Background: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before bonding (3M, Clinpro + 3M, Ormco, Clinpro + Ormco) each group was subdivided into four equal subgroups each with 8 teeth. After passing twenty-four hours of bonding procedure, where the samples were kept at 37˚C the brackets were debonded by using Tinius-Olsen universal testing machine to record the shear and tensile bond strength value. The difference in bond strength was analyzed by using ANOVA test at p≤0.05. Results: The use of Clinpro with 3M Unitek orthodontic bonding agent shows higher shear and tensile bond strength than Clinpro with Ormco orthodontic bonding agent. Conclusions: Using Clinpro white varnish before bonding can be successfully used with 3M Unitek orthodontic bonding agent.
In this research TiO2 nano-powder was prepared by a spray pyrolysis technique and then adds to the TiO2 powder with particle size (0.523 μm) in ratio (0, 5, 10, 15 at %) atomic percentage, and then deposition of the mixture on the stainless steel 316 L substrate in order to use in medical and industrial applications.
Structure properties including x-ray diffraction (XRD) and scanning electron microscope (SEM0, also some of mechanical properties and the effect of thermal annealing in different temperature have been studied. The results show that the particle size of a prepared nano-powder was 50 up to 75 nm from SEM, and the crystal structure of the powders (original and nano powder) was rutile with tetragonal cell. An improvement in
Objectives: Successful endodontic treatment outcome requires effective shaping and cleaning of root canals. This study aims to evaluate the smear layer removal after continuous chelation (CC) ) NaOCL\HEDP( and sequential chelation (SC) )NaOCL\EDTA( and their influence on the push-out bond strength (POBS) of Bio-C sealer. Materials and Methods: Palatal roots of the maxillary first molar (n=72) were divided into four groups (n=18) as follows: 3% NaOCL, SC: 3% NaOCL followed by 17% EDTA, CC: 3% NaOCL \9% HEDP and Distilled water. Thirty-two roots (n=8/group) were split longitudinally for smear layer evaluation using SEM. Forty roots were obturated with Guttapercha and Bio-C sealer using a single cone technique. Thre
... Show MoreBackground: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreThe marine collagens are biocompatible and biodegradable materials that are considered as a biomimetic approach for tissue regeneration. This study evaluated the effect of daily consumption of marine collagen supplement drink on enamel white spot lesions (WSLs), comparing the results against Regenerate system and Sylc air abrasion methods. Fifty human enamel slabs were allocated into five groups (n = 10 per group): non-treated (sound); non-treated (WSLs, 8% methylcellulose gel with 0.1 M lactic acid (pH 4.6) at 37 °C for 21 days); and three treated surfaces with marine collagen; Regenerate system; and Sylc air abrasion. The treatment lasted for 28 days followed by four weeks’ storage in artificial saliva (pH = 7.0, 37 °C). Evalu
... Show MoreBackground: Sliding mechanics is widely used during orthodontic treatment. One of the disadvantages of this mechanics is the friction generated at the bracket/archwire interface, which may reduce the amount of desired orthodontic movement obtained. The aim of the present in vitro study was to evaluate and compare the static frictional forces produced by two passive self-ligating brackets stainless-steel and hybrid and two conventional brackets stainless-steel and monocrystal ligated with stainless-steel ligature wire at two degrees of torque(zero and twenty) under dry condition. Materials and method: One hundred and sixty brackets were used in this study divided into four groups each group consisted of forty brackets these are: Two self-li
... Show MoreBackground: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CA
... Show MoreAbstract
Stainless steel (AISI 304) has good electrical and thermal conductivities, good corrosion resistance at ambient temperature, apart from these it is cheap and abundantly available; but has good mechanical properties such as hardness. To improve the hardness and corrosion resistance of stainless steel its surface can be modified by developing nanocomposite coatings applied on its surface. The main objective of this paper is to study effect of electroco-deposition method on microhardness and corrosion resistance of stainless steel, and to analyze effect of nanoparticles (Al2O3, ZrO2 , and SiC) on properties of composite coatings. I
... Show MoreUsing an electrochemical polymerization technique at room temperature, poly nicotine amide (PNA) was produced from the monomer nicotine amide (NA) in aqueous solution. The structure of polymer layer generated on the stainless steel surface (316 L) (working electrode) is investigated by Fourier Transmission Infrared Region (FT-IR). The anti-corrosion activity of polymer coating on the stainless steel (SS 316 L) is investigated by electrochemical polarization in 0.20M solution of HCl at 293-323K. The graphene -modified polymer film-coated SS had greater protection efficiency (PE percent) when compared to Nano ZnO -modified polymer film-coated SS. For the corrosion process of SS 316 L, kinetic and thermo-dynamic parameters of activatio
... Show More