Background: To evaluate the ISO depth of cure of bulkfill composites and depth of cure which determined by Vickers microhardness test. Materials and Methods: Bulkfill resin composite specimens (n=150) were prepared of three bulkfill composite materials (TetricEvo Ceram, Quixfil and SDR) and light cured by Flash max p3 for 3, 10, 20 seconds and by wood pecker for 10, 20 seconds respectively, a mold was filled with one of the three bulkfill composites and light cured. The specimens removed from the mold and scraped by plastic spatula and the remaining length (absolute length) was measured which represent the ISO depth of cure. After that the specimens were returned into the mold and a microhardness indentation device applied on the specimen and hardness measurements (Vickers hardness, VHN) were made at defined distance, beginning at the resin composite that had been closest to the light curing unit (i.e. at the top) and proceeding toward the uncured resin composite (i.e. toward the bottom) on the basis of the VHN measurement, Vickers hardness test generated for each group. Results and Conclusion: ISO depth of cure of bulkfill composite materials is time and type of light curing protocol dependent rather than type of material of bulkfill composite while the depth of cure determined by Vickers hardness number is material dependent in addition to the light curing protocol. Key words: Bulkfill composite light curing intensity, depth of cure.
The study concern with the preparation of three type of mixtures; which are prepared from different percentage of polyvenil Butyral, Di-n-butyl phathalate and paraffin wax pastillated. The solvent used is Xylolzul analyses. After washing, Drying and milling the kaolin Dukhla, as a matrix in this study, and by using sieving Tech. The range of particle size used is less than and less than as a mesh batch. The added percentage from prepared mixture were 5% and 10% to 95% and 90% of the matrix respectively. Then disk samples were prepared by using a compaction pressure with heating. After cooling and drying the samples were undergo heat treatment in the range of (1250 – 1350) oC. The measurement of shrinkage and Dielectric properties sho
... Show MoreCuInSe2(CIS) thin films have been prepared by use vacuum thermal evaporation technique, of thickness750 nm with rate of deposition 1.8±0.1 nm/sec on glass substrate at room temperature and pressure (10-5) mbar. Heat treatment has been carried out in the range (400-600) K for all samples. The optical properties of the CIS thin films are been studied such as (absorption coefficient, refractive index, extinction coefficient, real and imaginary dielectric constant) by determined using Measurement absorption and transmission spectra. Results showed that through the optical constants we can make to control it are wide applications as an optoelectronic devices and photovoltaic applications.
Background: The preparation of Platelet-rich plasma (PRP) is minimally invasive way, simple, low cost to obtain natural autologous growth factors and is now being widely used in different fields of medicine for its ability to increase the regeneration potential of tissue. The aim of this study was to investigate the effect of local application of autologous PRP gel on acceleration rate of osseointegration period by clinical assessment accomplished by determining the changes in implant stability during 3 months healing period using resonance frequency analysis (RFA). Materials and methods: A total of 28 dental implants were inserted in edentulous maxillae or mandibles of 13 patients using a split mouth design, i.e. each patient was received
... Show MoreChitosan (CH) / Poly (1-vinylpyrrolidone-co-vinyl acetate) (PVP-co-VAc) blend (1:1) and nanocomposites reinforced with CaCO3 nanoparticles were prepared by solution casting method. FTIR analysis, tensile strength, Elongation, Young modulus, Thermal conductivity, water absorption and Antibacterial properties were studied for blend and nanocomposites. The tensile results show that the tensile strength and Young’s modulus of the nanocomposites were enhanced compared with polymer blend [CH/(PVP-co-VAc)] film. The mechanical properties of the polymer blend were improved by the addition of CaCO3 with significant increases in Young’s modulus (from 1787 MPa to ~7238 MPa) and tensile strength (from 47.87 MPa to 79.75 MPa). Strong interfacial
... Show MoreEP/ metal composites were prepared as adhesives between two steel rods. Epoxy resin (EP) was used as a matrix with metal as fillers (Al, Cu, Fe,).
The preparation method for tensile adhesion tests includes two steel rods with adhesive composites between the rods to measure adhesion strength Sad and adhesion toughness Gad.
Results of tensile adhesion tests show that EP/ metals composite have maximum strength Sad for certain weight percentage of metals 2.95 and 9MPa at 10% for EP/Al and EP/Cu composite and 8.2MPa at 40% for EP/Fe composites