Background: Separation and deboning of artificial teeth from denture bases present a major clinical and labortory problem which affect both the patient and the dentist. The optimal bond strength of artificial teeth with denture base reinforced with nanofillers and flexible denture bases and the effect of thermo cycling should be evaluated. This study was conducted to evaluate and compare the shear bond strength of artificial teeth (acrylic and porcelain) with denture bases reinforced by 5% Zirconium oxide nanofillers and flexible bases under the effect of different surface treatments and thermo cycling and comparing the results with conventional water bath cured denture bases. Material and methods: Two types of artificial teeth; acrylic and porcelain were used and prepared for this study. Five specimens of each tooth type were processed to each denture base materials after the application of different surface treatments; these teeth were bonded to heat polymerized, nano composite resin and flexible denture bases. Specimens were thermo cycled and tested for bond strength until fracture with an Instron universal testing machine. Data were analyzed with analysis of variance and student T-test. Photomicrographic examinations were used to identify adhesive and cohesive failures within debonded specimens. Results: The mean force required to fracture the specimens were obviously larger for nanocomposite specimens compared with the heat cured and flexible specimens. The most common failure was cohesive within the tooth or the denture base. With each base material, the artificial teeth which were treated with thinner exhibited highest shear bond strength. Thermocycling had deleterious effect on the flexible denture base specimens. In general, nanocomposite and heat cured groups failed cohesively within the artificial tooth. While the valplastic groups failed adhesively at the tooth denture base interface. Conclusions: Within the limitations of this study, the type of denture base materials and surface treatments of the tooth selected for use may influence the shear bond strength of the tooth to the base. Selection of more compatible combinations of base and artificial teeth may reduce the number of prosthesis fractures and resultant repairs. Key words: acrylic teeth, porcelain teeth, Nano composite denture base, thermo cycling, flexible denture, thinner,
Objective: The aim of this study was to evaluate the effect of pumice, burning investment material
and black sand on the surface roughness of heat cure acrylic resin.
Methodology: Sixty specimens were prepared from pink heat cure acrylic resin, the specimens
where grouped into; 20 specimens which polished with pumice and water (control group); 20
specimens which polished with investment material (after burning it) and water; and 20 specimens
which polished with black sand and water. The average surface roughness of specimens after
polishing procedure had been determined by profilometer (surface roughness tester).
Results: Through the application of ANOVA and LSD tests, the result of this study showed that there
wa
Background: The aim of this study was to evaluate the push-out bond strength of four different obturation materials to intraradicular dentin and to determine the failure mode. Materials and method: forty straight palatal roots of the maxillary first molars teeth were used in this study, the roots were instrumented using crown down technique and rotary EndoSequence system, the roots were randomly divided into four groups according to the materials used for obturation (n=10).Group (1): AH Plus sealer and gutta-percha. Group (2): Activ GP glass ionomer sealer and Activ GP gutta-percha (Activ GP system). Group (3): Bioceramic sealer and Bioceramic gutta-percha. Group (4): GuttaFlow2 sealer and gutta-percha. For all groups single cone obturatio
... Show MoreBackground: The aim of this study was to evaluate the effect of thermo cycling and different pH of artificial saliva (neutral, acidic, basic) on impact and transverse strength of heat cure acrylic resin reinforced of with 5% silanated ZrO2 nano fillers. Materials and methods: 120 samples were prepared, 60 samples for impact strength test and another 60 samples for transverse strength test, for each test, samples were divided into two major groups (before and after thermo cycling), then each of these major groups were further subdivided into 3 subgroups according to the pH of prepared artificial saliva (neutral, acidic, basic). Charpy impact device was used for impact strength test and Flexural device was used for transverse strength test. R
... Show MoreBackground: This study was performed to determine the effect of aging of different types of composite material restorations on: Shear bond strength (SBS) to light cure and no mix chemical cure orthodontic adhesives with sapphire bracket and the debonding failure sites. Materials and methods: One hundred forty four composite disks were made from three different composite resin materials which are: 3M Filtek Z250, 3M filtek Z350 and 3M Valux plus, each group with (48) disks each, then according to the duration of storage each group was subdivided into two equal groups one of them stored for one day and the other was stored for one month, then each group was further subdivided into two equal subgroups with (12) disks each one bonded with ligh
... Show MoreBackground: The main drawback of soft lining materials was that they debonded from the denture base after a certain period of usage. Therefore, the purpose of this research was to determine the impact of oxygen and argon plasma treatment on the shear bonding strength of soft liners to two different kinds of denture base materials: conventional acrylic resin and high impact acrylic resin. Materials and Methods: Heat cure conventional and high impact acrylic blocks (40 for each group) were prepared. A soft liner connected the final test specimen of two blocks of each acrylic material. Shear bond strength (SBS) was assessed using universal testing machine. Additional blocks were also prepared for analyzing Vickers microhardness, contact ang
... Show MoreBackground: The aim of this study was to evaluate the shear bond strength (SBS) and adhesive remnant index (ARI) of different orthodontic adhesive systems after exposure to aging media (water storage and acid challenge). Materials and methods: Eighty human upper premolar teeth were extracted for orthodontic purposes and randomly divided into two groups (40 teeth each): the first group in which the bonded teeth were stored in distilled water for 30 days at 37°C, and the second group in which the bonded teeth were subjected to acid challenge. Each group was further subdivided into four subgroups (10 teeth each) according to the type of adhesive system that would be bonded to metal brackets: either non-fluoride releasing adhesive (NFRA),
... Show MoreBackground: With the increased in the demands of adult orthodontics, the challenge of direct bonding to non-enamel surface (zirconium) had been increased. The present study was carried out to compare the shear bond strength of three different brackets (stainless steel, sapphire and composite) bonded to zirconium surface and study the mode of bond failure. Materials and methods: The sample was comprised of 30 models (8mm *6mm*1.5mm) of full contour zirconium veneers. They were divided into three groups according to the brackets type; all samples were treated first by sandblast with aluminum oxide particle 50 µm then coated by z-prime plus primer. A central incisor bracket of each group was bonded to the prepared zirconium surface with lig
... Show MoreBackground: This study was conducted to assess the effects of various beverages on the shear bond strength of light-cured orthodontic composite used to bond stainless steel orthodontic brackets on human teeth and to determine the site of bonding failure of this material. Materials and Methods: Fifty extracted human premolars were selected and randomly divided into five equal groups each with 10 teeth according to the beverage type (Control, One Tiger, Milk, Green tea and Coffee). After bonding, the teeth were immersed in specific beverages for 5 minutes twice daily with equal intervening intervals then washed and stored in distilled water at 37º C for the reminder of the day. The process was carried out for 30 days. The samples were then
... Show MoreBackground: evaluate the effects of three different intracoronal bleaching agents on the shear bond strengths (SBS) and failure site of stainless steel and monocrystalline (sapphire) orthodontic brackets bonded to endodontically treated teeth using light cured orthodontic adhesive in vitro. Materials and methods: Eighty extracted sound human upper first premolars were selected, endondontically treated and randomly divided equally (according to the type of the brackets used) into two main groups (n = 40 per group). Each main group were subdivided (according to the bleaching agent used) into four subgroups 10 teeth each; as following : control (un bleached) group, hydrogen peroxide group (Hp) 35%, carbamide peroxide group (CP) 37% group and s
... Show More