Preferred Language
Articles
/
jbcd-1492
Evaluation of Impact and Transverse Strength of Denture Bases Repaired with Nano Reinforced Resin
...Show More Authors

Background: Failure of resin bases were a major disadvantage recorded in the constructed dentures. Reinforcements of the repair joint with nano fillers represent an attempt to enhance the strength and durability. The purpose of the research was to estimate the influence of nano fillers reinforcement with (ZrO2 and Al2O3) on impact and transverse strength of denture bases repaired with either cold or hot processing acrylic resin. Materials and methods: A hundred and forty (140) samples were processed with hot cured resin and organized in subgroups depending on the repair materials and condition (without repair (control), repair with hot cure, cold cure, hot and cold cure reinforced with either (5% Zr2O or 0.5% Al2O3). The samples in these subgroups were processed depending on the test applied (impact and transverse strength). The samples were immersed in distalled water for about four weeks at 37°C before testing, after that, the samples prepared for each test were subdivided depending on the selected subgroups of the study. Repairing the samples with cold cure resin was done with the aid of Ivomet; after that the samples incubated for 48 hours in 37°C distilled water. Transverse strength test was done by using INSTRON universal testing machine while the impact test was done by using CHARPY impact testing machine. Results: The reinforcement of the repair joint with nano-fillers improves both impact and transverse strengths. Conclusion: Repair strength is directly proportional to the mode of resin processing, reinforcement with nano-fillers improve the strength of the repaired joint significantly.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Fri Jan 01 2021
Journal Name
Aip Conference Proceedings
Synthesis and characterizations of core-shell SiO2/Au/Ag nano-particles by exploding of wire and pulsed laser plasmas
...Show More Authors

View Publication
Scopus (2)
Crossref (1)
Scopus Crossref
Publication Date
Tue Dec 01 2020
Journal Name
Systematic Reviews In Pharmacy)srp)
Evaluation the response to infliximab therapy in patients with ulcerative colitis and crohn's disease
...Show More Authors

Scopus
Publication Date
Tue Jan 08 2019
Journal Name
Iraqi Journal Of Physics
Effect of UV radiation on dielectric properties of PU/nano-TiO2 composites
...Show More Authors

The dielectric constant of most polymers is very low; the addition of TiO2 particles into the polymers provides an attractive and promising way to reach a high dielectric constant. Polymer-based materials with a high dielectric constant show great potential for energy storage applications. Four samples were prepared, one of them was polyurethane (PU) and the other were PU with different weight percent (wt %) of TiO2 (0.1, 0.2, 0.3) powder AFM test was used to distinguish the nanoparticles. The result shows that the most shape of these nanoparticles are spherical and the roughness average is 0.798 nm. The dielectric properties were measured for all samples before and after the exposure to the UV radiation. The result illustrates that the

... Show More
View Publication Preview PDF
Crossref
Publication Date
Wed Sep 01 2021
Journal Name
Iop Conference Series: Earth And Environmental Science
Effect of Nano Calcium Carbonate on Some Properties of Reactive Powder Concrete
...Show More Authors

View Publication
Scopus (9)
Crossref (8)
Scopus Crossref
Publication Date
Fri Jun 16 2023
Journal Name
Iraqi Journal Of Pharmaceutical Sciences ( P-issn 1683 - 3597 E-issn 2521 - 3512)
Impact of omega 3 alone or in combination with irinotecan on bone marrow and spleen of rats: in vivo study
...Show More Authors

Abstract

Objectives: The present study designed to explore the genotoxicity through measurement of Mitotic index in bone marrow and the spleen cells, as possible mechanism of bone marrow and spleen toxicity that induced by irinotecan; and to describe the protective actions of omega 3 against irinotecan induced genotoxicity in bone marrow and the spleen of rats.

