Background: Separation and deboning of artificial teeth from denture bases present a major clinical and labortory problem which affect both the patient and the dentist. The optimal bond strength of artificial teeth with denture base reinforced with nanofillers and flexible denture bases and the effect of thermo cycling should be evaluated. This study was conducted to evaluate and compare the shear bond strength of artificial teeth (acrylic and porcelain) with denture bases reinforced by 5% Zirconium oxide nanofillers and flexible bases under the effect of different surface treatments and thermo cycling and comparing the results with conventional water bath cured denture bases. Material and methods: Two types of artificial teeth; acrylic and porcelain were used and prepared for this study. Five specimens of each tooth type were processed to each denture base materials after the application of different surface treatments; these teeth were bonded to heat polymerized, nano composite resin and flexible denture bases. Specimens were thermo cycled and tested for bond strength until fracture with an Instron universal testing machine. Data were analyzed with analysis of variance and student T-test. Photomicrographic examinations were used to identify adhesive and cohesive failures within debonded specimens. Results: The mean force required to fracture the specimens were obviously larger for nanocomposite specimens compared with the heat cured and flexible specimens. The most common failure was cohesive within the tooth or the denture base. With each base material, the artificial teeth which were treated with thinner exhibited highest shear bond strength. Thermocycling had deleterious effect on the flexible denture base specimens. In general, nanocomposite and heat cured groups failed cohesively within the artificial tooth. While the valplastic groups failed adhesively at the tooth denture base interface. Conclusions: Within the limitations of this study, the type of denture base materials and surface treatments of the tooth selected for use may influence the shear bond strength of the tooth to the base. Selection of more compatible combinations of base and artificial teeth may reduce the number of prosthesis fractures and resultant repairs. Key words: acrylic teeth, porcelain teeth, Nano composite denture base, thermo cycling, flexible denture, thinner,
The change in project cost, or cost growth, occurs from many factors, some of which are related to soil problem conditions that may occurs during construction and/or during site investigation period. This paper described a new soil improvement method with a minimum cost solution by using polymer fiber materials having a length of (3 cm) in both directions and (2.5 mm) in thickness, distributed in uniform medium dense .
sandy soil at different depths (B, 1.5B and 2B) below the footings. Three square footings has been used (5,7.5 and 10 cm) to carry the above investigation by using lever arm loading system design for such purposes.
These fibers were distributed from depth of (0.1B) below the footing base down to the investigated dep
This study involves adding nano materials and interaction with cement mortar behavior for several mortar samples under variable curing time with constant water to cement ratio (W/C = 0.5). The effects of adding nano materials on the microstructure of cement mortar were studied by (Scanning Electronic Microscopy (SEM) and X-Ray (for samples at different curing time 28 and 91 days. Small ratio replacements of nano particles (SiO2 or Al2O3) were added to Ordinary Portland Cement (OPC) type (I). The percentage of nano materials additives replacement by weight of ordinary Portland cement includes (1, 2, 3, 4 and 5%) for both types of nano materials with constant (W/C) ratio, also the amount of the fin
... Show MoreUltra-High Temperature Materials (UHTMs) are at the base of entire aerospace industry; these high stable materials at temperatures exceeding 1600 °C are used to manage the heat shielding to protect vehicles and probes during the hypersonic flight through reentry trajectory against aerodynamic heating and reducing plasma surface interaction. Those materials are also recognized as Thermal Protection System Materials (TPSMs). The structural materials used during the high-temperature oxidizing environment are mainly limited to SiC, oxide ceramics, and composites. In addition to that, silicon-based ceramic has a maximum-use at 1700 °C approximately; as it is an active oxidation process o
The prostaglandins inside inflamed tissues are produced by cyclooxygenase-2 (COX-2), making it an important target for improving anti-inflammatory medications over a long period. Adverse effects have been related to the traditional usage of non-steroidal anti-inflammatory drugs (NSAIDs) for the treatment of inflammation, mainly centered around gastrointestinal (GI) complications. The current research involves the creation of a virtual library of innovative molecules showing similar drug properties via a structure-based drug design. A library that includes five novel derivatives of Diclofenac was designed. Subsequently, molecular docking through the Glide module and determining the binding free energy implementing the P
... Show MoreThe current investigation included study of leaf surface epidermis beside indumentum for the species Galium aparine L., G. ceratopodum Boiss, G. setaceum Lam., G. spurium L., and G. tricornatum Dandy, the study showed that paracytic type of stomatal complex is the only type occur in leaf. The indumentum compose of eglandular hairs vary in their apices, length and occurrence of different part of plant body
Background: The purpose of this study is to compare the color changes between the bonded middle third and the unbonded gingival and incisal thirds, fallowing fixed orthodontic treatment Material and method: The color parameter l, a, b has been recorded for each thirds in upper anterior teeth by mean of easy shad device. The has been calculated for gingival, middle and incisal thirds for the upper anterior teeth in 34 patient, 17 males and 17femals, those subject undergone fixed orthodontic treatment Results: The in middle bonded third is highly significant higher than that in incise and gingival thirds p<0.01 because the middle third isn’t expose to oral fluid and dental brushing since it covered by the bracket. Also there
... Show MoreBackground: The purpose of this study was to assess the relation among the ramal length and width with various cervical and cranio-facial measurements for a sample of Iraqi adults with different skeletal classes. Materials and method: The sample composed of 71 Iraqi adults (36 females and 35 males) with an age ranged between 17-30 years and had different skeletal mal-relations using SNA, SNB and ANB to differentiate between them and assorting them into CL.I, CL.II and CL.III mal-relation. Each individual was subjected to clinical examination and digital true lateral cephalometric radiograph that had been analyzed using AutoCAD 2007 software computer program to determine sixteen linear and ten angular measurements. Descriptive statistics wer
... Show More