ABSTRACT Background: Piezosurgery device is a system developed recently to overcome the limitation of the traditional surgical technique in implant site preparation, which use the principle of ultrasonic microvibrations to create precise & selective cut in bone in harmony with the surrounding tissues. The aim of this study was to evaluate the outcomes of implants inserted by ultrasonic implant site preparation protocol (UISP) using piezosurgery device, regarding the survival rate, stability and other related factors, at 16 weeks postoperative follow up period. Materials and Methods: A total of (24) patients, (6) males and (18) females, aged between (19-51) years old, contributed in this study receiving a total of (42) implants, all of these implants bed were prepared by means of special tips mounted in piezosurgery device. For each patient thorough clinical and radiographical preoperative assessment was applied. Implant stability quotient (ISQ) values were measured at baseline, 8 weeks and at 16 weeks. Postoperative clinical and radiographic evaluation was applied for each patient for 16 weeks postoperatively. Results: (24) patients received (42) implants accomplished the follow-up period, After 16 weeks all implants (42) were osseointegrated and the overall implants survival rate was 100% with no failure and no complication was observed. The mean ISQ value at baseline was (74.32±6.42), the mean ISQ value at 8 weeks was (72.62±9.05) and at 16 weeks the mean ISQ (±SD) value was (76.68±7.35) the changes in the mean stability during the healing period showed significant increase in the implant stability (P≤0.05). At the 16th week the number of implants that achieved ISQ≥70 was 35 (83.3%), and 7 implants attained ISQ> 70 (16.7%). Conclusions: high and significant survival rate, significant secondary stability, early positive shifting of the mean ISQ value, no remarkable complications in implants inserted by ultrasonic implant site preparation indicated that piezosurgery is a reliable alternative and safe method used in dental implant osteotomy.
TiO2 thin films have been deposited at different concentration of
CdO of (x= 0.0, 0.05, 0.1, 0.15 and 0.2) Wt. % onto glass substrates
by pulsed laser deposition technique (PLD) using Nd-YAG laser
with λ=1064nm, energy=800mJ and number of shots=500. The
thickness of the film was 200nm. The films were annealed to
different annealing (423 and 523) k. The effect of annealing
temperatures and concentration of CdO on the structural and
photoluminescence (PL) properties were investigated. X-ray
diffraction (XRD) results reveals that the deposited TiO2(1-x)CdOx
thin films were polycrystalline with tetragonal structure and many
peaks were appeared at (110), (101), (111) and (211) planes with
preferred orientatio
A thermal evaporation technique was used to prepare ZnO thin films. The samples were prepared with good quality onto a glass substrate and using Zn metal. The thickness varied from (100 to 300) ±10 nm. The structure and optical properties of the ZnO thin films were studied. The results of XRD spectra confirm that the thin films grown by this technique have hexagonal wurtzite, and also aproved that ZnO films have a polycrystalline structure. UV-Vis measurement, optical transmittance spectra, showed high transmission about 90% within visible and infrared range. The energy gap is found to be between 3.26 and 3.14e.V for 100 to 300 nm thickness respectivly. Atomic Force Microscope AFM (topographic image ) shows the grain size incre
... Show MoreMixed phase rutile/anatase of TiO2 was prepared and studied by a closed field DC magnetron sputtering configuration (CFDCMS). It was found that the contents of rutile increased from the ratio of 38% to 53% as the deposition time increased from 3.5 hours to 4.5 hours.
The photocatalytic activity of the mixed phase rutile/anatase TiO2 was measured by monitoring the degradation of the blue methylene dye in an aqueous solution, under exposure to UV-radiation, using UV-vis absorption spectroscopy. It was proven that the photocatalytic activity in the mixed phase (TiO2) is a function of rutile content reaching a maximum value at 53% rutile. Thus, the effect of synergy between anatase- TiO2 and rutile- TiO2 was observed. It was observed that
Cr2O3 thin films have been prepared by spray pyrolysis on a glass substrate. Absorbance and transmittance spectra were recorded in the wavelength range (300-900) nm before and after annealing. The effects of annealing temperature on absorption coefficient, refractive index, extinction coefficient, real and imaginary parts of dielectric constant and optical conductivity were expected. It was found that all these parameters increase as the annealing temperature increased to 550°C.
Zinc Oxide transparent thin films (ZnO) with different thickness from (220 to 420)nm
±15nm were prepared by thermal evaporation technique onto glass substrates at 200 with
the deposition rate of (10 2) nm sec
-1
, X-ray diffraction patterns confirm the proper phase
formation of the material. The investigation of (XRD) indicates that the (ZnO) film is
polycrystalline type of Hexagonal and the preferred orientation along (002) plane. The Optical
properties of ZnO were determined through the optical transmission method using ultraviolet-visible spectrophotometer with wavelength (300 – 1100) nm. The optical band gap values of
ZnO thin films were slightly increased from (2.9 - 3.1) eV as the film thickn
The electrical properties of pure NiO and NiO:Au Films which are
deposited on glass substrate with various dopant concentrations
(1wt.%, 2wt%, 3wt.% and 4wt.%) at room temperature 450 Co
annealing temperature will be presented. The results of the hall effect
showed that all the films were p-type. The Hall mobility decreases
while both carrier concentration and conductivity increases with the
increasing of annealing temperatures and doping percentage, Thus,
indicating the behavior of semiconductor, and also the D.C
conductivity from which the activation energy decrease with the
doping concentration increase and transport mechanism of the charge
carriers can be estimated.
In this study, the potential of adsorption of amoxicillin antibiotic (AMOX) from aqueous solutions using prepared activated carbon (AC) was studied. The used AC was prepared from an inexpensive and available precursor (sunflower seed hulls (SSH)) and activated by potassium hydroxide (KOH). The prepared AC was examined for its ability to remove AMOX from aqueous contaminated solutions and characterized with the aid of N2 -adsorption/desorption isotherm Brunauer–Emmett– Teller, scanning electron microscopy, energy-dispersive X-ray spectroscopy and Fourier-transform infrared. Zeta potential of the prepared activated carbon from sunflower seed hulls (SSHAC) were studied in relation to AMOX adsorption. The physical and chemical propert
... Show MoreChromium oxide (Cr2O3) doped ZnO nanoparticles were prepared by pulsed laser deposition (PLD) technique at different concentration ratios (0, 3, 5, 7 and 9 wt %) of ZnO on glass substrate. The effects of ZnO dopant on the average crystallite size of the synthesized nanoparticles was examined By X-ray diffraction. The morphological features were detected using atomic force microscopy (AFM). The optical band gap value was observed to range between 2.78 to 2.50 eV by UV-Vis absorption spectroscopy, with longer wavelength shifted in comparison with that of the bulk Cr2O3 (~3eV). Gas sensitivity, response, and recovery times of the sensor in the presence of NH3
... Show MoreIn this work, metal oxide nanostructures, mainly copper oxide (CuO), nickel oxide (NiO), titanium dioxide (TiO2), and multilayer structure, were synthesized by the DC reactive magnetron sputtering technique. The effect of deposition time on the spectroscopic characteristics, as well as on the nanoparticle size, was determined. A long deposition time allows more metal atoms sputtered from the target to bond to oxygen atoms and form CuO, NiO, or TiO2 molecules deposited as thin films on glass substrates. The structural characteristics of the final samples showed high structural purity as no other compounds than CuO, NiO, and TiO2 were found in the final samples. Also, the prepared multilayer structures did not show new compounds other than th
... Show More