Background: This study was performed to compare the marginal fit changes and facture resistance of metal ceramic crowns constructed from Ceramill Sintron metal coping veneered with three different porcelain veneering materials (Vita Master Koromikos VMK, Willi Geller Creation CC and GC initial MC), also to evaluate the influence of thermocycling on load at fracture. Materials and Methods: Master brass die was scanned ,then metal coping was designed and milled from Ceramill Sintron blank to get 60 metal copings, then divided randomly into three groups(20 sample), then veneered with porcelain: VITA, Creation or GC. The marginal gaps were measured before and after porcelain veneering then marginal fit changes was calculated. Fracture resistance test was done by Instron®, the master die was duplicated to sixty analogs then each analog was fixed into acrylic base. After that each crown was cemented onto the corresponding die analog. Ten samples of each group were subjected to compressive loading to fracture and other ten subjected to thermocycling followed by compressive loading to fracture. Result and Conclusion: The result of marginal fit changes showed that GC group had the lowest marginal gap follow by VITA and Creation. While VITA group showed the highest fracture resistance follows by GC then Creation. Thermocycling process did not significantly reduce the load at fracture for all groups.
Prostheses are used as an alternative to organs lost from the body. Flex-Foot Cheetah is considered one of the lower limb prostheses used in high-intensity activities such as running. This research focused on testing two samples of Flex-Foot Cheetah manufactured of two various materials (carbon, glass) with polyester and compare between them to find the foot with the best performance in running on the level of professional athlete. In the numerical analysis, the maximum principal stress, maximum principal elastic strain, strain energy; finally, the blade total deformation were calculated for both feet. In experimental work, the load-deflection test was done for foot to calculate the bending the results were very close to
... Show MoreBackground: The success and maintenance of indirect dental restorations is closely related to the marginal accuracy, which is affected by many factors like preparation design, using of different fabrication techniques, and the time of taking final impression and pouring it. The purpose of this in vitro study was to evaluate the effect of different pouring time of conventional impression on the vertical marginal gap of full contour zirconia crowns in comparison with digital impression technique. Materials and Methods: Forty sound recently extracted human permanent maxillary first premolar teeth of comparable size and shape were collected. Standardized preparation of all teeth samples were carried out to receive full contour zirconia crown re
... Show MoreBackground: The success and maintenance of indirect dental restorations is closely related to the marginal accuracy, which is affected by many factors like preparation design, using of different fabrication techniques, and the time of taking final impression and pouring it. The purpose of this in vitro study was to evaluate the effect of different pouring time of conventional impression on the vertical marginal gap of full contour zirconia crowns in comparison with digital impression technique. Materials and Methods: Forty sound recently extracted human permanent maxillary first premolar teeth of comparable size and shape were collected. Standardized preparation of all teeth samples were carried out to receive full contour zirconia crown re
... Show MoreAim: The reduction in the amount of marginal bone is the most important demand for the long term success of dental implants. This prospective clinical study was aimed to investigate the marginal bone loss of early loaded SLActive implants with different dimensions and surgical approaches. Materials and methods Fifteen patients aged from 18 to 60 years were divided into 2 groups (flapped and flapless approach) that underwent delayed implant placement protocol with SLActive implants. The marginal bone level was estimated by cone-beam computed tomography during three different periods: preoperatively, 8 weeks after surgery and 24 weeks after loading of the prosthesis. Results: The mean value of marginal bone level was not significantly chan
... Show MoreThis research studies the possibility of producing Bone China with available local and geological substitutes and other manufactured ones since it’s traditionally produced by Bone ash, Cornish stone, and China clay, while the substitutes are Kaolin instead of China clay and Feldspar potash instead of Cornish stone. Because of the unavailability of Feldspar in Iraq, it was substituted with the manufactured alternative Feldspar. Bone ash was prepared from cow bones with heating treatments, grinding and sifting. The alternative Feldspar was prepared by chemical analysis of the natural Feldspar potash with local materials that include Dwaikhla Kaolin, Urdhuma Silica sand, Potassium Carbonate, and Sodium Carbonate. The mixture was burned at
... Show MoreThe problem in the design of a cam is the analyzing of the mechanisms and dynamic forces that effect on the family of parametric polynomials for describing the motion curve. In present method, two ways have been taken for optimization of the cam size, first the high dynamic loading (such that impact and elastic stress waves propagation) from marine machine tool which translate by the roller follower to the cam surface and varies with time causes large contact loads and second it must include the factors of kinematics features including the acceleration, velocity, boundary condition and the unsymmetrical curvature of the cam profile for the motion curve.
In the theoretical solution
... Show MoreObjective: This study evaluated the effect of immediate dentin sealing on the marginal adaptation of lithium disilicate overlays with three different types of resin-luting agents: preheated composite, dual-cure adhesive resin, and flowable composite. Materials and Methods: Forty-eight maxillary first premolars of similar size were prepared with a butt joint preparation design. The teeth were separated into two primary groups, each with twenty-four teeth: Group DDS: Delay dentin sealing (non-IDS) teeth were not treated. Group IDS: dentin sealing was applied immediately after teeth preparation. Each group was subsequently separated into three separate subgroups. Subgroups (DDS+Phc, IDS+Phc): cemented with preheated composite (Enamel plus HRi,
... Show MoreBackground: Denture lining materials are widely used in prosthodontic treatment and management of traumatized oral mucosa. A contaminated prosthesis can provide a source of cross-contamination between patients and dental personnel as well as a cause for denture stomatitis. Therefore, denture disinfection has been recommended as an essential procedure for maintenance of a healthy oral mucosa. This study investigated the effect of SOLO disinfectant solution on some properties of different denture lining materials. Materials and methods: Three different solutions were used in this study; SOLO disinfectant solution, sodium hypochlorite solution, and water on three types of acrylic denture lining materials; hot cure, cold cure, and soft acrylic
... Show More