Comparison of Shear Bond Strength of Three Different Brackets Bonded on Zirconium Surfaces (In Vitro Study)
...Show More Authors

Background: With the increased in the demands of adult orthodontics, the challenge of direct bonding to non-enamel surface (zirconium) had been increased. The present study was carried out to compare the shear bond strength of three different brackets (stainless steel, sapphire and composite) bonded to zirconium surface and study the mode of bond failure. Materials and methods: The sample was comprised of 30 models (8mm *6mm*1.5mm) of full contour zirconium veneers. They were divided into three groups according to the brackets type; all samples were treated first by sandblast with aluminum oxide particle 50 µm then coated by z-prime plus primer. A central incisor bracket of each group was bonded to the prepared zirconium surface with light cure adhesive resin (Transbond TM XT, 3M Unitek, USA). Shear bond strength was measured by using Tinius Olsen universal testing machine at crosshead speed of 0.5\min. After debonding, each bracket and zirconium surface were examined using magnifying lens and adhesive remnant index was recorded. The difference in shear bond strength between main groups was analyzed by using ANOVA at p≤0.05. Results: The results revealed high significant difference among all tested groups and the highest value was for sapphire brackets (7.49±1.45 Mpa) of all groups followed by stainless steel brackets (6.46±1.43Mpa) and composite brackets had the least value (4.35±0.72). Non-significant difference in the site of bond failure among all groups of brackets and zirconium-adhesive interface failure (score III) was the predominant. Conclusion: the new zirconium prime plus primer can be successfully used in bonding stainless steel and sapphire brackets to zirconium surface.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Sun Mar 25 2018
Journal Name
Biomedical And Pharmacology Journal
Comparing the Impact Strength and Transverse Flexure Strength of Three Different Dentures Base Materials
...Show More Authors

View Publication
Crossref (8)
Crossref
Publication Date
Fri Dec 15 2017
Journal Name
Journal Of Baghdad College Of Dentistry
In Vitro Comparative Assessment Of The Effect Of Gutta-Fusion Obturation On The Push Out Bond Strenght Of Three Types Of Sealers
...Show More Authors

Background: The bond strength of the root canal sealers to dentin is very important property for maintaining the integrity and the seal of root canal filling. The aim of this study was to evaluate and compare the push-out bond strength of root filled with total fill Bioceramic, AH Plus and Gutta-flow®2 sealers using GuttaFusion®obturation system versus single cone obturation technique. Materials and method: sixty of mandibular premolars teeth with straight roots were used in this study, these roots were instrumented using Reciproc system, instrumentation were done with copious irrigation of 3 mL 5.25% sodium hypochlorite solution (NaOCl) during all the steps of preparation, and smear layer will be removed with 1 ml of 17% EDTA kept in

... Show More
View Publication Preview PDF
Crossref (2)
Crossref
Publication Date
Sat Dec 31 2022
Journal Name
International Journal Of Dentistry
Bond Strength Survival of a Novel Calcium Phosphate-Enriched Orthodontic Self-Etching System after Various Ageing Protocols: An In Vitro Study
...Show More Authors

Objective. This study aimed to evaluate the orthodontic bond strength and enamel-preserving ability of a hydroxyapatite nanoparticles-containingself-etch system following exposure to various ageing methods. Materials and Methods. Hydroxyapatite nanoparticles (nHAp) were incorporated into an orthodontic self-etch primer (SEP, Transbond™ plus) in three different concentrations (5%, 7%, and 9% wt) and tested versus the plain SEP (control) for shear bond strength (SBS), adhesive remnant index (ARI) scores, and enamel damage in range-finding experiments using premolar teeth. The best-performing formulation was further exposed to the following four artificial ageing methods: initial debonding, 24 h water storage, one-month water stora

... Show More
View Publication
Scopus (5)
Crossref (6)
Scopus Clarivate Crossref
Publication Date
Thu Apr 13 2023
Journal Name
Sustainability
Experimental Study of the Effect of Tack Coats on Interlayer Bond Strength of Pavement
...Show More Authors

The performance and lifetime of the flexible asphalt pavement are mainly dependent on the interfacial bond strength between layer courses. To enhance the bond between layers, adhesive materials, such as tack coats, are used. The tack coat itself is a bituminous material, which is applied on an existing relatively non-absorbent surface to ensure a strong bond between the old and newly paved layer. The primary objective of this study was to evaluate the effects of various types of tack coat materials on interlayer bond strength and to determine the optimal application rate for each type. The tack coat types used in this paper were RC-70, RC-250, and CSS-1h. Both laboratory-prepared and field-constructed hot mix asphalt concrete pavements usin

... Show More
View Publication
Scopus (4)
Crossref (3)
Scopus Clarivate Crossref
Publication Date
Tue May 27 2025
Journal Name
Journal Of Baghdad College Of Dentistry
Early and delayed effect of 2% chlorhexidine on the shear bond strength of composite restorative material to dentin using a total etch adhesive
...Show More Authors

