Background: To evaluate the ISO depth of cure of bulkfill composites and depth of cure which determined by Vickers microhardness test. Materials and Methods: Bulkfill resin composite specimens (n=150) were prepared of three bulkfill composite materials (TetricEvo Ceram, Quixfil and SDR) and light cured by Flash max p3 for 3, 10, 20 seconds and by wood pecker for 10, 20 seconds respectively, a mold was filled with one of the three bulkfill composites and light cured. The specimens removed from the mold and scraped by plastic spatula and the remaining length (absolute length) was measured which represent the ISO depth of cure. After that the specimens were returned into the mold and a microhardness indentation device applied on the specimen and hardness measurements (Vickers hardness, VHN) were made at defined distance, beginning at the resin composite that had been closest to the light curing unit (i.e. at the top) and proceeding toward the uncured resin composite (i.e. toward the bottom) on the basis of the VHN measurement, Vickers hardness test generated for each group. Results and Conclusion: ISO depth of cure of bulkfill composite materials is time and type of light curing protocol dependent rather than type of material of bulkfill composite while the depth of cure determined by Vickers hardness number is material dependent in addition to the light curing protocol. Key words: Bulkfill composite light curing intensity, depth of cure.
Background: White spot lesions (WSLs) are subsurface enamel demineralization manifested as white opacities which had an esthetic problem. The purpose of this in-vitro study was to evaluate the lesion depth improvement of WSLs following application of fluoride varnish, tooth mousse and resin infiltration (ICON). Materials and methods: Artificial WSLs were created on 120 premolar teeth using demineralization solution with pH (4-4.5). Samples randomly allocated into four groups; fluoride varnish, tooth mousse, ICON and untreated group. Groups were discolored in Cola and orange juice for 24 hours. Teeth were ground sectioned by longitudinal cutting then these sections examined and photographed under stereomicroscope at 12X magnification then an
... Show MoreObjectives: The purpose of this in vitro study was to compare the effect of adding poloxamer surfactant to irrigant solutions on the penetration de..
Experimental investigations had been done in this research to demonstrate the effect of carbon fiber and Ceramic fillers contents on the tribological behaviour of (15% volume fraction) carbon-epoxy composite system under varying volume fraction, load, time and sliding distance. The wear resistance were investigated according to ASTM G99-05standard using pin on disc machine to present the composite tribological behaviour. The influence of three ceramic fillers, granite, perlite and calcium carbonate (CaCO3), on the wear of the carbon fabric reinforced epoxy composites under dry sliding conditions has been investigated. The effect of variants in volume fraction, applied load, time and sliding distance on the wear behaviour of po
... Show MoreBackground: Denture cleansing was an important step that could prevent the spread of infection and improve a patient's health, the durability of the dentures, and the overall quality of life; therefore, it was necessary to choose a suitable cleanser that, in addition to being effective, did not have an unfavorable effect on the qualities of the denture base resin itself when used for an extended period. For this purpose, this study aimed to evaluate the effect of tea tree oil (TTO) on Candida albicans adhesion and the surface roughness property of poly(methyl methacrylate) denture material after immersion in TTO. Methods: A total of 55 heat-cured acrylic resin specimens were used for C. albicans adherence and surface roughness tests. The
... Show MoreBackground: This study aimed to evaluate the effect addition of polyester fibers on the some mechanical properties of heat cured acrylic resin (implant strength, flexural strength and hardness) Materials and methods: Ninety specimens were used in the study. Thirty specimens were used for impact strength measurements (80mm X 10mm X 4mm) length, width and thickness respectively. The specimens divided into three test groups (n=10), first group formed from heat cure acrylic resin without fiber reinforcement. Second group was formed from heat cure acrylic resin was reinforced with 2 mm length polyester fiber and third group was formed from heat cure acrylic resin reinforced with 4mm length polyester fiber, impact strength measured by impact test
... Show MoreThe Effect of Chicken Eggshell Extract on Microhardness of Artificially Induced Dental Erosion in Permanent Teeth (In Vitro Study), Shatha A Abbas*, Alhan A Qasim
Dynamic loads highly influence soil properties and may cause real damage to structures and buildings. This article reports the experimental results from 24 tests to study the settlement of flexible and rigid raft foundation with different embedment depth rested on dense sandy soil. A small scale building model of dimension 200*200 mm and 320 mm in height was performed with reinforced concrete raft foundation of 10 mm thickness for flexible raft and 23 mm for rigid raft, The shaking table technique was used to simulate the seismic effect, the shaker was sat to give three different excitation frequencies 1,2,and3 Hz and displacement amplitude equal to 13 mm, the foundation was placed at
The aim of this research is to study the influence of additives on the properties of soap greases, such as lithium, calcium, sodium, lithium-calcium grease, by adding varies additives, such as graphite, molybdenum disulfide, carbon black, corrosion inhibitor, and extreme pressure.
These additives have been added to grease to obtain the best percentages that improve the properties of grease such as load carrying, wear resistance, corrosion resistance, drop point, and penetration.
The results showed the best weight percentages to all types of grease which give good properties are 1.5% extreme pressure additive, 3% graphite, 1% molybdenum disulfide, 2.5% carbon black.
The other hand, the best weight percentage for corrosion inhibit