Objective: the aim of this study is to invest age and determine the effect of using (2) packing
technique (conventional and new tension technique) on hardness of (2) types of heat cure acrylic
resin which are (Ivoclar and Qual dental type).
Methodology : this study was intended the using of two types of heat cure acrylic (IVoclar and
Qual dental type) which are used in construction of complete denture which packed in two different
packing technique (conventional and new tension technique) and accomplished by using a total of
(40) specimens in diameter of ( 2mm thickness, 2 cm length and 1 cm width) . This specimens were
sectioned and subdivide into (4) group each (10) specimens for one group , then signed as (A, Al B , B
1) according to the method of technique and type of acrylic that used . The hardness of the specimens
were measured by shore hardness test in technology university, Baghdad.
Results: this study revealed that the type of acrylic which packed by new tension technic had less
effect by hardness in compared with conventional packing technic, the result also showed that the
type of acrylic resin have a little effect on hardness of the two types, and also it show highly mean
value of hardness was indicate in Qual dental type in conventional technique, while the least mean
value of hardness showed in Ivoclar type in new tension technique.
Recommendations : this study has been conducted as a preliminary for future studies to give a sit
of about the effect of hardness on other types of commercial heat acrylic resin that used in
construction of prosthodontics restoration and dented prosthesis, it necessary to evaluate the
hardness of any material used in construction of denture bases , it is suggested to under take a farther
studies about using advance technique and better apparatus and device in packing the acrylic
material and measured the value of hardness and its effect on this material.
Background: Poly (methylmethacrylate) is the most widely used material in denture fabrication. The characteristics of acrylic resin which support microorganism development can threaten the oral health of denture users. This study was assigned to prepareand incorporate Ag-Zn zeolite powder into heat cured denture base material as antimicrobial material and to investigate its effect on some properties of heat cured acrylic denture base materials. Materials and methods: Sliver –zinc zeolite was prepared by ion exchange method and characterized then incorporated into poly (methylmethacrylate) powder in0.5% by weight. Specimens were constructed and divided into 6 groups according to the using tests; each group was subdivided into 2 groups
... Show MoreBackground: The geriatric patients wearing removable partial dentures are increasing in proportion. At the same time, the root caries prevalence accompanied by gingival recession is increasing. A variety of vehicles can deliver fluoride into the oral cavity, including fluoride mouth-rinse, fluoride dentifrice, topical fluoride, and fluoride-releasing restorative materials, all of which effectively prevent root caries and suppress recurrent caries. This study aimed to evaluate the effect of sodium fluoride addition on some mechanical properties of heat cure acrylic denture base material. Material and method: A total of 90 samples were prepared in this study, then divided into three main groups according to the type of test used (hardness, te
... Show MoreBackground: Dental stone casts come into contact with impression materials and becomes susceptible to cross contamination from saliva and blood. This study was done to evaluate the physical and mechanical properties of dental stone type IV after treatments with various disinfecting agents and regimes (methods). Materials and Methods: Type IV dental stone and different types of disinfecting agents were used and divided into seven groups: G1: dental stone without disinfection (control group), G2: dental stone mixed with silver nitrate powder 0.5% , G3: dental stone mixed with silver nitrate powder 1%, G4: dental stone mixed with copper sulfate powder 0.5%, G5: dental stone mixed with copper sulfate powder 1% ,G6: dental stone immersed in prop
... Show MoreMany extracted material were used as mouthwash to settle different kinds of oral fungi and bacteria. In this study an extractive of Cyperus rotundus plant E.C.R. which is very active as a mouthwash, was used in concentration range (10-25) ppm in artificial saliva at pH=6.4 and temperature range (288-318) K, to study it’s inhibitory effect on the corrosion of dental amalgam. Potentiostatic and cyclic polarization were used to follow this study. The presence of E.C.R. lead to shift the corrosion potential to the active direction and decreased the corrosion rate to about 98.87%, the inhibition action of E.C.R. resulting from the adsorption of C.R.E. layer between amalgam and saliva as FTIR spectrums shows, where the variety of FTIR adsorptio
... Show MoreBackground: Debonding and fracture of artificial teeth from denture bases are common clinical problem, bonding of artificial teeth to heat cure acrylic and high impact heat cure acrylic denture base materials with autoclave processing method is not well known. The aim of this study was to evaluate the effect of autoclave processing method on shear bond of artificial teeth to heat cure denture base material and high impact heat cure denture base material. Materials and methods: Heat polymerized (Vertex) and high impact acrylic (Vertex) acrylic resins were used. Teeth were processed to each of the denture base materials after the application of different surface treatments. The sample (which consist of artificial tooth attached to the dentur
... Show MoreBackground: White spot lesions (WSLs) are subsurface enamel demineralization manifested as white opacities which had an esthetic problem. The purpose of this in-vitro study was to evaluate the lesion depth improvement of WSLs following application of fluoride varnish, tooth mousse and resin infiltration (ICON). Materials and methods: Artificial WSLs were created on 120 premolar teeth using demineralization solution with pH (4-4.5). Samples randomly allocated into four groups; fluoride varnish, tooth mousse, ICON and untreated group. Groups were discolored in Cola and orange juice for 24 hours. Teeth were ground sectioned by longitudinal cutting then these sections examined and photographed under stereomicroscope at 12X magnification then an
... Show MoreBackground: This in vitro study measure and compare the effect of light curing tip distance on the depth of cure by measuring vickers microhardness value on two recently launched bulk fill resin based composites Tetric EvoCeram Bulk Fill and Surefil SDR Flow with 4 mm thickness in comparison to Filtek Z250 Universal Restorative with 2 mm thickness. In addition, measure and compare the bottom to top microhardness ratio with different light curing tip distances. Materials and Method: One hundred fifty composite specimens were obtained from two cylindrical plastic molds the first one for bulk fill composites (Tetric EvoCeram Bulk Fill and Surefil SDR Flow) with 4 mm diameter and 4 mm depth, the second one for Filtek Z250 Universal Restorative
... Show MoreThis research studies the effect of adding micro, nano and hybrid by ratio (1:1) of (Al2O3,TiO2) to epoxy resin on thermal conductivity before and after immersion in HCl acid for (14 day) with normality (0.3 N) at weight fraction (0.02, 0.04, 0.06, 0.08) and thickness (6mm). The results of thermal conductivity reveled that epoxy reinforced by (Al2O3) and mixture (TiO2+Al2O3) increases with increasing the weight fraction, but the thermal conductivity (k) a values for micro and Nano (TiO2) decrease with increasing the weight fraction of reinforced, while the immersion in acidic solution (HCl) that the (k) values after immersion more than the value in before immersion.
The zirconia ceramic restoration (ZCR) is used as substitutes for the metal-ceramic restoration. Clinical studies demonstrating of ZCRs showed a high fracture incidence of veneering layer than metal-ceramic restorations. This attributed to the low bond strength of zirconia to veneering ceramic as a result of lacking of glass content in its matrix. Surface treatment was proposed to improve the bonding strength between zirconia and veneering ceramic. Several studies revealed that some treatment such as airborne particle abrasion (APA) is responsible for generating chipping of veneering ceramic. The study aimed to develop a new zirconia coatings to increase bonding strength between zirconia substrate and veneering porcelain. Three groups of 15
... Show More