Zinc Oxide thin film of 2 μm thickness has been grown on glass substrate by pulsed laser deposition technique at substrate temperature of 500 oC under the vacuum pressure of 8×10-2 mbar. The optical properties concerning the absorption, and transmission spectra were studied for the prepared thin film. From the transmission spectra, the optical gap and linear refractive index of the ZnO thin film was determined. The structure of the ZnO thin film was tested with X-Ray diffraction and it was formed to be a polycrystalline with many peaks.
Au nanoparticle-functionalized (TiO2)1−x(ZnO:MgO)x nanocomposite thin films (0≤x≤0.3) were effectively produced by chemical spray pyrolysis and annealed at 600 °C. The effects of ZnO incorporation and Au nanoparticle modification on the films' structural, optical, and antibacterial properties were studied using X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), UV–Vis spectroscopy, and field-emission scanning electron microscopy (FESEM). XRD analysis confirms the formation of polycrystalline anatase TiO2 and shows a composition-dependent structural develop- ment with increasing ZnO concentration. The optical experiments revealed increased transmittance and a progressive wid- ening of the optical band gap f
... Show MoreAu nanoparticle-functionalized (TiO2)1−x(ZnO:MgO)x nanocomposite thin films (0≤x≤0.3) were effectively produced by chemical spray pyrolysis and annealed at 600 °C. The effects of ZnO incorporation and Au nanoparticle modification on the films' structural, optical, and antibacterial properties were studied using X-ray diffraction (XRD), Fourier transform infrared spectroscopy (FTIR), UV–Vis spectroscopy, and field-emission scanning electron microscopy (FESEM). XRD analysis confirms the formation of polycrystalline anatase TiO2 and shows a composition-dependent structural development with increasing ZnO concentration. The optical experiments revealed increased transmittance and a progressive widening of the optical band gap from 3
... Show MoreDenture bases are fabricated routinely using Poly(methyl methacrylate) (PMMA) acrylic resin. Yet, it is commonly known for its major drawbacks such as insufficient strength and ductility. The purpose of this study was to improve the performance of PMMA acrylic resin as a denture base material by reinforcement with surface treated lithium disilicate glass ceramic powder. The ceramic powder was prepared by grinding and sieving IPS e.max CAD MT blocks. Then, the powder was surface treated with an organosilane coupling agent (TMSPM) and added to PMMA in amount of 1%, 3%, 5% and 7% by weight. Characterizations of the powder was done by particle size analysis, XRD and FTIR. Transverse strength, Impact strength, Shore D hardness and surface roughn
... Show MoreWe report here the observation of 16 µm superradiance laser action generated from optical pumping of CF4 gas molecules (which is cooled to 140 Kº by a boil-off liquid-N2) by a TEA-CO2 laser 9R12 line. Output laser pulses of 7 mJ and 200 ns have been obtained.
An optical video communication system is designed and constructed using pulse frequency modulation (PFM) technique. In this work PFM pulses are generated at the transmitter using voltage control oscillator (VCO) of width 50 ns for each pulse. Double frequency, equal width and narrow pulses are produced in the receiver be for demodulation. The use of the frequency doubling technique in such a system results in a narrow transmission bandwidth (25 ns) and high receiver sensitivity.
The existing investigation explains the consequence of irradiation of red laser on the optic properties of (CoO2) films. The film was equipped by the utilization of semi-computerized spray pyrolysis technique (SCSPT), it is the first time that this technique is used in the preparation and irradiation using a laser in this technique. From the XRD analysis, the crystalline existence with trigonal crystal system was when the received films were processed by continuous red laser (700 nm) with power (>1000mW)for different laser irradiation time using different number of times a laser scan (0, 6, 9, 12, 15 and 18 times) with total irradiation time(0,30,45,60,75,90 mi
Exploding wire Technique is a way for production metal and its compound nanoparticle that is capable of production of bulk amount at low cost semiconductor. In this work a copper iodine nanoparticles were fabricate by exploding copper wires with different currents in iodine solution. The produced samples were examined by XRD, FTIR, SEM and TEM to characterize their properties. The XRD proved the Nano-size for producer. The crystalline size increases with increasing current. FTIR measurements show a peaks located at 638.92 for Cu-I stretch bond indicate on formation of copper iodide compound and the peaks intensities increase with increasing current. The SEM and TEM measurements show that the thin films have nanostructures.
Nanoparticle has pulled in expanding consideration with the developing enthusiasm for nanotechnology which hold potential as essential segments for development applications. In the present work, a copper nanoparticle is manufactured as a suspension in distilled water by beating a bulk copper target with laser source (532 nm wavelength, 10 ns pulse duration and 10 Hz repletion rate) via method. UV- visible absorption spectra and AFM analysis has been done to observe the effect of repetition rate for the pulsation of laser. Copper nanoparticles (Cu-NPs) were successfully synthesized with green color. The Cu- NPs have very high purity because the preparation was managed in aqueous media to eliminate ambient contaminations. Absorption
... Show MoreThe present work was done in an attempt to build systematic procedures for treating warts by 810 nm diode laser regarding dose parameters, application parameters and laser safety. The study was done in Al- Kindy Teaching Hospital in Baghdad, Iraq during the period from 1st October 2003 till 1st April 2004. Fifteen patients completed the treatment and they were followed for the period of 3 months. Recalcitrant and extensive warts were selected for the study. Patients were randomly divided into 3 groups to be treated by different laser powers 9, 12 and 15 W, power density of 286 W/cm2, 381W/cm2, 477 W/cm2 pulse duration of 0.2 s, interval of 0.2 s and repeated pulses were used. The mode of application was either circular or radial. Pain oc
... Show More