Preferred Language
Articles
/
iqjmc-1121
Effect of some disinfectant solutions on the hardness property of selected soft denture liners after certain immersion periods.
...Show More Authors

Background: Disinfection of denture and soft denture liners became among the priorities for cross contamination control as well as patient's health. All the trials aimed to have maximum infection control with minimal adverse changes in the materials properties.
Materials and methods: Discs of 30x2mm were made from Coe Super Soft and Coe Soft denture liners. Every 5 specimens were immersed separately and daily in CHX, Sodium hypochlorite and chlorine dioxide, control group specimens were immersed in the distilled water. Hardness property of the experimental and control groups was evaluated by using Shore A durometer after 1, 7, 30 days. 
Results: Statistical analysis indicated non significant differences when the control group was compared with every disinfectant solution regarding tested periods, while ANOVA test showed significant differences among tested solutions after every testing period. Further LSD attributed these differences to the chlorine dioxide since it is the only solution that decreases hardness value after immersion.
Conclusion: Either of the tested solutions can be used safely regarding hardness property, although CHX and Sodium hypochlorite are more recommended since their effects on the hardness property was relatively same in comparison to the control.

Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Tue Dec 24 2024
Journal Name
Journal Of Baghdad College Of Dentistry
The Effect of Plasma Treatment on Shear Bond Strength of High Impact Acrylic Resin Denture Base Lined with Two Types of Soft Lining Materials after Immersion in Distilled Water and Denture Cleanser
...Show More Authors

Background: In dentistry, dentist takes the advantages of soft lining materials due to the viscoelastic properties. The major problem is the adhesion of the soft liner with the denture base material. Materials and Methods: Heat cured of high impact acrylic resin specimens prepared with dimensions 75x13x13mm for shear bond strength test, soft lining material (Refit and Mollosil) with a 3-mm thickness and used to join each two acrylic blocks. Also four specimens with the same previous dimensions utilized for chemical and physical surface analysis. The specimens grouped as control (without plasma) and experiment (with oxygen plasma) treated high impact acrylic specimens. Results: Plasma treatment increased the shear bond strength for both Refi

... Show More
View Publication Preview PDF
Publication Date
Sun Jun 01 2014
Journal Name
Baghdad Science Journal
Study the effect of acid immersion on the hardness of (Epoxy – Granite) composite
...Show More Authors

This work has been done with using of epoxy resin mixed with Granite powder were weighted by percent volume (5,10,15, and 20)%and then mixed with epoxy polymer to compose polymer composite. Hand lay-up technique is used in fabrication of the composite samples. Hardness test was carried out for the proper samples in both normal condition and after immersion in HCL (1 M and 2 M) solutions for periods ranging up to 10 weeks. After comparing the results between the polymer and their composite, the hardness increased with increasing Granite weight percent, it was found that Hardness were greater for the composites before immersion compared with their values after immersion.

View Publication Preview PDF
Crossref
Publication Date
Wed May 29 2019
Journal Name
Iraqi Journal Of Physics
Impact strength behaviour of PMMA denture base through addition of different nanoparticles after immersion in some nutrition liquids
...Show More Authors

Poly methyl methacrylate PMMA polymer could be considered the main material that used mostly in the recent years in denture base fabrication. It commonly known by it is poor strength properties such as low impact strength. The aim of the present research was to enhance the performance of PMMA denture base through the addition of two kind of nanoparticles (nano particles that selected from artificial and natural sources). Nano -particles from both Al2O3 and crushed peanut Peel were used for comparing purposes.Various weight fraction used in this study for both kinds of the additive (1%, 2% and 3%). Moreover, in this work a study and evaluation in impact strength (I.S.) value were done before and after immersion. The new prepared nanocompo

... Show More
View Publication Preview PDF
Crossref (5)
Crossref
Publication Date
Tue Dec 24 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of certain chemical surface treatments on repair bond strength of some denture base materials
...Show More Authors

Background: Fracture of different types of acrylic denture base is a common problem associated with dental prosthesis. Studies suggested that the repair strength may be improved by several means including surface treatment with chemical agents. The aim of the study was to evaluate the effect of surface treatment with acrybond-bonding agent and monomer on fractured denture base in respect to transverse, tensile and shear bond strength and evaluation of the mode of failure by light microscope. Materials and methods: Two hundred seventy specimens were prepared and divided into 3 groups according to the material used (regular conventional, rapid simplified and high impact) heat cure acrylic. The specimen in each groups were prepared specificall

... Show More
View Publication Preview PDF
Publication Date
Tue Sep 25 2018
Journal Name
Iraqi Journal Of Science
The Bending Property of the Epoxy (Ep / Mgo)And (Ep/Sio2) Composites After Immersion in Chemical Solution
...Show More Authors

