Background: the aim of this study was to evaluate the effect of different surface acids treatments (37%phospjoric acid, 5%hydrofluoric acid, 1.23 acidulated phosphate fluoride) of feldspathic ceramic VITA 3D MASTER , and the effect of thermocycling on shear bond strength using a ceramic repair kit (ivoclar/vivadent). Material and Methods: sixty Nickel-Chromium metal base plates were prepared(9mm diameter,3mm depth) using lost wax technique, 2mm thick layer of ceramic(VITA 3D MASTER) fused to metal plates, all specimens were embedded in acrylic resin blocks except their examined surfaces and divided into 3 main groups 20 specimens each, Grp A: treatment with 37%phosphoric acid for 2 mins, Grp B: etching with 5% hydrofluoric acid for 2mins, Grp C: etching with 1.23% acidulated phosphate fluoride for 10 mins; monobond-plus, heliobond, resin composite(Tetric EvoCeram) were applied to each specimen according to manufacturer's instruction using transparent split mold(5mm diameter, 4 mm height); specimens were stored in 37OC distilled water for 12 weeks, 10 specimens of each group were subjected to thermocycling between 5 oC and 55 o C for 800 cycles with 30s dwell time; shear bond strength was determined by a universal testing machine (instron 1122) at a cross head speed 0.5mm/min; One way ANOVA test, LSD test and student-t test were used to analyze shear bond strength. Results: Mean shear bond strength values for the tested groups were: A1= 11.65±0.68 Mpa, A2=10.88±0.58 Mpa, B1=17.93±0.41 Mpa, B2=17.42±0.35 Mpa, C1=15.17±0.61 Mpa, C2=14.51±0.48 Mpa ; one way ANOVA test showed highly significant difference among groups; LSD test revealed that the use of 5% HF for ceramic surface treatment(GB) was highly significant than the treatment with 37%PA(GA) or 1.23%APF(GC) respectively and the use of 1.23%APF(GC) was highly significant than the use of 37%PA(GA); Student t- test showed a significant difference between subgroups of the same group with and without thermocycling. Conclusion: ceramic surface treated with 5% HF acid for 2 mins recorded the highest shear bond strength, followed by surface treatment with 1.23% APF for 10 mins, most specimens treated with 5%HF showed cohesive failure with in ceramic while specimens treated with 1.23%AFP showed more (adhesive/cohesive) failure than adhesive or cohesive alone, and specimens treated with 37% PA showed nearly 50:50 adhesive and combination failure, thermocycling reduced the bond strength of each group significantly
The aim of this study was to evaluate tensile properties of low and medium carbon ferrite -martensite dual phase steel, and the effect cryogenic treatment at liquid nitrogen temperature (-196 ºC) on its properties. Low carbon steel (C12D) and medium carbon steels (C32D & C42D) were used in this work. For each steel grade, five groups of specimens were prepared according to the type of heat treatment. The first group was normalized, the second group was normalized and subsequently subjected to cryogenic treatment then tempered at (200 ºC) for one hour, the third group was quenched from intercritical annealing temperature of (760 ºC) to obtain dual phase (DP) steel, the fourth and fifth groups were both quenched from (760 ºC), but
... Show MoreZSM-5 zeolite was synthesis under hydrothermal conditions at 175oC. The synthesis parameters have been investigated to find optimum synthesis method. Firstly, the crystallization time has been investigated to find the optimum crystallization time. Also, the ageing time was studied. The morphology, structure, and composition of the synthesized ZSM-5 zeolite were characterized using scanning electron microscopy (SEM), pH meter, viscometer, and X-ray powder diffraction (XRD). The bulk Si/Al ratio of ZSM-5 zeolite was in the range of 9.5—11.7. The synthesized ZSM-5 zeolite with appropriate ageing time could adjust crystal size and degree of the crystallinity. The crystal size of ZSM-5 zeolite obtained at an agei
