ABSTRACT Background:Hydrogen absorption and related degradation in the mechanical properties of Ni-Ti based orthodontic wires has been demonstrated following exposure to fluoride prophylactic agents. This study was designed to investigate the effects of three fluoride containing agents on the load deflection characteristics of heat activated nickel titanium arch wires during unloading phase. Material and method: Eighty specimens of heat activated nickel titanium arch wires were obtained from Ortho Technology Company, half of which had a 0.016 inch round and 0.019x0.025 rectangular. Ten specimens from both wire size were immersed in one of the tested fluoride prophylactic agents (neutral sodium fluoride gel, stannous fluoride gel or phos-flur mouth rinse) or in the controlled medium “normal salineâ€, and incubated at 37ËšC for sixty minutes. A Wp 300 universal material testing machine was modified and used to perform a three point bending test in a water path at 37ËšC ±1ËšC.The statistical difference between the different agents were analyzed using ANOVA and LSD tests. Results: The unloading forces at 0.5, 1.0, and 1.5 mm where significantly reduced especially in neutral sodium fluoride treated specimens. Conclusion: Based on the results founded in th study it might be preferred to use prophylactic agent with the least fluoride ions concentration.It can be concluded that the tested agents have only a limited effect on the load deflection behavior of the heat activated Ni-Ti wires, in a way that they do not have a clinically significant effect on the mechanical behavior of these wires.
Background: Even the wide use of dental implants, still there is a proportion of implants are failed due to infection. Much considerable attention has been paid to modify the implant surface. Coating of dental implant with a biocomposite material of suitable properties can improve osseointegration. And this is the main concern of this study. The aim of present study was to evaluate the use of a biocomposite coating of dental implant with (ceramic nano Al2O3 and metalic AgNo3) on the bond strength at bone – implant interface and tissue reaction. Materials and methods: A total number of forty-eight screws, CpTi dental implant used in this study. Half of these screws were coated with a biocomposite material of nano (Al2O3and AgNo3), thi
... Show MoreBackground: Endodontically treated teeth have low resistance to fracture against occlusal forces. The strengthening effect of bonded esthetic onlay restoration on weakened tooth has been reported. This study aimed to assess the fracture resistance of endodontically treated premolars restored with composite with and without cuspal coverage by using direct and indirect techniques. Indirect technique done by CAD/CAM system (computer aided design –computer aided manufacturer) and laboratory processing. Material and methods: Forty human extracted maxillary premolars of approximately comparable sizes were divided into four groups: Group (A): Ten endodontically treated teeth directly filled with Filtek Z250xt without cuspal coverage. Group
... Show MoreBackground: This study was conducted to assess the effects of various beverages on the shear bond strength of light-cured orthodontic composite used to bond stainless steel orthodontic brackets on human teeth and to determine the site of bonding failure of this material. Materials and Methods: Fifty extracted human premolars were selected and randomly divided into five equal groups each with 10 teeth according to the beverage type (Control, One Tiger, Milk, Green tea and Coffee). After bonding, the teeth were immersed in specific beverages for 5 minutes twice daily with equal intervening intervals then washed and stored in distilled water at 37º C for the reminder of the day. The process was carried out for 30 days. The samples were then
... Show MoreIn the present research, the electrical properties which included the ac-conductivity (σac), loss tangent of dielectric (tan δ) and real dielectric constant (ε’) are studied for nano polycarbonate in different pressures and frequencies as a function of temperature these properties were studied at selective temperature gradients which are (RT-50-100-150-250)°C. The results of the study showed that the values of dielectric constant and dissipation factor increase with increasing pressure and temperature and decreases by increasing frequency. And the results of electrical conductivity showed that it increases with increasing temperature, pressure and frequency.
Different parameters of double pipe helical coil were investigation experimentally. Four coils were used; three with a curvature ratio (0.037, 0.031, and 0.028) and 11mm diameter of the inner tube while the fourth with 0.033 curvature ratio and 13 mm diameter of the inner tube. The hot water flow in the inner tube whereas the cold water flows in the annulus. The inlet temperatures of hot and cold water are 50 0C and 18 0C respectively. The inner mass flow rate ranges from 0.0167 to 0.0583 kg/s. The results show the Nusselt number increase with increase curvature ratio. The Nusselt number of the coil with 0.037 curvature ratio increases by approximately 12.3 % as compare with 0.028 curvature ratio. The results also r
... Show MoreBackground: The study aim was to evaluate thermocycling effect on microleakage of occlusal and cervical margins of MOD cavity filled with bulk filled composites in comparison to incrementally placed nanohybrid composite and to evaluate the difference in microleakage between enamel and dentin margins for the three materials groups. Materials and method: Forty eight maxillary first premolars were prepared with MOD cavities. Samples were divided into three groups of sixteen teeth according to material used: Grandio: Grandio. SDR: SDR +Grandio. X-tra: X-tra base + Grandio. Each group was subdivided into two according to be thermocycled or not. After 24 hrs immersion in 2% methylene blue, samples weresectioned and microleakage was estimated. Res
... Show MoreThe fouling depositions of crude oil stream were studied theoretically in a shell and tube heat exchanger to investigate the effect of depositions on the heat transfer process. The employed heat exchanger was with steam flowing in the inner tubes and crude oil in the shell at different velocities and bulk temperatures. It is assumed that fouling occurs only on the heated stream side (crude oil). The analysis was carried out for turbulent flow heat transfer conditions with wide range of Reynolds number, bulk temperature and time. Many previously proposed models for fouling resistance were employed to estimate a new model for fouling rate. It is found that the fouling rate and consequently the heat transfer coefficient were affected by Rey
... Show MoreThe Mishrif reservoir (Cenomanian - Turonian) in the Z, H, B and N oilfields in southern Iraq was investigated to clarify how nickel, vanadium, asphaltene, NSO and sulfur content affect the crude oil quality. The GC-Mass and ICP-MS analyses were used to provide fruitful hydrocarbon results. Classification of crude oil based on API gravity broadly indicates the oil's density and general properties. Typically, lighter crude oils are easier to refine, yield higher percentages of valuable products such as gasoline and diesel, and have a higher market value. Heavier crude oils require more processing and may yield more residual products, such as heavy fuel oil and asphalt. The Mishrif crude oil was classified as a medium sour crude oil c
... Show MoreBackground: Poly-ether-ether-ketone(PEEK) has been introduced to many dental fields. Recently it was tested as a retainer wire‎ following orthodontic treatment. This study aimed to investigate the effect of changing the bonding spot size and location on the performance of PEEK retainer wires. Methods: A biomechanical study involving four three-dimensional finite element models was performed. The basic model was with a 0.8 mm cylindrical cross-section PEEK wire, bonded at the center of the lingual surface of the mandibular incisors with 4 mm in diameter composite spots. Two other models were designed with 3 mm and 5 mm composite sizes. The last model was created with the composite bonding spot of the canine away from the center of t
... Show More