Background: Dental implants act as infrastructure for fixed restoration to look like as a natural tooth. Osseointegration is a biological events and considered as a base for success of dental implant. The aim of this study is to evaluate the bond strength between bone and Ti implant coated with mixture of nano hydroxyapatite-chitosan-collagen compared with Ti implants coated with nano hydroxyapatite implanted in rabbit tibia, after different period of implantation time (two and six weeks) by torque removal test. Material and methods: 36 screws of commercially pure titanium; 8mm in length and 3mm diameter , 18 screws coated with mixture of nano hydroxyapatite-chitosan-collagen and18 screws coated with nano hydroxyapatite by dip coating. Structural characteristics was assessed by scanning electron microscope, and FTIR analysis. The screws were implanted in 18 healthy adult male New Zeeland rabbits each tibia received one screw, right tibia received screw coated with nano hydroxyapatite while left tibia received screw coated nano hydroxyapatite-chitosan-collagen composite. Removal torque test was done by torque meter to determine the highest torque value necessary to remove the implants from tibia bone after different period of time of implantation(2 and 6 weeks). Result: Nano hydroxyapatite-chitosan-collagen composite coating was resulting in higher torque removal value than nano hydroxyapatite coating for two periods of time. Conclusion: Concluded that addition of collagen and chitosan to nano hydroxyapatite was more efficient in rapid bone formation than nano hydroxyapatite only.
Abstract: In this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
Background: The insertion torque (IT) values and implant stability quotient (ISQ) values are the measurements most used to assess primary implant stability. This study aimed to assess the relationship between ISQ values and IT. Materials and methods: This study included 24 patients with a mean (SD) age of 47.9 (13.64) years (range 25-75 years). The patients received 42 dental implants (DI), 33 in the mandible and 9 in the maxilla. The DI were installed using the motorized method with 35 Ncm torque, When DI could not be inserted to the requisite depth by the motorized method, a hand ratchet was used and the IT was recorded as ˃ 35 Ncm. Implant stability was measured utilizing Osstell® ISQ. The secondary stability was measured after 16
... Show MoreBackground: Glass ionomers have good biocompatibility and the ability to adhere to both enamel and dentin. However, they have certain demerits, mainly low tensile and compressive strengths. Therefore, this study was done to assess consistency and compressive strength of glass ionomer reinforced by different amount of hydroxyapatite. Materials and Methods: In this study hydroxyapatite materials were added to glass ionomer cement at different ratios, 10%, 15%, 20%, 25% and 30% (by weight). The standard consistency test described in America dental association (ADA) specification No. 8 was used, so that all new base materials could be conveniently mixed and the results would be of comparable value and the compressive strength test described by
... Show MoreSludge from stone-cutting (SSC) factories and stone mines cannot be used as decorative stones, stone powder, etc. These substances are left in the environment and cause environmental problems. This study aim is to produce artificial stone composite (ASC) using sludge from stone cutting factories, cement, unsaturated resin, water, silicon carbide nanoparticles (SiC-NPs), and nano-graphene oxide (NGO) as fillers. Nano graphene oxide has a hydrophobic plate structure that water is not absorbed due to the lack of surface tension on these plates. NGO has a significant effect on the properties of artificial stone due to its high specific surface area and low density in the composite. Its uniform distribution in ASC is very low due to its hydropho
... Show MoreBackground: Polishing technique for acrylic resin material have great effect on properties of acrylic material and bacterial colonization such as staphylococcus aurous, which are responsible for many acrylic prosthetic infections such as the commonly ocular infections. Ineffective polishing technique could affect roughness and subsequently porosity of acrylic materials.So, a new effective method for polishing acrylic was used depending on the use of optiglaze coating material. So, this study aimed to evaluate the effect of optiglaze polishing on porosity of acrylic resin material and staphylococcus aurous activity in comparison to conventional polishing technique.
Materials and methods: Specimen(n=120) were prepared :20 spe
... Show MoreJava is a high-level , third generation programming language were introduced Javaoptics Open Source Physics (OSP) as a new simulation for design one of the most important interference optical coating called antireflection coating. It is recent developments in deign thin-film coatings. (OSP) shows multiple beam interferences from a parallel dielectric thin film and the evolution of reflection factors. It is simple to use and efficiently also can serve educational purposes. The obtained results have been compared with needle method
Industrial and urban development has resulted in the spread of plastic waste and the increase in the emissions of carbon dioxide resulting from the cement manufacturing process. The current research aims to produce green (environmentally friendly) concrete by using plastic waste as coarse aggregates in different proportions (10% and 20%) and nano silica sand powder as an alternative to cement in different proportions (5% and 10% by weight). The results showed that compressive strength decreased by 12.10% and 19.23% for 10% and 20% plastic waste replacement and increased by 12.89% and 20.39% for 5% and 10% silica sand replacement respectively at 28 days. Flexural strength decreased by 12.95% and 19.64% for 10% and 20% plastic waste r
... Show MoreAbstract-Industrial and urban development has resulted in the spread of plastic waste and the increase in the emissions of carbon dioxide resulting from the cement manufacturing process. The current research aims to produce green (environmentally friendly) concrete by using plastic waste as coarse aggregates in different proportions (10% and 20%) and nano silica sand powder as an alternative to cement in different proportions (5% and 10% by weight). The results showed that compressive strength decreased by 12.10% and 19.23% for 10% and 20% plastic waste replacement and increased by 12.89% and 20.39% for 5% and 10% silica sand replacement respectively at 28 days. Flexural strength decreased by 12.95% and 19.64% for 10% and 20% plastic waste
... Show MoreBack ground: Glass ionomer materials lack resistance to wear and pressure and are susceptible to moisture during the initial stages of setting and dehydration. So this study was done to assess diametral tensile strength and microhardness of glass ionomer reinforced by different amounts of hydroxyapatite. Materials and methods: In this study a hydroxyapatite material was added to glass monomer cement at different ratios: 10%, 15%, 20%, 25% and 30% (by weight). The diametral tensile strength test described by the British standard specification for zinc polycarboxylate cement was used in this study and the microhardness test was performed using Vickers microhardness testing machine and the microhardness values were calculated and statistical c