Back ground: Microbial penetration inside the implant's internal hole creates a bacterial reservoir that is related with an area of inflamed connective tissue opposite the fixture-abutment junction and this can affect the health of the peri-implant tissue. Aims of the study: Evaluate the types aerobic and anaerobic bacterial count-percentage and difference between Aerobic and Anaerobic microflora in the implant screw hole three months after implant placement. Monitor the periodontal health status of all patients, throughout the study. Material and methods: Study methodology; Eight partially edentulous patients received 20 dental implants and these implants done with flapless surgical procedure. All patients examined clinically to determined their oral health status by examination of their plaque index, Gingival index and Bleeding on probing, each two weeks for 90 days (8visits) throughout the study period. Three months after that, the plaque sample collected from the internal hole of fixture and transfer to bacterial investigation and assessment the amount of anaerobic and aerobic bacteria. Results: Although the anaerobic viable count is higher than that of aerobic, but with statistically not significant difference between those counts (P>0.05). Keywords: screw hole, flapless surgical implant placement, bacterial count, Aerobic and Anaerobic bacteria
In this study, a Hydroxyapatite (HA) coating was prepared on a titanium implant by an electrochemical deposition process. The titanium pre-treatment by anodizing in 1.65 mol/L sulfuric acid with (10V) at room temperature. The deposition was all conducted at a constant voltage of 6.0 V, for 1 h at room temperature. The coatings thus prepared were characterized with Fourier transform infrared spectroscopy (FTIR) and thickness of the coated layer.The electrochemical deposition of HA occurred on the titanium as a cathode. Coated titanium by HA after anodizing revealed a good corrosion protection efficiency even at a temperature ranged (293-323) K in artificial saliva. Activation energy and pre-exponential factor (kinetic parameters) were calcul
... Show MoreBackground: The use of osseointegrated fixtures in dentistry has been demonstrated both histologically and clinically to be beneficial in providing long term oral rehabilitation in completely edentulous individual. Most patients suffer from denture instability; particularly with mandibular prosthesis, the use of dental implant will be benefit significantly from even a slight increase in retention. The concept of implanting two to four fixtures in a bony ridge to retain a complete denture prosthesis appealing therefore, as retention, stability and acceptable economic compromise to the expanse incurred with the multiple fixture supported fixed prosthesis. Materials and methods in this study the sample were eight patients selected from a hosp
... Show MoreBackground: The Initial (primary) stability is one of the factors that play an important role in the success of the dental implants. The purpose of this study was to evaluate the initial stability of dental implant with horizontal plate by using five analytical tests: insertion torque, removal torque, resonance frequency analysis, push-in test and pull-out test. Materials and methods: Two different lengths of dental implants (5mm and 10mm) were tested in this study; each dental implant was 4mm in diameter with a square threads shape of 1mm pitch and 0.5mm depth. The crestal area was 4.2mm diameter contained a right angle margin circumferential ring while the apical area was tapered with two self-tapping grooves. In this study, the initial s
... Show MoreAbstract: Recombinant human bone morphogenetic protein-2 (rhBMP-2) and platelet-rich fibrin (PRF) bioactive materials have been used to enhance healing and improve dental implant stability. This study aimed to compare the effect of rhBMP-2 and PRF bioactive materials on dental implant stability at different intervals and to evaluate the correlation of implant length and diameter with implant stability. Two bioactive materials were compared to evaluate their effect on dental implant stability. A total of 32 patients (102 dental implants) were divided into 3 groups: 24 dental implants with bone morphogenetic protein (BMP), 27 dental implants with PRF, and 51 dental implants without BMP or PRF (control group). Data were statistically analyzed
... Show MoreBackground: The healing period for bone–implant contact takes 3–6 months or even longer. Application of Escherichia coli-derived recombinant human bone morphogenetic protein-2 (ErhBMP-2) to implant surfaces has been of great interest on osseointegration due to its osteoinductive potential. The objective of this study was to evaluate the effect of ErhBMP-2 on implant stability. Materials and methods: A total of 48 dental implants were inserted in 15 patients. Twenty four implants coated with 0.5 mg/ml ErhBMP-2 (study group). The other 24 implants were uncoated (control group). Each patient was received at least two dental implants at the same session. Both groups were followed with repeated implant stability measurements by me
... Show MoreBackground: the primary objective for many researches carried out in dental implantology was to reduce the period needed for functional implant loading, simvastatin (cholesterol lowering medication) had many pleiotropic effects, one of which was increasing bone density around titanium implants (1) and subsequently establishing faster osseointegrated dental implants (2,3). This study aims to reduce the period of time needed to establish secondary stability of dental implant measured in ISQ (Implant Stability Quotient) by investigating the effect of orally administered simvastatin on bone. Materials and methods: simvastatin tablets (40mg/day for three months) were administered orally for 11 healthy women aged (40-51) years old who received 1
... Show MoreObjective: Evaluation of the poly ether keton keton polymer (PEKK) coating material on the commercial pure titanium disks (CP Ti) with or without laser surface structuring. Design: In vitro experimental study of PEKK polymer coated material on the CP Ti disks with or without laser surface structuring. Materials and methods: coating the surface of the commercial pure titanium (CP Ti) disks with PEKK polymer was performed via using frictional mode CO2 laser, then the samples disks analyzed by using FESEM. Results: the FESEM reveal good adherence and distribution of the PEKK coated material over the CP Ti substrate by using the frictional mode CO2 laser at 2 watt and 6 ms pulse duration. Conclusion: the frictional mode CO2 laser considered an
... Show MoreBackground: The aims of this study were to evaluate the effect of implant site preparation in low-density bone using osseodensification method in terms of implant stability changes during the osseous healing period and peri-implant bone density using CBCT. Material and methods: This prospective observational clinical study included 24 patients who received 46 dental implants that were installed in low-density bone using the osseodensification method. CBCT was used to measure the bone density pre- and postoperatively and implant stability was measured using Periotest® immediately after implant insertion and then after 6 weeks and 12 weeks postoperatively. The data were analyzed using paired t-test and the probability value <0.05 was conside
... Show MoreBackground: Contact between implant material and bones must be strong and fast creation, to fulfill these properties appropriate surface modifications must apply on used implants. In this contribution; double surface modifications are applied on Ti-6Al-4V alloy to accelerate osseointegration. Materials and methods: Anodic process is utilized to create titania nanotubes (TNTs) on the screws made from Ti-6Al-4V alloy. These implants were coated with nano ZrO2 particles. Second modification was annealing anodized screws at 8000C, and implanted in tibiae of nine adult New Zealand white rabbits. Results: Physical and histological consequences of two surface modifications on Ti-6Al-4V alloy screws were studied. Scanning electron microscope (SEM)
... Show MoreAim: surface modification of titanium using fiber laser 1064 nm to enhance the bond strength to resin cement. Material and Methods: thirty titanium discs of 0.6 cm x 0.3 cm (diameter and thickness respectively) were categorized after preparation into three groups (n=10) as follows: control group with no surface treatment and two test groups were treated with fiber laser after estimation the appropriate parameters in the pilot study which are 81 ns pulse duration, 30,000 Hz frequency, 50 µm spot size and 10,000 mm/s scanning speed and different average power values (10 W and 20 W) depending on the tested group. Titanium discs surface characterization was performed by scanning electron microscope (SEM), a