Background: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive resin. Shear bond strength was measured by using Tinius Olsen universal testing machine. After debonding, each bracket and zirconium surface were examined and adhesive remnant index was registered. The difference in shear bond strength among groups was analyzed by using ANOVA test. The adhesive remnant index was assessed using Chi-square test. Results: The 2nd laser group had the highest mean value of shear bond strength then the 1st laser group followed by the sandblasting group, while the control group had the least value, non-significant difference in the shear bond strength was found between the laser groups and highly significant difference was found between all other comparable groups. Non-significant difference in the site of bond failure was found between the laser groups and sandblasting group, and between the two laser groups. Conclusion: The laser conditioning method showed higher value of shear bond strength than the sandblasting conditioning method.
In this research, deposition of titanium oxide (TiO2) and vanadium oxide (V2O5) thin film in different mixing percentage (0, 25 ,50, 75 and100)% on the substrate of glass .The coating thickness was ( 50 nm ).
In this research contact angle was measured and the effect of weather conditions. Results showed that the value of the contact angle of the prepared films reached its highest value at 50% (TiO2+V2O5) was 160º.
The results showed that the optical transmittance of TiO2 and V2O5 thin film decrease with increasing the deposition angle and decrease with increasing V2O5 pro
... Show MoreMagnesium oxide nanoparticles were synthesized via a co-precipitation procedure. Comprehensive characterization included infrared fluorescence, X-ray scattering spectroscopy, scanning electron microscopy, as well as X-ray diffraction and atomic force microscopy. Surface properties were analyzed using Langmuir, Brunauer -Emmett-Teller, Barrett–Joyner–Halenda, t-plot techniques, and the N2 adsorption-desorption isotherms methods to determine surface area and pore structure. Results confirmed the nanoparticles possess high purity. The size of the synthesized particles ranged from 30-40 nm, which was determined by scanning electron microscopy. The surface area of the prepared particles is 31,227 m2 g-1, and it was found that the por
... Show MoreBackground: The development of orthodontic biomaterials that attract less biofilm has been a goal for decades. Adhesion and colonization of cariogenic streptococci are considered to play key roles in the development of enamel demineralization related to orthodontic materials. The aim of this study was to quantitatively evaluate the Mutans streptococci adhesion to coated orthodontic archwires (Epoxy and Teflon) and uncoated archwires (stainless steel and nickel-titanium) with respect to incubation time in the presence and absence of saliva. Material and Method: Six types of archwires stainless steel and nickel titanium with two type of coating (Epoxy, Teflon) were used in this study. Twelve specimens of each archwire were incubated in steri
... Show MoreBackground: Maxillary first premolar with wide MOD cavity more susceptible to fracture. The aim of this study was to assess the influence of cavity design for cusp coverage on the fracture resistance of weakened maxillary first premolar restored with CAD/CAM hybrid ceramic versus nanohybide composite. Materials and Methods: Fifty six intact maxillary first premolars of approximately comparable sizes were divided into seven groups eight for each: Group A: Intact teeth (control group); Group B: teeth prepared for MOD inlay; Group C: teeth prepared for MOD onlay covering the lingual cusp; Group D: teeth prepared for MOD covering buccal and lingual cusps ,the previous three groups indirectly restored with nanohybrid composite (3M ESPE Z 250 X
... Show MoreBecause of the experience of the mixture problem of high correlation and the existence of linear MultiCollinearity between the explanatory variables, because of the constraint of the unit and the interactions between them in the model, which increases the existence of links between the explanatory variables and this is illustrated by the variance inflation vector (VIF), L-Pseudo component to reduce the bond between the components of the mixture.
To estimate the parameters of the mixture model, we used in our research the use of methods that increase bias and reduce variance, such as the Ridge Regression Method and the Least Absolute Shrinkage and Selection Operator (LASSO) method a
... Show MoreThe aim of this study is to investigate the antibacterial capabilities of different coating durations of three nanoparticle (NP) coatings: molybdenum (Mo), tantalum (Ta), and zinc oxide (ZnO), and their effects on the surface characteristics of 316L stainless steel (SS). The coated substrates underwent characterization utilizing field emission scanning electron microscopy (FE-SEM), energy dispersive X-ray spectrometry (EDX), and X-ray diffractometer (XRD) techniques. The antibacterial efficacy of NPs was evaluated using the agar diffusion method. The FE-SEM and EDX images confirmed the presence of nano-sized particles of Mo, Ta, and ZnO on the surface of the substrates with perfectly symmetrical spheres and a uniform distribution of
... Show MoreTo evaluate the effectiveness of different microwave irradiation exposure times on the disinfection of dental stone samples immersed in different solutions, and its affect on the dimensional accuracy and surface porosity. Dental stone casts were inoculated with an isolate of Bacillus subtilis to examine the efficiency of microwave irradiation as a disinfection method while immersed in different solutions; water, 40% sodium chloride, or without immersion for different durations. Dimensional accuracy and surface porosity were also evaluated. Significant reduction in colony counts of Bacillus subtilis were observed after 5 minutes of microwave irradiation of immersed dental casts in water and NaCl solution. No evidence of growth was observed a
... Show MoreObjective: To evaluate the effect of mouth rinses (Biofresh and ZAK) on the surface micro hardness
of two light cure restorative material (Tetric ceram ivoclar-vivadent) and (3M Z 250) dental
composite.
Methodology: The microhardness values of (sixty) composite specimens were measured at the top
surfaces after 24 hours of immersion in different solutions (Biofresh, Zak mouth wash and distilled
water as control). Comparison done using descriptive statistics (mean, SD, SEM, minimum and
maximum values) and inferential statistics (ANOVA and LSD) test.
Results: The biofresh mouth rinse which has high alcohol containing has less effect on
microhardness of tetric ceram than the zak &distiled water , while the effect