Background: Dental implants act as infrastructure for fixed restoration to look like as a natural tooth. Osseointegration is a biological events and considered as a base for success of dental implant. The aim of this study is to evaluate the bond strength between bone and Ti implant coated with mixture of nano hydroxyapatite-chitosan-collagen compared with Ti implants coated with nano hydroxyapatite implanted in rabbit tibia, after different period of implantation time (two and six weeks) by torque removal test. Material and methods: 36 screws of commercially pure titanium; 8mm in length and 3mm diameter , 18 screws coated with mixture of nano hydroxyapatite-chitosan-collagen and18 screws coated with nano hydroxyapatite by dip coating. Structural characteristics was assessed by scanning electron microscope, and FTIR analysis. The screws were implanted in 18 healthy adult male New Zeeland rabbits each tibia received one screw, right tibia received screw coated with nano hydroxyapatite while left tibia received screw coated nano hydroxyapatite-chitosan-collagen composite. Removal torque test was done by torque meter to determine the highest torque value necessary to remove the implants from tibia bone after different period of time of implantation(2 and 6 weeks). Result: Nano hydroxyapatite-chitosan-collagen composite coating was resulting in higher torque removal value than nano hydroxyapatite coating for two periods of time. Conclusion: Concluded that addition of collagen and chitosan to nano hydroxyapatite was more efficient in rapid bone formation than nano hydroxyapatite only.
Background: Poly-ether-ether-ketone(PEEK) has been introduced to many dental fields. Recently it was tested as a retainer wire‎ following orthodontic treatment. This study aimed to investigate the effect of changing the bonding spot size and location on the performance of PEEK retainer wires. Methods: A biomechanical study involving four three-dimensional finite element models was performed. The basic model was with a 0.8 mm cylindrical cross-section PEEK wire, bonded at the center of the lingual surface of the mandibular incisors with 4 mm in diameter composite spots. Two other models were designed with 3 mm and 5 mm composite sizes. The last model was created with the composite bonding spot of the canine away from the center
... Show More 
The objective of this study is to demonstrate the corrosion behavior of dental alloys Co-Cr-Mo, Ni-Cr-Mo and Ti-Al-V in artificial saliva at pH=4 and 37oC enriched with ethyl alcohol at 8% percentage. The linear and cyclic polarizations were investigated by electrochemical measurements. Laser surface modification was achieved for the three dental alloys to improve corrosion resistance. The results show that corrosion resistance of Co-Cr-Mo and Ni-Cr-Mo alloys only were increased after laser treatment due to the fact that laser radiation has caused a smoother surface, in addition to the decrement in corrosion current densities (icorr) for Co-Cr-Mo and Ni-Cr-Mo alloys and the reverse scan in cyclic polarization became in the wider range of
... Show MoreBurnishing improves fatigue strength, surface hardness and decrease surface roughness of metal because this process transforms tensile residual stresses into compressive residual stresses. Roller burnishing tool is used in the present work on low carbon steel (AISI 1008) specimens. In this work, different experiments were used to study the influence of feed parameter and speed parameter in burnishing process on fatigue strength, surface roughness and surface hardness of low carbon steel (AISI 1008) specimens. The first parameter used is feed values which were (0.6, 0.8, and 1) mm at constant speed (370) rpm, while the second parameter used is speed at values (540, 800 and 1200) rpm and at constant feed (1) mm. The results of the fatigue
... Show MoreConfigured binary polymer blends of epoxy and Polyurethane was chosen varying proportions of these materials led to the production of homogeneous mixtures of Althermust Althermust and descent was poured polyurethane models required in the form of 4 mm thick plates
The printed circuit heat exchanger is a plate type heat exchanger with a high performance and compact size. Heat exchangers such as this need a unique form of bonding and other techniques to be used in their construction. In this study, the process of joining plates, diffusion bonding, was performed and studied. A special furnace was manufactured for bonding purposes. The bonding process of copper metal was carried out under specific conditions of a high temperature up to 700 oC, high pressure of 3.45 MPa, and in an inert environment (Argon gas) to make tensile samples. The tensile samples are cylindrical shapes containing groves representing the flow channels in the printed circuit heat exchanger and checking their tensile st
... Show MoreThis contribution investigates the effect of the addition of the Hubbard U parameter on the electronic structural and mechanical properties of cubic (C-type) lanthanide sesquioxides (Ln2O3). Calculated Bader's charges confirm the ionic character of Lnsingle bondO bonds in the C-type Ln2O3. Estimated structural parameters (i.e., lattice constants) coincide with analogous experimental values. The calculated band gaps energies at the Ueff of 5 eV for these compounds exhibit a non-metallic character and Ueff of 6.5 eV reproduces the analogous experimental band gap of cerium sesquioxide Ce2O3. We have thoroughly investigated the effect of the O/Ce ratios and the effect of hafnium (Hf) and zirconium (Zr) dopants on the reduction energies of C
... Show MoreIn this work, the effect of atomic ratio on structural and optical properties of SnO2/In2O3 thin films prepared by pulsed laser deposition technique under vacuum and annealed at 573K in air has been studied. Atomic ratios from 0 to 100% have been used. X-ray diffraction analysis has been utilized to study the effect of atomic ratios on the phase change using XRD analyzer and the crystalline size and the lattice strain using Williamson-Hall relationship. It has been found that the ratio of 50% has the lowest crystallite size, which corresponds to the highest strain in the lattice. The energy gap has increased as the atomic ratio of indium oxide increased.
Background: Osteoporosis is a systemic skeletal disorder affects general health in addition to effect on salivary physical and chemical composition which lead to an adverse effect on oral health status. This study was conducted to evaluate the concentration of glycoprotein (osteonectin) in saliva and its effect on dental caries in relation to salivary flow rate and viscosity among osteoporotic women and compared to control group. Materials and Methods: The total sample composed of 60 females aged 60-65 years attending Al-Yarmook Teaching Hospital, 30 females diagnosed with osteoporosis by measuring bone density at the spine and femur with a dual-energy X-ray absorptiometry at T-score of >2.5, and 30 women without osteoporosis with T-score o
... Show MoreThis study provides valuable information on secondary microbial infections in H1N1 patients compared to Seasonal Influenza in Iraqi Patients. Nasopharynx swabs were collected from (12 ) patients infected with Seasonal influenza (11 from Baghdad and 1 Patient from south of Iraq) ,and ( 22 ) samples from patients with 2009 H1N1 ( 20 from Baghdad and 2 from south of Iraq). The results show that the patients infected with 2009 H1N1 Virus were younger than healthy subjects and those infected with seasonal influenza. And the difference reached to the level of significance (p< 0.01) compared with healthy subjects.Two cases infected with 2009 H1N1 virus (9.1%) were fro