Background: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three groups (n = 10) according to the debond times: I: debond after 24 hour, II: debond after 7 days and III: debond after 30 days. Within 24 hr, half of the sample was thermocycled manually for 500 complete cycles between 5/55°C and the remaining sample was stored in distilled water at room temperature and water was changed daily until debond time for each group was performed. The adhesive remnant index was tested under 20X magnification lens using stereomicroscope. Results and Conclusions: Both bracket types demonstrated high shear bond strength values before thermocycling (P?0.05), whereas after 500 thermocycles, there were significant changes in shear bond strength resulted in marked reduction in the stainless steel brackets than in the sapphire brackets (P?0.05). Shear bond strength values increased with time for both stainless steel and sapphire brackets with and without thermocycling (P?0.05). The tendency of bond failure was increased at the bracket/adhesive interface rather than enamel/bracket interface in the stainless steel brackets whereas at the enamel/bracket interface rather than bracket/adhesive interface in the sapphire brackets.
م.د. فاطمة حميد ،أ.م.د وفاء صباح محمد الخفاجي, International Journal of Psychosocial Rehabilitation,, 2020 - Cited by 1
Thin films of pure polycarbonate (PC) with anthracene doping PC films for different doping ratios (10, 20, 30, 40, 50 and 60 ml) were prepared by using a casting method. The influence of anthracene doping ratio on photo-fries rearrangement of polycarbonate was systematic investigated. Furthermore, pure PC and anthracene doping PC films were irradiated via UV light at a wavelength (254 nm) for different periods (5, 240, 288, and 360 hrs). The photo-fries rearrangement occurring in pure PC and anthracene doping PC films were monitored using UV and FTIR spectroscopies. The photo-fries rearrangement leads to scission the carbonate linkage and formation phenylsalicylate and dihydroxybenzophenes. The result of the UV spectrum confirms disappea
... Show MoreFour localities were selected in Euphrates River and Ramadi sewage treatment plant to collect water samples monthly during the period between October 2001 to July 2002 . Total cell count of phytoplankton and its physico- chemical concentrations were determined . The study aimed to demonstrate the effect of Ramadi sewage treatment plant on Euhprates River . It is concluded that the sewage had an dilution effect for the total hardness , total alkalinity , electrical conductivity and salinity of Euphrates River , but it is also caused in the presence of a contaminated area . This was cleared from the depletion of dissolved oxygen and high values of biological oxygen demand with lower valuse of pH in this area . The water of Euphrates
... Show MoreThis experiment was conducted to study the effect of injecting hatching eggs into a flock of broiler aged mothers with different concentrations of the alcoholic extract of Moringa oleifera powder on productive performance of broilers during the period of rearing of 35 days. The study included two experiments for a period at 2/10/2021 to 28/11/2021, where eggs were injected into the Mustafa Poultry Hatchery/ Wasit Governorate- Aziziyah District. A 400 hatching eggs of 308 Ross mothers of modern broilers used at age of 48 week, eggs of average weight 66 ± 1 g/egg were collected in same day then stored for two days. A quarter of treatments were randomly distributed with 100 eggs for each treatment.
... Show MoreABSTRACT
Naproxen(NPX) imprinted liquid electrodes of polymers are built using polymerization precipitation. The molecularly imprinted (MIP) and non imprinted (NIP) polymers were synthesized using NPX as a template. In the polymerization precipitation involved, styrene(STY) was used as monomer, N,N-methylenediacrylamide (N,N-MDAM) as a cross-linker and benzoyl peroxide (BPO) as an initiator. The molecularly imprinted membranes and the non-imprinted membranes were prepared using acetophenone(AOPH) and di octylphathalate(DOP)as plasticizers in PVC matrix. The slopes and detection limits of the liquid electrodes ranged from)-18.1,-17.72 (mV/decade and )4.0 x 10-
... Show MoreIn the last years, new non-invasively laser methods were used to detect breast tumors for pre- and postmenopausal females. The methods based on using laser radiation are safer than the other daily used methods for breast tumor detection like X-ray mammography, CT-scanner, and nuclear medicine.
One of these new methods is called FDPM (Frequency Domain Photon Migration). It is based on the modulation of laser beam by variable frequency sinusoidal waves. The modulated laser radiations illuminate the breast tissue and received from opposite side.
In this paper the amplitude and the phase shift of the received signal were calculated according to the orig
... Show MoreBackground: Elastomeric chains are used to generate force in many orthodontic procedures, but this force decays over time, which could affect tooth movement. This study aimed to study the force degradation of elastomeric chains. Data and Sources: An electronic search on Cochrane Central Register of Controlled Trials (CENTRAL), MEDLINE, LILACS, and PubMed was made, only articles written in English were included, up to January 2022.Study selection: Fifty original articles, systematic reviews, and RCTs were selected. Conclusion: Tooth movement, salivary enzymes, alcohol-containing mouthwash, whitening mouthwash, and alkaline and strong acidic (pH <5.4) solutions all have a significant impact on elastomeric chain force degradation. T
... Show MoreBackground: Elastomeric chains are used to generate force in many orthodontic procedures, but this force decays over time, which could affect tooth movement. This study aimed to study the force degradation of elastomeric chains. Data and Sources: An electronic search on Cochrane Central Register of Controlled Trials (CENTRAL), MEDLINE, LILACS, and PubMed was made, only articles written in English were included, up to January 2022.Study selection: Fifty original articles, systematic reviews, and RCTs were selected. Conclusion: Tooth movement, salivary enzymes, alcohol-containing mouthwash, whitening mouthwash, and alkaline and strong acidic (pH <5.4) solutions all have a significant impact on elastomeric chain force degradation. The fo
... Show More