Background: Denture fracture is one of the most common problems encountered by the patients and prosthodontists. The objective of present study was to evaluate the transverse strength of nylon denture base resin repaired by using conventional heat polymerized, autopolymerized and visible light cure {VLC} resins, surface treatment that used for repair and adjustment of insufficient nylon denture bases and in case of addition of artificial teeth. As these corrective procedures are common chair side procedures in dental clinic. Materials and methods: One hundred twenty nylon specimens were prepared by using metal patterns with dimension of (65x10x2.5 mm) length, width, and thickness respectively for transverse strength test while for tensile bond strength a dumbbell-shaped with measurement (65x12.5x25mm) length, width, and thickness respectively were flasked with stone. The nylon specimens were molded by reflasked with dental stone that used as an index for these specimens in the repair procedure and repaired with 45 degree bevel joint by using metal holding device. The two parts of nylon specimen to be repaired were realigned in its repair index and adhere with special adhesive material to stabilize the combination during repair procedure. The dough of heat and cold cure resin was packed into the joint and then cured. The specimen repaired with cold cure resin was placed in the Ivomat containing water at (40°C) and pressure (30IB/inch²) for 15 minutes. The specimen repaired with {VLC} was placed in the light cure unit for 4 minutes following manufacturer’s instruction. The fractured nylon specimens were divided according to the type of repaired materials into (40) specimens received heat cure acrylic and the (40) specimens received cold cure acrylic and the other 40 specimens received {VLCR}. Each 40 specimens were subdivided according to the type of surface treatment received into 20 specimens were treated with coarse stone bur (control), 20 specimens were treated with combination of coarse stone bur and monomer of the heat cure acrylic. After that the specimens were subjected to transverse {Tr} and tensile bond {TB} strength tests. For each test 10 specimens. Results and conclusions: This study showed that specimens treated with combination of coarse stone bur and monomer of the acrylic (heat, cold or VL cure) had the highest transverse and tensile strength values, followed by the specimens treated with coarse stone bur. The results showed that the specimens repaired with heat cure acrylic had transverse and tensile strength values higher than the specimens repaired with cold and VL cure acrylic when compared between subgroups of heat, cold and VL cure acrylic that received the same treatments.
KE Sharquie, AA Noaimi, HG Mahmood, SM Al-Ogaily, Journal of Cosmetics, Dermatological Sciences and Applications, 2015 - Cited by 6
Steady natural convection in a square enclosure with wall length (L= 20 cm) partially filled by saturated porous medium with same fluid (lower layer) and air (upper layer) is investigated. The conceptual study of the achievements of the heat transfer is performed under effects of bottom heating by constant heat flux (q=150,300,450,600W/m2 ) for three heaters size (0.2,0.14,0.07)m with symmetrically cooling with constant temperature on two vertical walls and adiabatic top wall. The relevant filled studied parameters are four different porous medium heights (Hp=0.25L,0.5L, 0.75L, L), Darcey number (Da1) 3.025×10-8 and (Da2) 8.852×10-4 ) and Rayleigh number range (60.354 - 241.41), (1.304×106 – 5.2166×106 ) for Da1 and Da2 cases respecti
... Show MoreThe heat transfer and flow resistance characteristics for air flow cross over circular finned tube heat exchanger has been studied numerically and experimentally. The purpose of the study was to improve the heat transfer characteristics of an annular finned-tube heat exchanger for better performance. The study has concentrated on the effect of the number of perforations and perforations shapes on the heat transfer and pressure drop across a staggered finned tube heat exchanger. The Numerical part of present study has been performed using ANSYS Fluent 14.5 using SST Turbulent model, while the experimental study consist from a test rig with different models of heat exchangers and all required measurement devices were build
... Show MoreDespite the great economic and commercial importance given to real estate by virtue of its view of the landscape or public roads, US courts have differed in their position on compensation for damages resulting from blocking that view or vision by public projects. Some courts compensated for such damages, other courts approved such compensation. Hence, this research came to shed light on the extent of the possibility of compensation for blocking the view or vision as a result of public projects, and the research has supported us with many judicial decisions.
The current research aims to identify the effect of Baska style on students’ achievement and the creative thinking in material rhetoric and the application of students for fifth grade literary. To achieve the study objectives, the researcher has designed an achievement test to measure group of students in the fifth grade literary in material application. The researcher chose a sample of 40 female students from Khansa School for Girls in Baghdad for the academic year (2014 - 2015), he applied the test on an exploratory sample consisted of 30 female students from the research community. The study resulted in being no statistically significant difference at the level of significance (0.05) between the mean scores of the experimental group
... Show MoreBackground: Esthetic correction represents one of the clinical conditions that required the use of laminate veneers in premolars region. Aim of the study: The purpose of this study was to evaluate the fracture strength of the laminate veneers in maxillary first premolars, fabricated from either composite (direct and indirect techniques) or ceramic CAD/CAM blocks. Materials and Methods: Fifty sound human maxillary premolar teeth were used in this in vitro study. Teeth were divided randomly into one control group and four experimental groups of ten teeth each; Group A: Restored with direct composite veneer (Filtek Z250 XT), Group B: Restored with indirect composite veneers (Filtek Z250 XT), Group C: Restored with lithium disilicate ceramic CA
... Show More