Objective(s): This study aims to evaluate the hardness of two commercially available cold cured acrylic resin material
(Vertex and PAN) when polymerized at different temperature in comparison to those polymerized by conventional
methods in air at 23C ± 5C.
Methodology: Eighty specimens, forty from cold cured acrylic (Vertex Type) and forty from cold cured acrylic (PAN
type) were prepared, flasking and packing procedure were done according to manufacturer direction and divided
according to processing as follow: 20 specimens (10 from Vertex type and 10 from PAN type) were processed in air for
two hours at 23C ± 5C under press (bench curing) as a control, and 60 specimens (30 from Vertex type and 30 from
PAN type) were processed by ivomat curing device containing water under air pressure 30 Pascal for 15 minutes at
different temperature: 40C, 60C, and 80C (10 specimens for each groups). All specimens were tested for hardness test
by shore D device.
Results: Result showed that cold cured acrylic type PAN (polymerized by elevated temperature 80˚C) show the
maximum value of hardness (88.696) followed by cold cured acrylic type vertex polymerized at 60˚C (88.471). While,
control group type PAN (polymerized at air bench) recorded the minimum value of hardness (81.83). All groups that
polymerized at high temperature: 40C, 60C, and 80C show the higher value of hardness in comparison to those
processed by conventional methods (at air bench) with significant and highly significant differences.
Recommendations: Studies need to study the effect of increasing time and pressure of curing process on the hardness
of cold cure acrylic material, also to study the effect of increasing temperature of curing on the other properties of
cold cure acrylic material.
Background Microorganisms and fungal growth especially Candida albicans, on soft denture lining material are the most common problem which can lead to chronic mucosal inflammation. The aim of this study was to evaluate the effect of zirconium nanoparticles into acrylic-based heat cured soft denture lining material against Candida albicans, and the amount of zirconium ion release of soft liner/ZrNPs composite. Furthermore, evaluate shear bond strength after ZrNPs addition to soft liner. Materials and methods: Zirconium nanoparticles were added into acrylic-based soft denture liner in various percentages (1%, and 1.5% by weight). Two hundred and fifty specimens were arranged and isolated into four groups as per the test to be done The antifu
... Show MoreThe current research aims to reveal the level of satisfaction of the mentors with the evaluation of their performance according to gender (male - female) and to formulate the predictive equation for the level of performance (dependent variable) from knowing the level of satisfaction with the evaluation (independent variable). (16 paragraphs) contains alternatives to the answer that measures the level of satisfaction (weak, medium, and high) (1,2,3), that is, with a hypothetical average of (32). It consisted of 100 educational counselors consisting of 45 males and 55 females, the results of the research concluded that the level of satisfaction with performance is below the mean when compared with the hypothetical average of the scale of s
... Show MoreUnderstanding breaking news necessitates a special attention, since they are written with a special style. The study aims at identifying the difficulties faced by the Iraqi university EFL learners in comprehending English breaking news. The study included 10 fourth year students enrolled at the Department of English, College of Education for Humanities, University of Anbar. Thus, a questionnaire as a research instrument, was sent online to the students. The questionnaire points were related to the identification of difficulties faced by the learners in comprehending English breaking news. The data of the study were (10) headlines selected purposively from Euronews website. The data were qualitatively analyzed based on quantifying the qua
... Show MoreBackground: Fixed orthodontic appliances impede the maintenance of oral hygiene and result in plaque accumulation leads to enamel demineralization caused by acids produced by bacteria. Studies on plaque control strategies in orthodontic populations are limited. This might be caused by difficulties in the quantitative evaluation of dental plaque because the teeth have various levels of bracket coverage, and different tooth sizes and malocclusions, making the traditional categorical indices complex. The present study aims to evaluate the effect of different hygiene protocols on plaque quantity on bands with different attachments. Materials and method: Twenty patients had four bands within the orthodontic appliance. Then randomly divided into
... Show MoreEnhancement of heat transfer in the tube heat exchanger is studied experimentally by using discrete twisted tapes. Three different positions were selected for inserting turbulators along tube section (horizontal position by α= 00, inclined position by α= 45 0 and vertical position by α= 900). The space between turbulators was fixed by distributing 5 pieces of these turbulators with pitch ratio PR = (0.44). Also, the factor of constant heat flux was applied as a boundary condition around the tube test section for all experiments of this investigation, while the flow rates were selected as a variable factor (Reynolds number values vary from 5000 to 15000). The results s
... Show MoreTin Oxide (SnO2) films have been deposited by spray pyrolysis technique at different substrate temperatures. The effects of substrate temperature on the structural, optical and electrical properties of SnO2 films have been investigated. The XRD result shows a polycrystalline structure for SnO2 films at substrate temperature of 673K. The thickness of the deposited film was of the order of 200 nm measured by Toulansky method. The energy gap increases from 2.58eV to 3.59 eV when substrate temperature increases from 473K to 673K .Electrical conductivity is 4.8*10-7(.cm)-1 for sample deposited at 473K while it increases to 8.7*10-3 when the film is deposited at 673K
Reflection cracking in asphalt concrete (AC) overlays is a common form of pavement deterioration that occurs when underlying cracks and joints in the pavement structure propagate through an overlay due to thermal and traffic-induced movement, ultimately degrading the pavement’s lifespan and performance. This study aims to determine how alterations in overlay thickness and temperature conditions, the incorporation of chopped fibers, and the use of geotextiles influence the overlay’s capacity to postpone the occurrence of reflection cracking. To achieve the above objective, a total of 36 prism specimens were prepared and tested using an overlay testing machine (OTM). The variables considered in this study were the thickness of the
... Show MoreReflection cracking in asphalt concrete (AC) overlays is a common form of pavement deterioration that occurs when underlying cracks and joints in the pavement structure propagate through an overlay due to thermal and traffic-induced movement, ultimately degrading the pavement’s lifespan and performance. This study aims to determine how alterations in overlay thickness and temperature conditions, the incorporation of chopped fibers, and the use of geotextiles influence the overlay’s capacity to postpone the occurrence of reflection cracking. To achieve the above objective, a total of 36 prism specimens were prepared and tested using an overlay testing machine (OTM). The variables considered in this study were the thickness of the
... Show MoreThe effects of temperature on an exotic aquatic snail Pomacea canaliculata (Lamarck, 1819) collected from the Shatt Al-Arab intertidal zone were investigated. A series of laboratory experiments were conducted during the summer period of 2017. Individuals of new born snails hatched in the laboratory from adult snails were collected from Shatt Al-Arab intertidal zone, and subjected to five fixed temperatures: 15, 25, 35, 40 and 45 Cº, after short term thermal acclimation. The heartbeats (HB) were counted at each temperature level. The results showed significant direct increase of HB from 15 Cº (19.8 HB/min) up to 25 Cº (76 HB/min) (P<0.05) as well as from 25 Cº to 35 Cº (93 HB/min). At 40 Cº the snail HB
... Show More