Background: Lack of durability of the bond of the dental adhesive systems to tooth structure is one of the most important problems in tooth colored restorative work. This in vitro study was performed to evaluate the effect of 2% chlorhexidine gluconate(CHX) on dentin bond strength by using total etch adhesive system at twenty-four hours and three months of water storage. Material and methods:A flat dentin surface was prepared for forty sound human maxillary premolar teeth which were acid etched with 36% phosphoric acid gel after being divided randomly into four groups of ten teeth each according to storage time and CHX application, theCHX was applied for 60 seconds before adhesive application for groups I and III which were tested after twe

... Show More
View Publication Preview PDF
Publication Date
Fri Jun 23 2023
Journal Name
Cumhuriyet Dental Journal
The effectiveness of continuous versus sequential chelation in the removal of smear layer and their influence on push-out bond strength of Bio-C sealer (An in vitro study)
...Show More Authors

Objectives: Successful endodontic treatment outcome requires effective shaping and cleaning of root canals. This study aims to evaluate the smear layer removal after continuous chelation (CC) ) NaOCL\HEDP( and sequential chelation (SC) )NaOCL\EDTA( and their influence on the push-out bond strength (POBS) of Bio-C sealer. Materials and Methods: Palatal roots of the maxillary first molar (n=72) were divided into four groups (n=18) as follows: 3% NaOCL, SC: 3% NaOCL followed by 17% EDTA, CC: 3% NaOCL \9% HEDP and Distilled water. Thirty-two roots (n=8/group) were split longitudinally for smear layer evaluation using SEM. Forty roots were obturated with Guttapercha and Bio-C sealer using a single cone technique. Thre

... Show More
View Publication Preview PDF
Scopus (3)
Crossref (2)
Scopus Crossref
Publication Date
Wed Dec 01 2010
Journal Name
Iraqi Journal Of Physics
Effect of Furnace Vacuum Pressure on the Joining Strength of Alumina Bonded Kovar
...Show More Authors

Ceramic to metal joining technique, which was used in this investigation includes the use of active filler alloy as a sandwich between the alumina and kovar alloy for brazing. High purity powdered metals of silver, copper, and additives of titanium were used to prepare the active filler alloy, through compacting the mixed powders and alloying in a furnace with argon atmosphere at the temperature of 800oC for 10 minutes. To use it as an active filler metal, it has been modified to a proper thickness. Two groups of alumina were prepared with different sintering temperatures (1450oC and 1650oC) and each group was tested under atmospheric pressure, vacuum furnace pressure of 2*10-4 torr and vacuum furnace pressure of 2*10-6 torr. All the pro

... Show More
View Publication Preview PDF
Publication Date
Fri Jun 11 2021
Journal Name
Journal Of Baghdad College Of Dentistry
The influence of different root canal irrigants on the push-out bond strength of AH plus and Bioceramic sealers
...Show More Authors

Background: The bond strength of endodontic sealers with dentin is a very important property for maintaining the integrity and seal of the root canal filling. The aim of this study was to evaluate and compare the effect of various irrigants (QMix, 17% EDTA and 2.5% NaOCl) on the push-out bond strength of AH plus and Bioceramic sealers. Materials and methods: Forty eight freshly extracted maxillary first molars human teeth with striaght palatal root were used in the study. The collected samples were randomly divided into three groups of equal sample size (n=16), according to the final irrigation regimen as follows: Group (1): QMix 2 in 1, Group (2): 17% ethylenediaminetetraacetic acid, Group (3): 2.5% sodium hypochloride. All samples were

... Show More
View Publication Preview PDF
Scopus (2)
Crossref (3)
Scopus Crossref
Publication Date
Mon Jun 01 2020
Journal Name
Iop Conference Series: Materials Science And Engineering
Effect of Adding Sand on Clayey Soil Shear Strength
...Show More Authors
Abstract<p>The effect of adding sand on clayey soil shear strength is investigated in this study. Five different percentage of clay-sand mixtures are used; 100% clay with 0% sand termed 100C, 60% clay with 40% sand termed 60C-40S, 30% clay with 70% sand termed 30C-70S, 15% clay with 85% sand termed 15C-85S, and as well as 100% sand termed 100S. The used clay was obtained from Baghdad city in Iraq and classified as CH soil, while the used sand was taken from Al-Khider area from Iraq and classified as SW soil. The initial dry unit weight for all mixtures is 16 kN/m<sup>3</sup>. The results show that the variations of the soil shear strength properties with soil components content changes</p> ... Show More
View Publication
Crossref (1)
Crossref
Publication Date
Wed Nov 15 2023
Journal Name
Bionatura
Evaluation of frictional forces between aesthetic brackets and archwires in wet conditions (An in-vitro study)
...Show More Authors

Frictional resistance occurs whenever sliding happens, negatively impacting treatment outcomes and duration. It is a clinical challenge and must be dealt with efficiently to achieve the best orthodontic results. Aims of this study: compare and evaluate the static frictional forces under the wet condition to mimic the oral environment produced by using a polycrystalline ceramic bracket, monocrystalline ceramic bracket, 0.014 of an inch nickel-titanium (Rhodium coated archwires, and ilusio aesthetic archwires), and 0.019 x 0.025 of an inch stainless steel (Rhodium coated archwires, and ilusio aesthetic archwires). Ninety-six aesthetic brackets (48 monocrystalline and 48 polycrystalline brackets) were used and stored in different incub

... Show More
View Publication Preview PDF
Crossref (1)
Scopus Crossref