The growing demand for sustainable and high-performance asphalt binders has prompted the exploration of waste-derived modifiers. This study investigates the performance enhancement of Natural Asphalt (NA) using Sugarcane Molasses (SM) and Waste Engine Oil (WEO). The modified blends were prepared by partially replacing 50 % NA with varying proportions of SM and WEO ranging from 10 % to 40 % of the total weight of NA. Comprehensive testing was conducted, including penetration, softening point, ductility, viscosity, Bending Beam Rheometer (BBR), Multiple Stress Creep Recovery (MSCR), Energy Dispersive X-ray Spectroscopy (EDX), Fourier Transform Infrared (FTIR) spectroscopy, and Scanning Electron Microscopy (SEM). The results demonstrated that modified blends with a high WEO content significantly increased fluidity, reducing rotational viscosity by up to 91 % for the blend with 40 % WEO and 10 % SM at 135 ◦C. Conversely, higher SM content increased stiffness, as seen in the blend with 40 % SM and 10 % WEO, with penetration values rising by 305 % compared to unmodified NA. Rheological testing showed that the 40 % SM and 10 % WEO blend achieved the highest rutting resistance with a Performance Grade (PG) of 88 ◦C, while the 40 % WEO and 10 % SM blend exhibited the best fatigue resistance with a 55 % reduction in G* .sinδ. Low-temperature performance was significantly improved across all blends, with the 40 % WEO and 10 % SM blend achieving the lowest creep stiffness and highest m-value, ensuring superior thermal cracking resistance. Chemical analysis revealed increased oxygen content (18.6 %) and reduced sulfur content (60 %) in the 40 % SM and 10 % WEO blend, indicating enhanced oxidation resistance. SEM analysis confirmed the development of dense morphology in the 40 % SM and 10 % WEO blend, correlating with superior structural integrity. Grey decision analysis identified the 40 % SM and 10 % WEO blend as the optimal blend with the lowest bull’s-eye distance, reflecting balanced performance across all parameters. These findings highlight the complementary effects of SM and WEO in enhancing the performance of NA, with the 40 % SM and 10 % WEO blend emerging as the most promising blend for bio-asphalt applications.
Aging of asphalt pavements typically occurs through oxidation of the asphalt and evaporation of the lighter maltenes from the binder. The main objective of this study is to evaluate influence of aging on performance of asphalt paving materials.nAsphalt concrete mixtures, were prepared, and subjected to short term aging (STA) procedure which involved heating the loose mixtures in an oven for two aging period of (4 and 8) hours at a temperature of 135 o C. Then it was subject to Long term aging (LTA) procedure using (2 and 5) days aging periods at 85 o C for Marshall compacted specimens. The effect of aging periods on properties of asphalt concrete at optimum asphalt content such as Marshall Properties, indirect tensile strength at 25 o C,
... Show MoreWarm mix asphalt (WMA) is relatively a new technology which enables the production and compaction of asphalt concrete mixtures at temperatures 15-40 °C lower than that of traditional hot mix asphalt HMA. In the present work, six asphalt concrete mixtures were produced in the mix plant (1 ton each) in six different batches. Half of these mixes were WMA and the other half were HMA. Three types of fillers (limestone dust, Portland cement and hydrated lime) were used for each type of mix. Samples were then taken from these patches and transferred to lab for performance testing which includes: Marshall characteristics, moisture susceptibility (indirect tension test), resilient modulus, permanent deformation (axial repeated load test)
... Show MoreWarm mix asphalt (WMA) is relatively a new technology which enables the production and compaction of asphalt concrete mixtures at temperatures 15-40 °C lower than that of traditional hot mix asphalt HMA. In the present work, six asphalt concrete mixtures were produced in the mix plant (1 ton each) in six different batches. Half of these mixes were WMA and the other half were HMA. Three types of fillers (limestone dust, Portland cement and hydrated lime) were used for each type of mix. Samples were then taken from these patches and transferred to lab for performance testing which includes: Marshall characteristics, moisture susceptibility (indirect tension test), resilient modulus, permanent deformation (axial repe
... Show MoreThis article aims to investigate how war contributes to the pollution of water bodies with harmful substances including heavy metals and toxic substances. The paper explains how these pollutants, carelessly dumped by military operations, have severely damaged the water quality of rivers and lakes all across Iraq. Based on the Jassim River as case study, the paper shows a close relationship between military operations and pollution. Shown is the effects of this pollution on local ecosystems like fish and wildlife, and human population, dependent on the river for drinking, irrigation, and other basic needs. The article reveals the problem of military waste in Iraq, focusing on the absence of satisfactory waste disposal techniques and
... Show MorePrepared zeolite type A was used for theremoval of cesium ions from aqueous solution. The experimental data were analyzed by Langmuir, Freundlich isotherms. Various parameters, such as contact time, zeolite weight, pH, and initial concentration, were studied. The results indicated that the highest removal efficiency was95.53% at (2h time, 0.04 g weight, and pH=6.8). The results also showed that the Freundlic model fits well with the experimental results and is better than the Langmuir model.
In this study, stabilization of expansive soils using waste materials namely; Cement Kiln Dust (CKD), and waste plastic bottles (WPB) was experimentally investigated. Using CKD and WPB are exponentially increasing day by day, due to their capability to solve both environmental and geotechnical problems successfully. Expansive soils were collected from locations with a wide range of plasticity index (PI) (15 - 27) and liquid limit (LL) (35% - 64%). Stabilizer percentages were varied from 0% to 20%, and curing durations for CKD cases were 7 and 28 days. Results showed the best percentages of CKD and WPB are 12% of each one respectively. LL, plastic limit (PL), and swelling percent (SP) loss were observed, which are 46%, 55%, and 96% respec
... Show More