Background: Separation and deboning of artificial teeth from denture bases present a major clinical and labortory problem which affect both the patient and the dentist. The optimal bond strength of artificial teeth with denture base reinforced with nanofillers and flexible denture bases and the effect of thermo cycling should be evaluated. This study was conducted to evaluate and compare the shear bond strength of artificial teeth (acrylic and porcelain) with denture bases reinforced by 5% Zirconium oxide nanofillers and flexible bases under the effect of different surface treatments and thermo cycling and comparing the results with conventional water bath cured denture bases. Material and methods: Two types of artificial teeth; acrylic and porcelain were used and prepared for this study. Five specimens of each tooth type were processed to each denture base materials after the application of different surface treatments; these teeth were bonded to heat polymerized, nano composite resin and flexible denture bases. Specimens were thermo cycled and tested for bond strength until fracture with an Instron universal testing machine. Data were analyzed with analysis of variance and student T-test. Photomicrographic examinations were used to identify adhesive and cohesive failures within debonded specimens. Results: The mean force required to fracture the specimens were obviously larger for nanocomposite specimens compared with the heat cured and flexible specimens. The most common failure was cohesive within the tooth or the denture base. With each base material, the artificial teeth which were treated with thinner exhibited highest shear bond strength. Thermocycling had deleterious effect on the flexible denture base specimens. In general, nanocomposite and heat cured groups failed cohesively within the artificial tooth. While the valplastic groups failed adhesively at the tooth denture base interface. Conclusions: Within the limitations of this study, the type of denture base materials and surface treatments of the tooth selected for use may influence the shear bond strength of the tooth to the base. Selection of more compatible combinations of base and artificial teeth may reduce the number of prosthesis fractures and resultant repairs. Key words: acrylic teeth, porcelain teeth, Nano composite denture base, thermo cycling, flexible denture, thinner,
The new tridentate Schiff base ligand (HL)namely 2-{[1-(3-amino-phenyl)-ethylidene]-hydrazono methyl}- phenol containing (N N O)as donors atoms was prepared in two steps:Step (1): By the reaction of 3- aminoacetophenone with hydrazine monohydrate under reflux in methanol and drops of glacial acetic acid gave the intermediate compound 3-(1- hydrazono ethyl)-phenol amine.Step (2): By the reaction of 3-(1-hydrazono ethyl)-phenol amine with salicyaldehyde under reflux in methanol, gave the ligand (HL).The prepared ligand was characterized by I.R, U.V-Vis,1H- 13C NMR spectra and melting point and reacted with some metal ions under reflux in methanol with (1:1) ratio gave complexes of the general formula: [MClL]. Where: M= Mn(II), Fe(II), Co(II),
... Show MoreBackground: Curve of Spee (CS) is an anteroposterior anatomical curve established by the occlusal alignment of the teeth viewed in the sagittal plane. This occlusal curvature has clinical importance in orthodontics and other fields of dentistry. This study aimed to evaluate the relationship between the CS and dentofacial morphology of different skeletal patterns in both genders. Materials and Methods: Eighty six Iraqi Arab subjects (44females,42 males ) their age ranged from 17 -30 years, classified into: Skeletal I with normal occlusion(15 females and 15 males), skeletal II with CI II div 1 malocclusion (15 females and 15 males) and skeletal III with CI III malocclusion (14 females and 12 males). Forty one variables measured us
... Show MoreAn experimental study was conducted on pressure drop of water flow through vertical cylindrical packed beds in turbulent region and the influence of the operating parameters on its behavior. The bed packing was made of spherical and non-spherical particles (spheres, Rasching rings and intalox saddle) with aspect ratio range 3.46 D/dp 8.486 obtaining bed porosities 0.396 0.84 and Reynolds number 1217 21758. The system is consisted of 5 cm inside diameter Perspex column, 50 cm long; distilled water was pumped through the bed with flow rate 875, 1000, 1125, 1250,1375 and 1500 l/h and inlet water temperature 20, 30, 40 and 50 ˚C. The packed bed system was monitored by using LabVIEW program, were the result
... Show MoreKE Sharquie, JR Al-Rawi, AA Noaimi, HM Al-Hassany, Journal of drugs in dermatology: JDD, 2012 - Cited by 47