In this paper, a polymer-based composite material was prepared by hand Lay-up method consisting of epoxy resin as a base material filled with by magnesium oxide powder once and silicon dioxide powder again and with different weight ratios (3%, 6%, 9%, 12%). The three-point bending test was performed in normal conditions and after immersion in sulfuric acid. The results showed that the bending value decreased with the increase of the weighted ratio of the filled nano powder (MgO, SiO2) .The Bending of samples filled with by SiO2 was found to be less than the bending of samples filled with by particles (MgO), the bending of the SiO2 sample (0.32mm) at the weighted ratio (3%) and for the MgO (0.18mm) sample

... Show More
View Publication Preview PDF
Publication Date
Tue Dec 24 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of disinfectant agents on certain physical and mechanical properties of type IV dental stone
...Show More Authors

Background: Dental stone casts come into contact with impression materials and becomes susceptible to cross contamination from saliva and blood. This study was done to evaluate the physical and mechanical properties of dental stone type IV after treatments with various disinfecting agents and regimes (methods). Materials and Methods: Type IV dental stone and different types of disinfecting agents were used and divided into seven groups: G1: dental stone without disinfection (control group), G2: dental stone mixed with silver nitrate powder 0.5% , G3: dental stone mixed with silver nitrate powder 1%, G4: dental stone mixed with copper sulfate powder 0.5%, G5: dental stone mixed with copper sulfate powder 1% ,G6: dental stone immersed in prop

... Show More
View Publication Preview PDF
Publication Date
Fri Dec 29 2017
Journal Name
Ibn Al-haitham Journal For Pure And Applied Sciences
The Study the Effect of Ultraviolet on the Compression and Hardness Property for Hybrid Material
...Show More Authors

The study was carried out by reinforcing the resin matrix material

which was (Epoxy- Ep828) by useing Kevlar fibers and glass fibers type (E-gl ass) both or them in the form of woven roving and poly propylene tlbcrs  in  the form chopped  strand  mats.  wi th (30%)  volume  fraction. Some mechan i cal  properties of the were prepared composite specimens U ltraviolet   radiation  were  stuied   after   being  subjected  to  different weathering conditi ons i ncluded. Compression and hardness testing were carried out using Briel! method so as to compare between composite behavior i n the environments previously mentioned .

 <

... Show More
View Publication Preview PDF
Publication Date
Tue Dec 24 2024
Journal Name
Journal Of Baghdad College Of Dentistry
Evaluating the effect of silver nanoparticles incorporation on antifungal activity and some properties of soft denture lining material
...Show More Authors

Background: Colonization of soft denture liners by Candida albicans and other microorganisms continued to be a serious problem. The aim of this study was to evaluate the effect of incorporating silver nanoparticles into heat cured acrylic-based soft denture liner on the antifungal activity, and on water sorption, solubility, shear bond strength and color change of the soft lining material. Furthermore, evaluating the amount of silver released. Materials and methods: Silver nanoparticles were incorporated into soft denture liner in different percentages (0.05%, 0.1% and 0.2% by weight). Four hundred and twenty specimens were prepared and divided into five groups according to the test to be performed. The antifungal activity of the soft liner

... Show More
View Publication Preview PDF
Publication Date
Fri Dec 15 2017
Journal Name
Journal Of Baghdad College Of Dentistry
The Effect of Addition of Zirconium Nano Particles on Antifungal Activity and Some Properties of Soft Denture Lining Material
...Show More Authors

Background Microorganisms and fungal growth especially Candida albicans, on soft denture lining material are the most common problem which can lead to chronic mucosal inflammation. The aim of this study was to evaluate the effect of zirconium nanoparticles into acrylic-based heat cured soft denture lining material against Candida albicans, and the amount of zirconium ion release of soft liner/ZrNPs composite. Furthermore, evaluate shear bond strength after ZrNPs addition to soft liner. Materials and methods: Zirconium nanoparticles were added into acrylic-based soft denture liner in various percentages (1%, and 1.5% by weight). Two hundred and fifty specimens were arranged and isolated into four groups as per the test to be done The antifu

... Show More
View Publication Preview PDF
Crossref (12)
Crossref
Publication Date
Wed Sep 15 2021
Journal Name
Journal Of Baghdad College Of Dentistry
Effect of plasma treatment on the bond of soft denture liner to conventional and high impact acrylic denture materials
...Show More Authors

Background: The main drawback of soft lining materials was that they debonded from the denture base after a certain period of usage. Therefore, the purpose of this research was to determine the impact of oxygen and argon plasma treatment on the shear bonding strength of soft liners to two different kinds of denture base materials: conventional acrylic resin and high impact acrylic resin. Materials and Methods: Heat cure conventional and high impact acrylic blocks (40 for each group) were prepared. A soft liner connected the final test specimen of two blocks of each acrylic material. Shear bond strength (SBS) was assessed using universal testing machine. Additional blocks were also prepared for analyzing Vickers microhardness, contact ang

... Show More
View Publication Preview PDF
Scopus (2)
Crossref (2)
Scopus Crossref