... Show MoreNisoldipine (NSD) is a dihydropyridine class of calcium channel blockers used for hypertension treatment, it belongs to class II BCS (low solubility with high permeability), its absolute bioavailability is only 5% due to presystemic metabolism in the gut wall. It is also a substrate for a CYP3A and P-gp. Bilosomes are lipid bilayer vesicles incorporating bile salts in their walls to prevent degredation by GIT bile salts. The aim of this study is to prepare nisoldipine bilosomes as vesicular carrier and assess the effect of different formulation variables such as type of surfactant, amount of cholesterol, surfactant and sonication time on particle size, entrapment efficiency and poly dispersity index of the prepared bilos
... Show MoreBackground: Wounds are any disruption to the normal anatomic structure of tissue which leads to the loss of epithelial continuity with or without a loss of underlying connective tissue, as well as the anatomic and functional integrity of the living tissue . Wound healing is a complex process with overlapping phases haemostasis, inflammation, proliferation and maturation/matrix Remodeling. Each phase of wound healing requires different management strategies, and inappropriate treatment can delay wound healing. The aim of wound treatment is a rapid wound closure and re-establish tissue function,chia seeds oil are widely used herbal medicines because of their anti-inflammatory and antioxidant capacity as they considerd agood source of polyunsa
... Show Moren-Hexane conversion enhancement was studied by adding TCE (Trichloro-ethylene) on feed stream using 0.3%Pt/HY zeolite catalyst. All experiments were achieved at atmospheric pressure and on a continuous laboratory unit with a fixed bed reactor at a temperature range 240-270◦C, LHSV 1-3h-1, H2/nC6 mole ratio 1-4.
By adding 435 ppm of TCE, 49.5 mole% conversion was achieved at LHSV 1h-1, temperature of 270ºC and H2/nC6 mole ratio of 4, while the conversion was 18.3 mol% on the same catalyst without adding TCE at the same conditions. The activation energy decreased from 98.18 for pure Pt/HY zeolite to 82.83 kJ/mole by adding TCE. Beside enhancement the activity, selectivity and product distribution enhanced by providing DMB (Dimethyl b
Cold atmospheric plasma (CAP) is used widely in medical and biological fields because of non-thermal effected. Direct application of plasma is preferred in medical functions, so, direct application of cold plasma has obtained by the floating electrode dielectric barrier discharge (FE-DBD) system. The purpose of this paper to review the effect of (CAP) on the reproductive hormones (testosterone, LH, E2, progesterone, for male rats. The study appeared that no significant effect on E2 and progesterone hormone for all time of exposure, besides this significant difference in LH hormone (P<0.05) at 15 sec, (P<0.0001) at 30, 90 sec and (P<0.001) at 60 sec of exposure to plasma. Added to that significant difference (P<0.01) at 15, 30, 60 sec and no
... Show MoreBackground: The healing period for bone–implant contact takes 3–6 months or even longer. Application of Escherichia coli-derived recombinant human bone morphogenetic protein-2 (ErhBMP-2) to implant surfaces has been of great interest on osseointegration due to its osteoinductive potential. The objective of this study was to evaluate the effect of ErhBMP-2 on implant stability. Materials and methods: A total of 48 dental implants were inserted in 15 patients. Twenty four implants coated with 0.5 mg/ml ErhBMP-2 (study group). The other 24 implants were uncoated (control group). Each patient was received at least two dental implants at the same session. Both groups were followed with repeated implant stability measurements by me
... Show MoreThe aim of the present work is to develop a new class of natural fillers based polymer composites with sawdust (S.D) which used two particle sizes (1.2 μm & 2.3 μm) and different weight percentage from sawdust (10%, 15%, and 20%). The mechanical properties studied include hardness (shore D) for all samples at normal conditions (N.C). The unsaturated polyester (UPE) and its composites samples were immersed in water for 30 days to find the effect of particle size of sawdust (S.D) on the weight gain (Mt %) by water for all the samples, also to find the effect of water on their hardness. The results show that the composite materials of sawdust (S.D) fillers which has particle size (1.2 μm) better than (2.3 μm) particle size bef
... Show More