Objective: One of the most important practical deficiencies of present denture base materials is fracture, therefore many
attempts have been made to reinforce of the repaired denture base resin. A desirable objective for this service is to obtain
optimum strength for repairs, which can be achieved by making available a good bond between original and repaired
materials.
Methodology: The present study was carried out to evaluate and compare the transverse strength of acrylic specimens
repaired by two different materials (hot-cure and cold-cure acrylic resin). A total of 50 specimens were prepared by hot
(40) repair: (10) by hot with retention bead, (10) by cold with retention bead and (10) repair by hot only, (10) repair by cold
only, and (10) un repair control made from hot cure acrylic resin. Transverse strength was measured for each specimen
using three points bending on a brinell transverse testing machine.
Results: The result showed that the repair with heat-cure acrylic resin with retention bead has a significant higher than the
repair with cold-cure acrylic resin with retention bead and higher than control specimen (unrepaired).
Recommendations: It can be concluded that the hot acrylic resin with retention bead are an important parameter in the
reinforcement of repaired acrylic denture base resin.
The fluorescence and absorption spectra of Fluoranthene dissolved in
cyclohexane and ethanol were studied and analyzed. The effect of the
concentration of this molecule and the polarity of the solvents on the spectral
shifts and on relative intensity has been investigated. A computational program
was written in order to convert the spectra from grapher to data. Some
photophysical parameters such as oscillator strength and quantum efficiency have
been calculated. Fluorescence quantum efficiency of Fluoranthene was measured
relative to Quinine Sulfate (QS) in 1N H2SO4. The obtained values were (0.5) in
cyclohexane and (0.45) in ethanol
The removal of heavy metal ions from wastewater by ion exchange resins ( zeolite and purolite C105), was investigated. The adsorption process, which is pH dependent, shows maximum removal of metal ions at pH 6 and 7 for zeolite and purolite C105 for initial metal ion
concentrations of 50-250 mg/l, with resin dose of 0.25-3 g. The maximum ion exchange capacity was found to be 9.74, 9.23 and 9.71 mg/g for Cu2+, Pb2+, and Ni2+ on zeolite respectively, while on purolite C105 the maximum ion exchange capacity was found to be 9.64 ,8.73 and 9.39 for Cu2+, Pb2+, and Ni2+ respectively. The maximum removal was 97-98% for Cu2+ and Ni2+ and 92- 93% for Pb2+ on zeolite, while it was 93-94% for Cu2+, 96-97% for Ni2+, and 87-88% for Pb2+ on puroli
Electrochemical Grinding (ECG) process is a mechanically assisted electrochemical process for material processing. The process is able to successfully machine electrically conducting harder materials at faster rate with improved surface finish and dimensional control. This research studies the effect of applied current, electrolyte concentration, spindle speed and the gap between workpiece and tool on hardness and material removal rate during electrochemical grinding for stainless steel 316. The characteristic features of the electrochemical grinding process are explored through Taguchi-design-based experimental studies. The better hardness can be obtained at 10 A of the current, 150 g/l of the electrolyte concentration, 0.3 mm of gap an
... Show MoreHands have consistently been an important vehicle in the transmission of disease (1). Thus, thorough hand-washing remains the single most important factor in preventing infection specially in hospitals and labs.Twenty-nine non-clinical volunteers (do not work or come in contact with a clinical or hospital setting) that lacked visible skin injuries, eczema or apparent skin disease were used, those subjects were all tested by a material of each of the three used in the study weekly and laboratory tests were done pre- and post washing.All three material were effective , Eugenol extract as effective as the bar and lotion soap. And this was confirmed statistically.Eugenol has a great antibacterial action even in small concentration and t
... Show MoreIn this study, nanocomposites have been prepared by adding
multiwall carbon nanotubes (MWCNTs) with weight ratios (0, 2, 3,
4, 5) wt% to epoxy resin. The samples were prepared by hand lay-up
method. Influence of an applied load before and after immersion in
sodium hydroxide (NaOH) of normality (0.3N) for (15 days) at
laboratory temperature on wear rate of Ep/MWCNTs
nanocomposites was studied. The results showed that wear rate
increases with increasing the applied load for the as prepared and
immersed samples and after immersion. It was also found that epoxy
resin reinforced with MWCNTs has wear rate less than neat epoxy.
The sample (Ep + 5wt% of MWCNTs) has lower wear rate. The
immersion effect in base so
This research studies the development and synthesis of blended nanocomposites filled with Titanium dioxide (TiO2). Blended nanocomposites based on unsaturated polyester resin (UPR) and epoxy resins were synthesized by reactive blending. The optimum quantity from nano partical of titanium dioxide was selected and different weight proportions 1%, 3%, 5%, and 7% ratios of new epoxy are blended with UPR resin. The dielectric breakdown strength and thermal conductivity properties of the blended nanocomposites were compared with those of the basis material (UPR and 3% TiO2).The results show good compatibility epoxy resins with the UPR resin on blending, dielectric breakdown strength values are higher while thermal conductivity values of
... Show MoreAim: To evaluate the effect of ultrasonic agitation for retrograde biodceramic root repair, MTA and biodentine filling materials on push-out bond strength to dentine walls. Materials and Methods: Ninety extracted human teeth with single straight roots were selected randomly. After disinfection and cleaning, the coronal portions were sectioned to standardize the root canal length at 15mm. following root canal shaping, obturation and apical roots resection, retrograde cavities were prepared. Teeth were categorized depending on the filling material used into three groups, 30 teeth each. Group A filled with bioceramic root repair material, B with MTA and C with Biodentine material. These groups were divided in to three subgroup (n= 10). Subgrou
... Show MoreThe current work discusses the removal of brilliant dyes. These dyes were Brilliant Cresyl Blue (BCB) and Brilliant Green (BG) by the use of poly acrylic acid hydrogel beads (PAA). We examined the adsorption isotherms and found that the factors preferring it are temperature and salt, shaking effects, wet PAA, (BCB) and (BG) follows Freundlich equation more than other equations. Based on the results, there is a positive correlation between adsorption of dyes (BCB and BG) and temperature (Endothermic process). We calculated the thermodynamic functions (ΔG, ΔS, and ΔH). The ion strength effects on the adsorptions at (20 °C) increased adsorption if the salt concentrations is high. We treated the kinetics outcomes based on Lagergren Equation
... Show MoreThe present work reports the performance of three types of polyethersulfone (PES) membrane in the removal of highly polluting and toxic lead Pb2+ and cadmium Cd2+ ions from a single salt. This study investigated the effect of operating variables, including pH, types of PES membrane, and feed concentration, on the separation process. The transport parameters and mass transfer coefficient (k) of the membranes were estimated using the combined film theory-solution-diffusion (CFSD), combined film theory-Spiegler-Kedem (CFSK), and combined film theory-finely-porous (CFFP) membrane transport models. Various parameters were used to estimate the enrichment factors, concentration polarization modulus, and Péclet number. The pH values signif
... Show MoreObjective:Fluorid-containing dental alginate impression materials can exert a considerable reduction in
enamel solubility. The objective was to evaluate the effect of fluoride addition on the setting time and
compressive strength of alginate impression materials.
Methodology: 60 samples were constructed from alginate impression material (30 samples for setting
time test and 30 samples for compressive strength test).Specimens of each test divided into three
subgroup. Group A: 10 specimens of alginate were mixed with distilled water [control], Group B: 10
specimens of alginate were mixed with100-ppm fluoride and Group C:10 specimens of alginate were
mixed with 2%Naf.
Results: the result of setting time test showed t