: Complete removal of filling material from the root canal is an essential requirement for endodontic retreatment. The purpose of the present study is to evaluate and compare the dissolving capabilities of various solvents (Xylene, Eugenate Desobturator, Eucalyptol, EDTA and Distilled water (as a control)) on four different types of sealer (Endofill, Apexit Plus, AH Plus and EndoSequence bioceramic sealer). Materials and method: Eighty samples of each sealer were prepared according to the manufacturers' instructions and then divided into ten groups (of 8 samples) for immersion in the respective solvents for 2 and 5 min immersion periods. Each sealer specimen was weighed to obtain its initial mass. The specimens were immersed in
... Show MoreBackground: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CA
... Show MoreThe present researchers are trying to enhance the properties of paper sheet that used widely in many fields such as printing and packaging. The enhancement of paper quality is also possible to preserve paper documents of all kinds, as they are the true record, full of the history, achievements of the human being and the intellectual and cultural of the country. It is possible to improve its physical and mechanical properties and preserve them from damage through the use of some solutions of polymeric adhesives, which act as protective barriers against water and moisture penetration. The paper also has the advantage of porosity, which has been overcome by using three types of polymeric adhesives (Nitro Cellulose, Polyvinyl alcohol acetate, a
... Show MoreBackground: Because of the demands for aesthetic orthodontic appliances have increased, aesthetic archwires have been widely used to meet patient's aesthetic needs. The color stability of aesthetic archwires is clinically important, any staining or discoloration will affect patient’s acceptance and satisfaction. This study was designed to evaluate the color stability of different types of aesthetic archwires after immersion into different types of mouth washes. Materials and methods: Four brands of nickel titanium coated aesthetic arch wires: Epoxy coated (Orthotechnology and G&H) and Teflon coated (Dany and Hubit) were evaluated after 1 week, 3 weeks and 6 weeks of immersion into two types of mouthwashes (Listerine with alcohol and
... Show MoreBackground: The miswak is a teeth cleaning twig made from a twig of the Salvadora persica tree (known as arak in Arabic).A traditional alternative to the modern toothbrush, it has a long, well-documented history and is reputed for its medicinal benefits. It also features prominently in Islamic hygienical jurisprudence. Materials and methods: Twenty maxillary first premolars were treated with the selected solutions which included siwak water extract (5%, 10%) and sodium fluoride 0.05% for 2minutes once daily for 20 days interval, deionized water was used as control negative. Then the concentration of the dissolved calcium ion in the etching solution of 2N HCL was measured. Results: The least amount of the dissolved calcium ion was registere
... Show MoreBackground: One common undesirable side effect of orthodontic treatment with fixed appliances is the development of incipient caries lesions around brackets, particularly in patients with poor oral hygiene. Different methods have been used to prevent demineralization; the recent effort to improve the resistance against the demineralization is by the application of lasers. Materials and method: Thirty human premolars extracted for orthodontic purposes were used to test the effect of two energy level of ER-YAG laser on enamel resistance to demineralization. The brackets were bonded on the teeth and all the labial surface excluding 2 mm area gingival to the brackets were painted with acid resistance varnish. Three groups were generated. The fi
... Show More