Background: The daily cleaning routine of the silicone maxillofacial prostheses by the patient may cause some alteration in the materials properties. The purpose of the present study was to investigate the effect of different disinfection procedures on some properties of silicon dioxide reinforced Cosmesil M511 HTV maxillofacial silicone. Materials and Methods: One hundred and sixty (160) specimens were prepared by mixing 5% SiO2 nano particles and 0.5% intrinsic cream color into the silicone polymer according to manufacturer's instructions. Specimens were divided into 4 groups according to the performed test (tear strength, surface hardness, surface roughness and color) with 40 specimens each. Each group was further subdivided according to the disinfection procedure conducted (control, microwave exposure, neutral soap and 4% chlorhexidine gluconate). Measurements for tear strength were done using universal testing machine. Surface hardness test was carried out with a Shore A Durometer. Surface roughness was analyzed with a portable digital Profilometer. Color change was established with a Spectrophotometer. After the initial testing, all specimens were submitted to disinfection procedure 3 times a week for 60 days. Measurements were repeated and data were statistically analyzed using one-way ANOVA followed by Fisher's LSD or Games-Howell test. Results: Spectrophotometer results showed non-significant decrease in the light absorbance of all experimental groups after disinfection, indicating a strong integration between the nano filler and the polymeric chains, which was not broken during the disinfection procedure. Highly-significant increase in Shore A hardness was recorded, while the decrease in surface roughness was highly significant in all experimental groups. Tear strength reduced significantly after disinfection in all experimental groups. Conclusion: Disinfection seemed to cause different amount of alteration in all of the tested properties of silicone. High color stability is expected in this type of maxillofacial silicone after disinfection.Although microwave exposure had increased the hardness of the material, it is considered a satisfactory disinfection procedure since it caused the least effect on the tear strength and surface roughness of the material. Therefore, microwave exposure is recommended for the disinfection of maxillofacial silicone prostheses.
Facial trauma in children and adolescents is reported to range from 1% to 30%. Because of many anatomical, physiological, and psychological characteristics of the pediatric population, maxillofacial injuries in children should be treated with special consideration that is attributable to certain features inherent in facial growth patterns of children. This study evaluated maxillofacial injuries in 726 children in terms of incidence, patterns of injury, causes, and treatment modalities and compared these parameters among 3 pediatric age groups. Intergroup differences were analyzed using Z test for 2 populations' proportion. The results showed that the incidence of pediatric maxillofacial injuries and fractures is higher than that reported el
... Show More An experimental and computational study is conducted to analyze the thermal performance of heat sinks and to pick up more profound information in this imperative field in the electronic cooling. One important approach to improve the heat transfer on the air-side of the heat exchanger is to adjust the fin geometry. Experiments are conducted to explore the impact of the changing of diverse operational and geometrical parameters on the heat sink thermal
performance. The working fluid used is air. Operational parameters includes: air Reynolds number (from 23597 to 3848.9) and heat flux (from 3954 to 38357 W/m
2 ). Conformational parameters includes: change the direction of air flow and the area of conduct
In this study a polymeric composite material was prepared by hand
lay-up technique from epoxy resin as a matrix and magnesium oxide
(MgO) as a reinforcement with different weight fraction (5,10,15,
and 20)% to resin. Then the prepared samples were immersed under
normal condition in H2So4(1 M) solution, for periods ranging up to
10 weeks. The result revealed that the diffusion coefficient
decreasing as the concentration of MgO increase. Also we studied
Hardness for the prepared samples before and after immersion. The
result revealed that the hardness values increase as the concentration
of MgO increase, while the hardness for the samples after immersion
in H2SO4 dec
Zinc sulfide (ZnS) thin films were deposited on glass substrates using pulsed laser deposition technique. The laser used is the Q-switched Nd: YAG laser with 1064nm wavelength and 1Hz pulse repetition rate and varying laser energy 700mJ-1000mJ with 25 pulse. The substrate temperature was kept constant at 100°C. The structural, morphological and optical properties of ZnS thin films were characterized with X-ray diffraction (XRD), scanning electron microscopy (SEM), atomic force microscope (AFM) and UV-VIS spectrophotometer.
The technical of Flame Thermal Spray had been used in producing a cermet
composite based on powders of stabilized zirconium oxide containing amount of
Yatteria oxide (ZrO2- 8Y2O3) reiforced by minerals powders of bonding material
(Ni-Cr- Al- Y) in different rates of additions (25, 35, 50) on stainless steel base type
(304) after preparing it by the way of Grit Blasting.
Before heat treatment, the coated cermet layers were characterized for porosity
and electric resistivity. All samples were heat treated in vacuum furnace at different
temperature and times. The physical tests had been operated after heat treatment
and gave best results especially porosity, which found to be reduced dramatically
and producing hig
The Dielectric properties of EP/TiO2 and MgO nanocomposite at
a frequency range of (102-106 Hz) were studied. The composite were
prepared with the state volume ratio (0, 0.05, 0.1) for EP/TiO2 and
MgO respectively. The impedance, dielectric constant and dielectric
loss were found decrease with frequency increase.
This research studies the effect of adding five different percentages of polymer (2, 4, 6, 8, and 10% of cement weight) on cement mortar's fresh and hardened properties, which was cured at laboratory temperature for 7, 14, and 28 days. Workability increases with increasing polymer. The workability value was lowest (25.6 and 29.4) % in mixtures containing 2% and 4% of (SBR). Increasing polymer ratios significantly decreased mechanical properties (compressive and flexural strength). Therefore, the best results were at 2% SBR and 4% SBR at 28 days of age. An inverse relationship was recorded between the increase in SBR ratios and polymer-modified cement mortar's compressive and flexural strength values. In general, the high
... Show More