Background: Debonding orthodontic brackets and removal of residual bonding material from the enamel surface include critical steps that may cause enamel damage. The aim of the present study was to evaluate and compare the site of bond failure and enamel surface damage after debonding of three types of esthetic brackets (composite, ceramic, sapphire) bonded with light cure composite and resin-modified glass ionomer adhesive. Materials and methods: Seventy two maxillary premolars teeth were divided into three groups each group consisted of 24 teeth according to the type of brackets. Each group was subdivided into two subgroups (12 teeth for each) according to the bonding material that was used. After 7 days of bonding procedure, the brackets were debonded using specifically designed debonding device in which the brackets were debonded by a debonding pliers to simulate the actual clinical debonding procedure. Instron Universal testing was used to apply the debonding force on the debonding pliers which transferred to the bracket. The teeth and the brackets were examined with a 10X magnifying lens to evaluate the site of failure. After the removal of residual adhesive, stereomicroscope was used to evaluate enamel surface damage. Results: The most common type of bond failure was cohesive failure (Score II) in all esthetic brackets. While enamel cracks (scale I) were found to be the most type of enamel damage. Chi- square showed non-significant differences among different types of esthetic bracket bonded with same type of adhesive and between the same types of brackets (ceramic, sapphire) bonded with the two types of adhesive. On the other hand, there was significant difference between composite brackets subgroups bonded with the two adhesives. Conclusion: The bond failure mostly within the adhesive itself and higher enamel damage was resulted from mechanical debonding of these esthetic brackets.
Background: Thermocycling simulates the temperature dynamics in the oral environment. This in vitro study done to measure and compare the effect of thermocycling on the shear bond strength of stainless steel and sapphire brackets bonded to human enamel teeth using light cured orthodontic adhesive and debonded at various time, and to measure adhesive remnant index after debonding. Materials and Methods: one-hundred-twenty extracted upper first premolars for orthodontic reason were used in this study; depending on weather thermocycled or not, the sample was divided into two main groups, then within each group 30 teeth were used for stainless-steel brackets (Bionic®) and for sapphire brackets (Pure®). Both groups were subdivided into three
... Show MoreBackground: Decalcification of surface enamel adjacent to fixed orthodontic appliances, in the form of white spot lesions, is a wide spread and familiar well-known side effect of orthodontic treatment. The present study was carried out to evaluate the effect of enamel protective agent (Clinpro white varnish) on shear and tensile bond strength of Dentaurum orthodontic stainless steel brackets by using 3M Unitek and Ormco as orthodontic adhesive agents. Materials and methods: Sixty-four extracted human upper first premolar teeth were selected and randomly divided into two groups with 32 teeth each, representing the shear and tensile bond strength testing groups. Then according to the type of bonding adhesive and the addition of Clinpro before
... Show MoreBackground: evaluate the effects of three different intracoronal bleaching agents on the shear bond strengths (SBS) and failure site of stainless steel and monocrystalline (sapphire) orthodontic brackets bonded to endodontically treated teeth using light cured orthodontic adhesive in vitro. Materials and methods: Eighty extracted sound human upper first premolars were selected, endondontically treated and randomly divided equally (according to the type of the brackets used) into two main groups (n = 40 per group). Each main group were subdivided (according to the bleaching agent used) into four subgroups 10 teeth each; as following : control (un bleached) group, hydrogen peroxide group (Hp) 35%, carbamide peroxide group (CP) 37% group and s
... Show MoreBackground: The present study was carried out to compare shear bond strength of sapphire bracket bonded to zirconium surface after using different methods of surface conditioning and assessment of the adhesive remnant index. Materials and methods: The sample composed of 40 zirconium specimens divided into four groups; the first group was the control, the second group was conditioned by sandblast with aluminum oxide particle 50 μm, the third and fourth group was treated by (Nd: YAG) laser (1064nm)(0.888 Watt for 5 seconds) for the 1st laser group and (0.444 Watt for 10 seconds) for the 2nd laser group. All samples were coated by z-prime plus primer. A central incisor sapphire bracket was bonded to all samples with light cure adhesive res
... Show MoreThis study evaluated the extent to which obturation materials bypass fractured endodontic instruments positioned in the middle and apical thirds of severely curved simulated root canals using different obturation techniques. Sixty resin blocks with simulated root canals were used, each with a 50° curvature, a 6.5 mm radius of curvature, and a length of 16.5 mm, prepared to an ISO #15 diameter and taper. Canals were shaped using ProTaper Universal files (Dentsply Maillefer) attached to an X-smart Plus endo motor (Dentsply), set at 3.5 Ncm torque and 250 rpm, up to size S2 at working length. To simulate fractures, F2 and F3 files were weakened 3 mm from the tip, then twisted to break in the apical and middle sections of the canal, re
... Show MoreABSTRACT Background: Bracket rebonding is a common problem in orthodontics which may result in many drawbacks. The aims of this study were to evaluate the effects of application of two enamel protective agents “Icon†and “ProSeal†on shear bond strength before and after rebonding of stainless steel orthodontic brackets using conventional orthodontic adhesive and to assess the site of bond failure. Materials and methods: Fifty sound extracted human upper first premolar teeth were selected and randomly divided into two equal groups; the first time bonding and the rebonding groups (n=30). Each group was subdivided into control, Icon and ProSeal subgroups. The enamel protective agents were applied after etching (precondi
... Show MoreBackground: The demand for esthetic orthodontic appliances is increasing; so the esthetic orthodontic archwires were introduced. Among them, Teflon and Epoxy coated stainless steel archwires. The amount of force available from the archwire depends on the structural properties and susceptibility to corrosion. All metallic alloys are changed during immersion in artificial saliva, chlorhexidine mouthwash andtoothpaste, but their behaviors differ from one type to another. They corrode at different rates, which lead to decrease the amount of force applied to the teeth. This in vitro study was designed to evaluate the corrosion pits in stainless steel archwires coated with Teflon and with Epoxy in dry and after immersion in artificial saliva, chl
... Show MoreBackground: The present study was conducted to evaluate the effects of different bleaching methods on the shear bond strength of orthodontic Sapphire brackets bonded to human premolars teeth using light cured composite resin and to determine the predominant site of bond failure. Materials and Methods: Thirty freshly extracted human premolars were selected and randomly divided into three groups (10 per group). These groups are: control (unbleached) group, hydrogen peroxide group (HP) 37.5% ; which is the in- office bleaching method group, carbamide peroxide group (CP) 16%; which is the at- home bleaching method group. After bleaching process was performed, all the teeth stored in distilled water in a sealed container at room temperature for
... Show MoreBackground: With the increased in the demands of adult orthodontics, the challenge of direct bonding to non-enamel surface (zirconium) had been increased. The present study was carried out to compare the shear bond strength of three different brackets (stainless steel, sapphire and composite) bonded to zirconium surface and study the mode of bond failure. Materials and methods: The sample was comprised of 30 models (8mm *6mm*1.5mm) of full contour zirconium veneers. They were divided into three groups according to the brackets type; all samples were treated first by sandblast with aluminum oxide particle 50 µm then coated by z-prime plus primer. A central incisor bracket of each group was bonded to the prepared zirconium surface with lig
... Show More