Background: Facial disfigurement can be the result of a congenital anomaly, trauma or tumor surgery, in many cases the prosthetic rehabilitation is indicated. Maxillofacial prosthetic materials should have desirable and ideal physical, aesthetic, and biological properties and those properties should be kept for long period of time in order to reach patient acceptance. Silicone elastomer are the most commonly used material for facial restoration because of its favorable properties mechanically and physically as the biocompatibility and good elasticity. Aim of this study: This study aimed to evaluate the effect of addition of Aluminum oxide (Al2O3) Nano fillers in different concentrations on tear strength and hardness of VST 50F room temperature vulcanized maxillofacial silicone. Methods: The Nano Al2O3 was added in a concentrations of 0.5, 1, 1.5 and 2 by weight to the VST 50F RTV maxillofacial silicone, the samples were tested for tear strength (ISO 34 -1) and shore A hardness (ISO 7619), the FTIR was used to analyze the interaction of the Nano Al2O3 with the silicone. The data were analyzed using descriptive and inferential statistics. One-way ANOVA test was used to test the changing significance. Results: There was no interaction between the Nano-Al2O3 and the silicone in the FTIR. The results showed highly significant increase in tear strength and shore A hardness for the 1 and 1.5 concentration groups when Compared to control group. Conclusion: The reinforcement of VST 50F maxillofacial silicone with 1 and 1.5 concentrations of Nano Al2O3 improved some of the mechanical properties of the room temperature vulcanized silicone.
In this study, some attenuation parameters of gamma shields were studied. This shields consisting of composite materials of Unsaturated polyester as a base material and Nano iron oxide (Fe2O3) and, micro iron (Fe) as reinforcement materials at different percentages (1, 3,5,7and 9)wt%, and with different thickness (1, 1.5, 2, 2.5, 3, 3.5and 4) cm. The results showed that the use of nanoparticles is better than the microparticales in the field of radiation shielding. It has been shown that the values of attenuation parameters of gamma it bitter in the case of nanoparticles than case of the use of micro material.
The design of components subjected to contact stress as local compressive stress is important in engineering application especially in ball and socket Joining. Two kinds of contact stress are introduced in the ball and socket joint, the first is from normal contact while the other is from sliding contact. Although joining two long links (drive shaft in steering cars) will cause the effect of flexural and tensional buckling stress in hollow columns through the ball and socket ends on the failure condition of the joining mechanism. In this paper the consideration of the combined effect of buckling Load and contact stress on the ball and socket joints have been taken, epically on the stress distribution in the contact area. Different
... Show MoreIn this work, two groups of nanocomposite material, was prepared from unsaturated polyester resin (UPE), they were prepared by hand lay-up method. The first group was consisting of (UPE) reinforced with individually (ZrO2) nanoparticles with particle size (47.23nm). The second group consists of (UPE) reinforced with hybrid nanoparticles consisting of zirconium oxide and yttrium oxide (70% ZrO2 + 30% Y2O3) with particles size (83.98nm). This study includes the effect of selected volume fraction (0.5%, 1%, 1.5%, 2%, 2.5%, 3%) for both reinforcement nano materials. Experimental investigation was carried out by analyzing the thermo-physical properties like thermal conductivity, thermal diffusivity and specific heat for the polymeric composit
... Show MoreThe CdSe pure films and doping with Cu (0.5, 1.5, 2.5, 4.0wt%) of thickness 0.9μm have been prepared by thermal evaporation technique on glass substrate. Annealing for all the prepared films have been achieved at 523K in vacuum to get good properties of the films. The effect of Cu concentration on some of the electrical properties such as D.C conductivity and Hall effect has been studied.
It has been found that the increase in Cu concentration caused increase in d.c conductivity for pure CdSe 3.75×10-4(Ω.cm)-1 at room temperatures to maximum value of 0.769(Ω.cm)-1 for 4wt%Cu.All films have shown two activation energies, where these value decreases with increasing doping ratio. The maximum value of activation energy was (0.319)eV f
Films of CdSe have been prepared by evaporation technique with thickness 1µm. Doping with Cu was achieved using annealing under argon atmosphere . The Structure properties of these films are investigated by X-ray diffraction analysis. The effect of Cu doping on the orientation , relative intensity, grain size and the lattice constant has been studied. The pure CdSe films have been found consist of amorphous structure with very small peak at (002) plane. The films were polycrystalline for doped CdSe with (1&2wt%) Cu contents and with lattice constant (a=3.741,c=7.096)A°, and it has better crystallinty as the Cu contents increased to (3&5wt%) Cu. The reflections from [(002), (102). (110), (112), and (201)]planes are more prominen
... Show MoreBruggeman's symmetric effective-medium model of vanadium oxide is introduced, in which the transmittance was studied because of its importance in the subject of smart windows, it was studied from ( 5 nm-1000 nm) for each of the regions of the electromagnetic spectrum, the ultraviolet and visible region, and the near and medium sub-regions of the infrared and the results showed that the importance of studying the transmittance of vanadium oxide as a good candidate For this kind of industries. Our results showed that the small sizes of the material guarantee an almost constant and high transmittance to the visible region; this is due to the agreement of the direction of the dipoles in the material with the direction of the internal el
... Show More
In this work, InSe thin films were deposited on glass substrates by thermal evaporation technique with a deposit rate of (2.5∓0.2) nm/sec. The thickness of the films was around (300∓10) nm, and the thin films were annealed at (100, 200 and 300)°C. The structural, morphology, and optical properties of Indium selenide thin films were studied using X-ray diffraction, Scanning Electron Microscope and UV–Visible spectrometry respectively. X-ray diffraction analyses showed that the as deposited thin films have amorphous structures. At annealing temperature of 100°C and 200°C, the films show enhanced crystalline nature, but at 300°C the film shows a polycrystalline structure with Rhombohedral phas