Background: This in vitro study was carried out to evaluate the effects of various veneering dentin ceramic thicknesses and repeated firings on the color of lithium disilicate glass-ceramic (IPS e.max Press) and zirconium-oxide (IPS ZirCAD) all-ceramic systems, measured by clinical spectrophotometers (Easyshade Advance 4.0) . Materials and methods: The 72specimens cube-shaped have the dimension of about 11 mm in width, 14 mm in length, 1mm in thickness, these cores divided into 3 groups according to the type of material each group have (24)core specimens. Each group had been divided into three sub-groups (each having 8 specimens) according to veneering with dentin ceramic thicknesses: as 0.5, 1, or 2 mm (n=8). IPS e.max press and ZirCAD cores group had been veneered with IPS e.max Ceram dentin ceramic shade A2 according to manufacturer’s instructions and the metal group had been veneered with IPS classic dentine ceramic with shade A2 according to manufacturer’s instructions. Repeat firings (3, 5 and 7 times) had been applied on all the specimens. Color differences among ceramic specimens had been measured using a clinical spectrophotometer (VITA Easyshade); the color data had been expressed according the Vita Classic shade guide. Results: The shade of all specimens had been compared inside the subgroups and with the main groups. The percentage of color agreement among the subgroups showed the color of all ceramic systems had been affecting by firing interval, the ceramic thickness and brand of ceramic. The number firings intervals applied on the all ceramic system has a significant effect on the final color, the increase of firing number change the color to a darker and reddish color. The 5th firing interval is the point at which the major color changes happened (darker shade), and in next interval (7th firing) less color changes happened. The thickness of veneering ceramic affected the color significantly. The 0.5 mm specimens in all groups showed the highest percentage of agreement (less color changes) after firing intervals, then the 1mm came and the least percentage of agreement ( highest color changes ) was the 2 mm specimens. The Brand of veneering ceramic and the type of core record a significance difference in color changes when exposed to firing heat. Conclusion: With limit of this study, the final color of the all ceramic system definitely affected by the number of firing cycle exposed to, and the veneering ceramic thickness have a clear effect on the final shade of the all ceramic tested.
Background: Ceramic veneers represent the treatment of choice in minimally invasive esthetic dentistry; one of the critical factors in their long term success is marginal adaptation. The aim of the present study is to evaluate the marginal gap of ceramic veneers by using two different fabrication techniques and two different designs of preparation. Material and methods: A typodont maxillary central incisor used in the preparation from which metal dies were fabricated, which were in turn used to make forty stone dies. The dies divided into four experimental groups, each group had ten samples: A1: prepared with butt-joint incisal reduction and restored with IPS e.max CAD, A2: prepared with overlapped incisal reduction and restored with IPS e.
