Background: The study aim was to evaluate thermocycling effect on microleakage of occlusal and cervical margins of MOD cavity filled with bulk filled composites in comparison to incrementally placed nanohybrid composite and to evaluate the difference in microleakage between enamel and dentin margins for the three materials groups. Materials and method: Forty eight maxillary first premolars were prepared with MOD cavities. Samples were divided into three groups of sixteen teeth according to material used: Grandio: Grandio. SDR: SDR +Grandio. X-tra: X-tra base + Grandio. Each group was subdivided into two according to be thermocycled or not. After 24 hrs immersion in 2% methylene blue, samples weresectioned and microleakage was estimated. Results: Thermocycling significantly increased microleakage at occlusal margin in Grandio group compared to other groups. SDR composite use before and after thermocycling significantly reduced microleakage at occlusal and cervical enamel margins compared to other groups. Grandio group had non significant difference to X-tra group in microleakage before thermocycling at occlusal and cervical enamel margins while it had a significant increase after thermocycling. No material had significantly reduced dentin margin microleakage before or after thermocycling. Only SDR group before thermocycling, significantly reduced microleakage in enamel margin compared to dentin margin. Conclusion: Thermocycling did not increase microleakage in all the groups except for Grandio group in occlusal margin. SDR group showed reduced microleakage in occlusal and enamel margins in comparison to other groups.None of the materials reduced microleakage in dentin margin.
Mixed ligand of Co and Ni (II) complexes were prepared from [5-(p-nitrophenyl)-4/-phenyl-1,2,4-triazole-3-dithiocarbamato hydrazide](TRZ.DTC) as primary ligand and 2,2'-bipyridyl (bipy) as a co-ligand with metal salts. These complexes were analytically and spectroscopically characterized in solid state by elemental analyses, flame atomic absorption, magnetic susceptibility and molar conductance measurements, as well as by UV–Vis and FTIR spectroscopy. Infrared, ultra violet spectra reveal a bidentate coordination of the two ligands with metal ions 1:1:1 mole ratio. Room temperature magnetic moments and solid reflectance spectra data indicate paramagnetic complexes with five-coordinate square pyramidal geometry for nickel (II) comple
... Show MoreIn this paper, effective slab width for the composite beams is investigated with special emphasis on the effect of web openings. A three dimensional finite element analysis, by using finite element code ANSYS, is employed to investigate shear lag phenomenon and the resulting effective slab width adopted in the classical T-beam approach. According to case studies and comparison with limitations and rules stipulated by different standards and codes of practice it is found that web openings presence and panel proportion are the most critical factors affecting effective slab width, whereas concrete slab thickness and steel beam depth are less significant. The presence of web opening reduces effective slab width by about 21%.
... Show MoreBackground: Ceramic veneers represent the treatment of choice in minimally invasive esthetic dentistry; one of the critical factors in their long term success is marginal adaptation. The aim of the present study is to evaluate the marginal gap of ceramic veneers by using two different fabrication techniques and two different designs of preparation. Material and methods: A typodont maxillary central incisor used in the preparation from which metal dies were fabricated, which were in turn used to make forty stone dies. The dies divided into four experimental groups, each group had ten samples: A1: prepared with butt-joint incisal reduction and restored with IPS e.max CAD, A2: prepared with overlapped incisal reduction and restored with IPS e.
... Show MoreThis research is carried out to study the effect of the external post-tensioning technique on the flexural capacity of simply supported composite castellated beam experimentally. In this research, seven composite castellated beams having the same dimensions and material properties were cast and tested up to failure by applied two concentrated loads at 700 mm from each end. Two external strands of 12.7 mm diameter were fixed at each side of the web of strengthening beams and located at depth 180 mm from top fiber of the section (dps) at each end of the beam. The strands have been tensioned by using a hydraulic jack with a constant stress of 100 MPa. This research aims to study the effect of the strengthening by different shapes of st
... Show MoreBackground:Â Various fluids in the oral environment can affect the surface roughness of resin composites. This in vitro study was conducted to determine the influence of the mouth rinses on surface roughness of two methacrylate-based resin (nanofilled and packable composite) and siloraine-based resin composites.
Materials and methods: Disc-shaped specimens (12 mm in diameter and 2mm in height) were prepared from three types of composi
... Show MoreBackground: As the development of zirconia crown using CAD/CAM technology, the usage of full zirconia crown is gradually increased. The aim of this in-vitro study was to evaluate and contrast the vertical marginal fit of single all-ceramic translucent zirconia crowns constructed from different brands translucent zirconia blanks. Materials and Methods: An acrylic resin model of a left maxillary premolar was prepared all around the tooth with (1 mm) depth and 3D scanning to get fifteen STL files, then distributed into three groups (Imes-icor, Whitepeaks and Dental direct), 3D scanning and milling machine by Imes-icor CAD/CAM devise. Marginal gaps along vertical planes were measured at four indentations at the (mid mesial, mid distal, mid bucc
... Show MoreIntroduction: We aimed to assess the impact of adhesive and wires types on the tensile bond strength of fixed lingual retainers. Methods: A total of 160 intact bovine teeth were collected, cleaned, stored in 25% sodium hypochlorite, and randomly assigned to two groups based on the adhesive type: a two-step adhesive and a one-step adhesive. Each group was further divided into four subgroups based on the type of lingual retainer wire, which included (A) 8-strand braided stainless steel wire, (B) three-strand titanium retainer wire, (C) stainless steel chain, and (D) fiber-reinforced retainer. A tensile bond strength test was conducted using a universal testing machine at a controlled speed of 10 mm/min. Result: The 8-strand braided stainles
... Show More