Background: Dental implant considers a unique treatment option for the replacement of missing dentition. The new trend of implants is looking for materials which accelerate bone formation in bone implant interface and enhance osseointegration to provide immediate loading directly after placement and decrease the time period which is disturbs patients and uncomfortable. The aim of the study was to evaluate the effect of nano zirconium oxide (ZrO2) and nano hydroxyapatite (Hap) mixture coating of screw shaped commercially pure titanium (cpTi) implants on bond strength at the bone implant interface with torque removal test and histological analysis in comparison with non coated implants. Materials and methods: Forty screws were machined from cpTi rods using a lathe machine. Then 20 screws coated by electrophoretic deposition method by a mixture of nano hydroxyl apatite and nano zirconium oxide, while the other 20 screws remain uncoated. The tibia of 10 adult white New Zealand experimental rabbits was chosen as implantation site, each rabbit tibia received 2 screws, one coated and the other uncoated. Torque removal test was performed to measure the torque required to remove the screw and histological analysis was performed to observe the new bone formation, after 2 and 4 weeks healing intervals. Results: Implant coated with a mixture of nano zirconium oxide and nano hydroxyl apatite showed a significantly higher removal torque values compared to uncoated one. There was more new bone formation with coated implants for both healing periods. Conclusions: Coating by electrophoresis considers a valuable process to coat metallic implants with a ceramic material and to form a uniform composite layer of coating. Osseointegration improved at bone-implant interface associated with the coated implants, which was illustrated by higher bone formation at the two intervals of time 2 weeks and 4 weeks.
In this study, hydroxyapatite (HAP, Ca10(PO4)6(OH)2) has been prepared as bioceramic material with biological specifications useful to used for orthopedic and dental implant applications. Wet chemical processing seems to form the fine grain size and uniform characteristic nanocrystalline materials by the interstice factors controlling which affected the grain size and crystallinity in order to give good mechanical and/or constituent properties similar as natural bone. Fluorinated hydroxyapatite [4-6 wt% F, (FHA, Ca10(PO4)6(OH)2–Fx] was developed in new method for its posses to increased strength and to give higher corrosion resistance in biofluids than pure HAP moreover reduces the risk of dental caries. The phase's and functional groups
... Show MoreIndustrial development has recently increased, including that of plastic industries. Since plastic has a very long analytical life, it will cause environmental pollution, so studies have resorted to reusing recycled waste plastic (sustainable plastic) to produce environmentally friendly concrete (green concrete). In this research, producing environmentally friendly load-bearing concrete masonry units (blocks) was considered where five concrete mixtures were compressed at the blocks producing machine. The cement content reduced from 400 kg/m3 (B-400) to 300 kg/m3 (B-300) then to 200 kg/m3 (B-200). While (B-380) was produced using 380 kg/m3 cement and 20 kg/m3 nano-sil
... Show MoreAbstract In the current contribution, a novel binuclear nickel(II) and zinc(II) complexes were prepared from a hexadentate ligand prepared via condensation of 3,3'-Bipyridine-6,6'-dicarbaldehyde , 2-amino-5-chlorobenzaldehyde and 2-Aminophenol .The symmetric ligand (H2DTPE) and its metal complexes were illustrated utilizing various techniques of physicochemical containing magnetic moment, analytical analysis and spectroscopy of mass, IR, 13C and 1H NMR, TGA and UV-Vis. The particles of MO Nanoscale were created from the labeled complex applying the ways of pyrolysis and utilizing methods of XRD, FT-IR, and FE-SEM, that specified close compatibility with the typical pattern for nanoparticles of NiO, ZnO and appeared the reasonable size in
... Show MoreIn the present paper, chitosan Schiff base has been synthesized from chitosan’s reaction with the salicyldehyde. The AuNPs was manufacture by extract of onion peels as a reducing agent. The Au NPs that have been prepared were characterized through the UV-vis spectroscopy, XRD analyses and SEM microscopy. The polymer blends of the chitosan Schiff base / PVP has been prepared through using the approach of solution casting. Chitosan Schiff base / PVP Au nano-composites was prepared. Nano composites and polymer blends have been characterized by FTIR which confirm the formation of Schiff base by revealing a new band of absorption at 1651cm-1 as a result of the (C=N) imine group. SEM, DSC and TGA confirms the thermal stability of
... Show MoreIn the present paper, chitosan Schiff base has been synthesized from chitosan’s reaction with the salicyldehyde. The AuNPs was manufacture by extract of onion peels as a reducing agent. The Au NPs that have been prepared were characterized through the UV-vis spectroscopy, XRD analyses and SEM microscopy. The polymer blends of the chitosan Schiff base / PVP has been prepared through using the approach of solution casting. Chitosan Schiff base / PVP Au nano-composites was prepared. Nano composites and polymer blends have been characterized by FTIR which confirm the formation of Schiff base by revealing a new band of absorption at 1651cm-1 as a result of the (C=N) imine group. SEM, DSC and TGA confirms the thermal stability of the pr
... Show MoreAbstract: The aim of this study was to evaluate the effect of bone density value in Hounsfield unit derived from cone beam computed tomography (CBCT), and implant dimensions in relation to implant stability parameters namely the resonance frequency analysis and the insertion torque (IT) value. It included 24 patients who received 42 dental implants (DI). The bone density of the planned implant site was preoperatively measured using cone beam computed tomography. The implant stability was measured using Osstell implant stability quotient (ISQ). The ISQ values were recorded immediately postoperatively and after 16 weeks. The IT value was categorized as 35 N/cm or > 35 N/cm. The mean (standard deviation) primary stability was 79.58 (5.27) ISQ,
... Show Moreفي هذا البحث تم تحضير المركبات المعدنية النانوية الجديدة لأيونات البلاتين 4+و الذهب 3+ مع ليكاند قاعدة مانخ جديد مشتق من السيبروفلوكساسين بطريقة الموجات فوق الصوتية. تم تشخيص المعقدات النانوية والليكاند الجديد بأستخدام تقنيات فيزيائية و كيميائية مختلفة مثل أطياف الاشعة تحت الحمراء، حيود الاشعة السينية ، المجهر الالكتروني الماسح ، المجهر الالكتروني النافذ و مجهر القوة الذرية. تم تحديد نشاط مضادات الأك
... Show MoreResilient polymeric materials such as silicone elastomers are currently used for maxillofacial prostheses construction but the strength of these materials and their clinical performance need to be optimized with the addition of reinforcing fillers. This study investigates the effect of zirconia nanopowder addition on tear strength, tensile strength, elongation at break, Shore A hardness, surface roughness and cytotoxicity of VST-50 maxillofacial silicone. Silicone base was mixed with different amounts (1%, 2% and 3%) of zirconia nanopowder using a vacuum mixer. Silicone without filler was used as control for comparison. Scanning Electron Microscopy and Atomic Force Microscopy were utilized to assess the efficiency of high-shear vacuum mixin
... Show More