Methods: Twenty four (24) rats (Sprague-Dawley) were randomly divided into four groups: Group Ӏ, rats  received single oral daily dose of distilled water (2 ml/kg) for 25 days (negative control group); Group ӀӀ (irinotecan-treated), receiv

... Show More
View Publication Preview PDF
Scopus (3)
Crossref (1)
Scopus Crossref
Publication Date
Mon Dec 30 2024
Journal Name
Iraqi Journal Of Science
The Impact of Fear and Anti-Predator Behavior on the Dynamics of Stage-Structure Prey–Predator Model With a Harvesting
...Show More Authors

In this paper, an ecological model with stage-structure in prey population, fear, anti-predator and harvesting are suggested. Lotka-Volterra and Holling type II functional responses have been assumed to describe the feeding processes . The local and global stability of steady points of this model are established. Finally, the global dynamics are studied numerically to investigate the influence of the parameters on the solutions of the system, especially the effect of fear and anti-predation.

Scopus (1)
Scopus Crossref
Publication Date
Wed Jul 14 2021
Journal Name
The Open Civil Engineering Journal
Producing Sustainable Concrete using Nano Recycled Glass
...Show More Authors
Background:

Many tools and techniques have been recently adopted to develop construction materials that are less harmful and friendlier to the environment. New products can be achieved through the recycling of waste material. Thus, this study aims to use recycled glass bottles as sustainable materials.

Objective:

Our challenge is to use nano glass powder by the addition or replacement of the weight of the cement for producing concrete with enhanced strength.

Methods:

A nano recycled glass p

... Show More
View Publication Preview PDF
Crossref (13)
Crossref
Publication Date
Wed Jul 14 2021
Journal Name
The Open Civil Engineering Journal
Producing Sustainable Concrete using Nano Recycled Glass
...Show More Authors
Background:

Many tools and techniques have been recently adopted to develop construction materials that are less harmful and friendlier to the environment. New products can be achieved through the recycling of waste material. Thus, this study aims to use recycled glass bottles as sustainable materials.

Objective:

Our challenge is to use nano glass powder by the addition or replacement of the weight of the cement for producing concrete with enhanced strength.

Methods:

A nano recycled glass p

... Show More
Scopus (13)
Crossref (13)
Scopus Crossref
Publication Date
Mon Dec 20 2021
Journal Name
Baghdad Science Journal
Synthesis and Characterization of New nano catalyst Mo-Ni /TiO2- γAl2O3 for Hydrodesulphurization of Iraqi Gas Oil
...Show More Authors

   A new nano-sized NiMo/TiO2-γ-Al2O3 was prepared as a Hydrodesulphurization catalyst for Iraqi gas oil with sulfur content of 8980 ppm, supplied from Al-Dura Refinery. Sol-gel method was used to prepare TiO2- γ-Al2O3 nano catalyst support with 64% TiO2, 32% Al2O3, Ni-Mo/TiO-γ-Al2O3 catalyst was prepared under vacuum impregnation conditions to loading metals with percentage 3.8 wt.% and 14 wt.% for nickel and molybdenum respectively while the percentage for alumina, and titanium became 21.7, and 58.61 respectively. The synthesized TiO2- γ-Al2O3 nanocomposites and Ni-Mo /TiO2

... Show More
View Publication Preview PDF
Scopus (6)
Crossref (4)
Scopus Clarivate Crossref
Publication Date
Mon Oct 01 2012
Journal Name
Iraqi Journal Of Physics
Effect of nano and micro SiO2 weight percent on interlaminar fracture toughness of woven roving/ epoxy composites
...Show More Authors

Effect of nano and micro SiO2 particles with different weight percent (2,4,6,8 and 10) %wt on the Interlaminar fracture toughness (GIc) of 16-plies of woven roving glass fiber /epoxy composites prepared by hand lay – up technique were investigated. The specimens were tested using DCB test (mode I).
Area method was used to compute the interlaminar fracture toughness. The results show that, GIc would increase with the increasing in the filler content, the main failure in microcomposites and nanocomposites was delamination in the layers, the delamination reduced with increasing in the filler content.

View Publication Preview PDF