ABSTRACT Background: Improving the properties of heat- cured and self-cured acrylic resin have been studied by many researchers. However, little studies concerned with visible light cured resin (VLCR) improved through addition of nanofiller are available. The purpose of this study was to evaluate some properties of (VLCR) after addition of SiO2 nanofiller. Materials and Methods: SiO2 nanofiller were added to (VLCR) tray material after being dissolved in tetrahydrofuran (THF) solvent. According to the pilot study 2% SiO2 nanofiller addition exhibited better properties than the other percentages (1%, 3%). The main study conducted involved (100) specimens divided into 5 groups according to the test included. (20) Specimens were selected for each test (10 samples for the control group and 10 samples for the experimental 2% SiO2 nanofiller group). The properties investigated were transverse strength, impact strength, surface hardness, surface roughness, water sorption and solubility. Scanning electron microscope (SEM) and energy dispersive spectroscopy (EDS) were used to assess nanofiller distribution and identification of elements. The data were subjected to descriptive statistical analysis and independent sample t-test. Results: The mean value of transverse strength of experimental group increased significantly, while the impact strength of experimental group decreased significantly when compared to control group. A significant increase in surface hardness was noticed in the experimental group, while non-significant increase in surface roughness was observed. The water sorption values were decreased significantly, while a non-significant decrease in water solubility was observed in the experimental group. Conclusion: Addition of SiO2 nanofiller to (VLCR), slightly improve the transverse strength and surface hardness, while water sorption and solubility slightly decreased. The impact strength was significantly deteriorated, while the surface roughness shows non-significant increment.
A sensitive, accurate, and affordable colorimetric method was developed for assaying prednisolone (PRZ) in various medicinal forms. The procedure involves the oxidation of PRZ by ferric ions, followed by complexation of the resulting ferrous ions with ferricyanide to produce a greenish-blue product. Common complexation conditions were thoroughly investigated. The mole ratio of FeCl₃·6H₂O to K₃Fe(CN)₆ was 8:1. The proposed mechanism of complexation was suggested and considered. Various parameters were optimized, including the reduction of the colorimetric reaction temperature to 50°C and the duration of heating and analysis to 20-30 minutes. The calibration curve was linear over the range of 1-60 µg/mL. The limit of detection (LOD
... Show MoreIn this paper the reinforced materials manufactured from steel continues fibers are used in Aluminum matrix to build a composite material. Most of researches concentrated on reinforced materials and its position in the matrix according to its size and distribution, and their effects on the magnitude of different kinds of the stresses, so this paper presents and concentrate on the geometrical shape of reinforced material and its effects on the internal stresses and strains on the composite strength using FEM as a method for analysis after loaded by certain force showing the deference magnitudes of stresses according to the different geometrical shapes of reinforced materials.
This study is concerned with the effect of adding two kinds of ceramic materials on the mechanical properties of (Al-7%Si- 0.3%Mg) alloy, which are zirconia with particle size (20μm > P.S ≥ 0.1μm) and alumina with particle size (20μm > P.S ≥ 0.1μm) and adding them to the alloy with weight ratios (0.2, 0.4, 0.6, 0.8 and 1%). Stirring casting method has been used to make composite material by using vortex technique which is used to pull the particles to inside the melted metals and distributed them homogenously.
After that solution treatment was done to the samples at (520ºC) and artificial ageing at (170ºC) in different times, it has been noticed that the values of hardness is increased with the aging time of the o
... Show MoreDue to the rapid advancement of technology and the technology of things, modern industries start to need a highprecision equipment and surface finishing, so many finishing processes began to develop. One of the modern processes is Magnetic Abrasive Finishing (MAF), which is a high-precision process for internal and external finishing under the influence of a magnetic field of abrasive particles. Boron Carbide (B4C) ceramics was tested by mixing it with iron (Fe) and produced abrasive particles to reduce the intensity of scraping on the surface, reduce the economic cost and achieve a high finishing addition to remove the edges at the same time. The material selected for the samples was mild steel (ASTM E415) under (Quantity of Abrasives, Mac
... Show MoreBackground: The aim of this study is to evaluate the color change ∆E of the dental enamel following treatment with 2 kinds of protector (icon infiltrant, clinpro varnish) before fixed orthodontic treatment to avoid the possible white spot lesions. Materials and Methods: Fifty four subjects treated with fixed appliances were divided into 3 groups: the 1st group was control, while the 2nd and 3rd groups were treated with icon infiltrant and clinpro varnish before bonding procedure, respectively. Color parameters (L,a,b) were recorded for the middle and gingival thirds before and after bonding procedure to get the ∆E of each group. Results: One-way ANOVA test showed a non-significant difference in ∆E between the 3 groups a
... Show MoreBackground: The purpose of this study is to compare the color changes between the bonded middle third and the unbonded gingival and incisal thirds, fallowing fixed orthodontic treatment Material and method: The color parameter l, a, b has been recorded for each thirds in upper anterior teeth by mean of easy shad device. The has been calculated for gingival, middle and incisal thirds for the upper anterior teeth in 34 patient, 17 males and 17femals, those subject undergone fixed orthodontic treatment Results: The in middle bonded third is highly significant higher than that in incise and gingival thirds p<0.01 because the middle third isn’t expose to oral fluid and dental brushing since it covered by the bracket. Also there
... Show MoreThis research studies the effect of addition of some nanoparticles
(MgO, CuO) and grain size (30,40nm) on some physical properties
(impact strength, hardness and thermal conductivity) for a matrix
blend of epoxy resin with SBR rubber. Hand –Lay up method was
used to prepare the samples. All samples were immersed in water for
9 weeks.
The Results showed decreased in the values of impact strength and
hardness but increased the coefficient of thermal conductivity.
Background: 37% phosphoric acid (PA) is the traditional enamel etching technique prior to bracket adhesion, yet it has been implicated in numerous enamel injuries. The purpose of the current study was to create a calcium phosphate (CaP) etching paste in a simplified capsule formula that can underpin clinically adequate bracket bond strength without jeopardizing the integrity of enamel upon the debracketing procedure. Materials and Methods: micro-sized hydroxyapatite (HA) powder was mixed with 40% PA solution to prepare experimental acidic CaP paste. Sixty human premolars were assigned into two groups of 30 each. Enamel conditioning was accomplished using 37% PA-gel for control group and CaP paste for e
... Show MoreAn acidic environment causes surface changes of resin composites. Filler particlesize and filler distribution also have a direct effect on these surface changes. This invitro study evaluated the influence of Pepsi Cola drink on the surface roughness ofComposan LCM and Composan Ceram over time. Sixteen disc shaped specimens(10mm diameter, 2mm thickness) of each resin composite were fabricated, therebyforming two groups (n= 8). Surface roughness (Ra) was analyzed after 24 hrs beforeexposure to beverage. The specimens were submitted to a five minutes immersion inPepsi Cola three times daily interrupted by immersion in deionized distilled water (37C˚). Surface roughness measurements were done at 10, 30, and 60 days intervals. Datawere
... Show More