... Show MoreThis study aims to test ceramic waste's capacity to remove nickel from aqueous solutions through adsorption. Ceramic wastes were collected from the Refractories Manufacturing Plant in Ramadi. Through a series of lab tests, the reaction time (5, 10, 15, 20, 25, 30, 35, 40, 45, and 50 minutes, and Ni concentrations (20, 40, 60, and 80) were tested using ceramic wastes with a solid to liquid ratio of 2g/30ml. At a temperature of 30ºC, the pH, total dissolved solids (TDS), and electrical conductivity (EC) were all measured. The equilibrium time was set at 30 min. Thereafter, the sorption (%) somewhat increased positively with the Ni concentration. Freundlich's equation showed that the adsorption intensity is 1.1827 and the Freundlich c
... Show MoreZinc sulfide(ZnS) thin films of different thickness were deposited on corning glass with the substrate kept at room temperature and high vacuum using thermal evaporation technique.the film properties investigated include their absorbance/transmittance/reflectance spectra,band gap,refractive index,extinction coefficient,complex dielectric constant and thickness.The films were found to exhibt high transmittance(59-98%) ,low absorbance and low reflectance in the visible/near infrared region up to 900 nm..However, the absorbance of the films were found to be high in the ultra violet region with peak around 360 nm.The thickness(using optical interference fringes method) of various films thichness(100,200,300,and 400) nm.The band gap meas
... Show MoreA particulate composite material was prepared by adding the Titanium dioxide (TiO2) with a particle size of (75-150) µm to Epoxy resin at weight percentage of (10%,20%,30%,40%,50%).The following some mechanical properties were studied,fracture toughness, hardness.casting preparation methods were used in this study includes preparing plate of matrix and composites. specimens were prepared according to ASTM for the Mechanical properties tests. After that Another samples were heat treated for three and six hour at 65C?. Fracture toughness (Kic) represent for stress intensity factor results were showed that the curve of three hours aging increases in fracture toughness (Kic) for composites but for six hours aging increases fracture tough
... Show MoreThe use of different materials in the art of ceramics is considered a new form of contemporary philosophical trends. That was introduced to art as a result of societal changes and transformations and rapid technological development. And it plays a very essential part in the beauty of the artistic structure. The contrast of using different materials in ceramics is considered a part of the old historical achievements since the art of ceramics used to follow strict standards. Which does not apply to contemporary ceramic, Because recently, it has become free from any religious and social control and created a whole new intellectual context, heading to new horizons in which it works with the newly added materials as a strategy to ensure the a
... Show MorePolymer matrix composites are suitable materials for medical applications, such as denture base resin polymethyl methacrylate (PMMA). This includes light weight and high strength. This paper describes the effect of selected weight fractions (1, 2, 3, 4 & 5) % wt of nano(Alumina AL2O3, Zirconia ZrO2, Hydroxyapatite HA and Halloysite nanoClay) reinforcements on the biopolymer matrix (PMMA). Some tribology tests were used to evaluate the prepared system (impact strength, hardness surface, and wear rate) tests. The samples were fabricated by (Hand Lay-Up) with different particle reinforcement percentages. All tests were accomplished at room temperature, and samples were developed according to the ASTM standard. The weight fraction of (4% for AL
... Show MorePolymer matrix composites are suitable materials for medical applications, such as denture base resin polymethyl methacrylate (PMMA). This includes light weight and high strength. This paper describes the effect of selected weight fractions (1, 2, 3, 4 & 5) % wt of nano(Alumina AL2O3, Zirconia ZrO2, Hydroxyapatite HA and Halloysite nanoClay) reinforcements on the biopolymer matrix (PMMA). Some tribology tests were used to evaluate the prepared system (impact strength, hardness surface, and wear rate) tests. The samples were fabricated by (Hand Lay-Up) with different particle reinforcement percentages. All tests were accomplished at room temperature, and samples were developed according to the ASTM standard. The weight fraction o
... Show MoreA thin CdS Films have been evaporated by thermal evaporation technique with different thicknesses (500, 1000, 1500 and 2000Å) and different duration times of annealing (60, 120 180 minutes) under 573 K annealing temperature, the vacuum was about 8 × 10-5 mbar and substrate temperature was 423 K. The structural properties of the films have been studied by X- ray diffraction technique (XRD). The crystal growth became stronger and more oriented as the film thickness (T) and duration time of annealing ( Ta) increases.
Al-Si alloys which are widely used in engineering applications due to their outstanding properties can be modified for more enhancements in their properties. Current work investigated the ability of these alloys to be modified by casting them through the addition of nanoparticles. So, Multi-wall carbon nanotubes (CNT) and titanium carbide ceramic particles (TIC) with size of (20 nm) were added with different amounts started from (0.5 up to 3%) weight to cast alloy A356 that was considered to be the base metal matrix, then stirred with different speeds of (270, 800, 1500, 2150) rpm at 520 °C for one minute. The results showed change in microstructure’ shape of the casted alloys from the dendritic to spherical gra
... Show More