Background: Denture fracture is one of the most common problems encountered by the patients and prosthodontists. The objective of present study was to evaluate the transverse strength of nylon denture base resin repaired by using conventional heat polymerized, autopolymerized and visible light cure {VLC} resins, surface treatment that used for repair and adjustment of insufficient nylon denture bases and in case of addition of artificial teeth. As these corrective procedures are common chair side procedures in dental clinic. Materials and methods: One hundred twenty nylon specimens were prepared by using metal patterns with dimension of (65x10x2.5 mm) length, width, and thickness respectively for transverse strength test while for tensile bond strength a dumbbell-shaped with measurement (65x12.5x25mm) length, width, and thickness respectively were flasked with stone. The nylon specimens were molded by reflasked with dental stone that used as an index for these specimens in the repair procedure and repaired with 45 degree bevel joint by using metal holding device. The two parts of nylon specimen to be repaired were realigned in its repair index and adhere with special adhesive material to stabilize the combination during repair procedure. The dough of heat and cold cure resin was packed into the joint and then cured. The specimen repaired with cold cure resin was placed in the Ivomat containing water at (40°C) and pressure (30IB/inch²) for 15 minutes. The specimen repaired with {VLC} was placed in the light cure unit for 4 minutes following manufacturer’s instruction. The fractured nylon specimens were divided according to the type of repaired materials into (40) specimens received heat cure acrylic and the (40) specimens received cold cure acrylic and the other 40 specimens received {VLCR}. Each 40 specimens were subdivided according to the type of surface treatment received into 20 specimens were treated with coarse stone bur (control), 20 specimens were treated with combination of coarse stone bur and monomer of the heat cure acrylic. After that the specimens were subjected to transverse {Tr} and tensile bond {TB} strength tests. For each test 10 specimens. Results and conclusions: This study showed that specimens treated with combination of coarse stone bur and monomer of the acrylic (heat, cold or VL cure) had the highest transverse and tensile strength values, followed by the specimens treated with coarse stone bur. The results showed that the specimens repaired with heat cure acrylic had transverse and tensile strength values higher than the specimens repaired with cold and VL cure acrylic when compared between subgroups of heat, cold and VL cure acrylic that received the same treatments.
Background: Cross contamination of dental appliances in the dental clinics and laboratories may potentially be a health hazard to the dental team and the patient. This study aimed to evaluate bacterial contamination of acrylic complete denture as received from dental laboratory before delivery to the patient, and then to evaluate the effectiveness of disinfection with 2% chlorhexidine and Kin denture cleaner tablet. Materials and methods: 45 newly made upper complete dentures undergone biaacterial examination for contamination before delivered to the patient. Samples were examined in two stages, first after finishing and polishing; when collected from the laboratory and before inserting to the patient mouth, second; after the samples were
... Show MoreBackground: The PMMA polymer denture base materials are low in thermal and strength properties. The aim of the study was to investigate the change in glass transition temperature, E-Moudulus and coefficient of thermal expansion of acrylic denture base material by addition of Al2O3, TiO2 and SiO2nano-fillers in 5% by weight. Materials and methods: The type of polymerization is free radical bulk polymerization. one hundred twenty (120) specimens were prepared , the specimens were divided into four groups according to the material had been added (one control and three for Al2O3, TiO2 and SiO2nanocomposite) each group was subdivided in to three groups according to the test had been done on it, the degree of transition (Tg) was measured by The d
... Show MoreBackground: During acrylic resin processing, the mold must be separated from the surface of the gypsum to prevent liquid resin from penetrating into the gypsum, and water from the gypsum seeping into the acrylic resin. For many years, tin foil was the most acceptable separating medium, and because it's difficult to apply, a tin-foil substitute is used. In this study, olive oil is used as an alternative to tin foil separating medium for first time, and evaluating its effect as a separating medium on some mechanical properties such as (indentation hardness and transverse strength) of acrylic resins denture base comparing it with those processed using tin-foil and tin foil substitute such as (cold mold seal) separating medium. Materials and M
... Show MoreBackground: The main drawback of soft lining materials was that they debonded from the denture base after a certain period of usage. Therefore, the purpose of this research was to determine the impact of oxygen and argon plasma treatment on the shear bonding strength of soft liners to two different kinds of denture base materials: conventional acrylic resin and high impact acrylic resin. Materials and Methods: Heat cure conventional and high impact acrylic blocks (40 for each group) were prepared. A soft liner connected the final test specimen of two blocks of each acrylic material. Shear bond strength (SBS) was assessed using universal testing machine. Additional blocks were also prepared for analyzing Vickers microhardness, contact ang
... Show MoreBackground: Denture cleansing is an important step that can prevent the spread of infection and improve a patient's health, the durability of the dentures, and the overall quality of life; therefore, it is necessary to choose a suitable cleanser that, in addition to being effective, does not have an unfavorable effect on the qualities of the denture base resin itself when used for an extended period. Aim: This research aims to assess the effects of ozonated water on the surface roughness and hardness of heat-cured acrylic resin by immersion technique. Materials: Sixty bars shapemade of heat-cured acrylicweremanufactured.Thirty samples for every test, including: (surface hardness and surface roughness). Then, these samples were divided into
... Show MoreBackground: Poly (methylmethacrylate) is the most widely used material in denture fabrication. The characteristics of acrylic resin which support microorganism development can threaten the oral health of denture users. This study was assigned to prepareand incorporate Ag-Zn zeolite powder into heat cured denture base material as antimicrobial material and to investigate its effect on some properties of heat cured acrylic denture base materials. Materials and methods: Sliver –zinc zeolite was prepared by ion exchange method and characterized then incorporated into poly (methylmethacrylate) powder in0.5% by weight. Specimens were constructed and divided into 6 groups according to the using tests; each group was subdivided into 2 groups
... Show MoreBackground: The purpose of this study was to verify the influence of post- pressing time of acrylic resin (immediate, 6, 12 and 24 hour) on the dimensional accuracy of denture base whish is a critical factor in the retention and stability of the complete denture that may occur during polymerization shrinkage. Materials and Methods: Forty maxillary stone casts were poured in plastic mold (Columbia Dentoform corp. NEW YORK, type III dental stone (Geastone, Zeus Sri Loc.Tamburine Roccastrada, GR, Italy). The stone casts were randomly assigned into 4 groups of 10 specimens each according to the post-pressing times into (immediate, 6, 12 and 24 h.). Heat cure acrylic resin denture base was constructed according to the previously mentioned pressi
... Show MoreBackground: The longevity of any prosthesis depends on the materials from which it was fabricated, that is why, defects in the material properties may reduce the service life of prosthesis and necessitate its replacement. The aim of this study was to evaluate the effect of adding different concentrations of Polyamide-6 (Nylon-6) on the tear and tensile strength of A-2186 RTV silicone elastomer. Materials and Methods: 80 samples were fabricated by the addition of 0%, 1%, 3% and 5% by weight PA-6 micro-particles powder to A-2186 platinum RTV silicone elastomer. The study samples were divided into four (4) groups, each group containing 20 samples. One control group was prepared without PA-6 micro particles and three experimental groups were pr
... Show More