Objective(s): This study aims to evaluate the hardness of two commercially available cold cured acrylic resin material
(Vertex and PAN) when polymerized at different temperature in comparison to those polymerized by conventional
methods in air at 23C ± 5C.
Methodology: Eighty specimens, forty from cold cured acrylic (Vertex Type) and forty from cold cured acrylic (PAN
type) were prepared, flasking and packing procedure were done according to manufacturer direction and divided
according to processing as follow: 20 specimens (10 from Vertex type and 10 from PAN type) were processed in air for
two hours at 23C ± 5C under press (bench curing) as a control, and 60 specimens (30 from Vertex type and 30 from
PAN type) were processed by ivomat curing device containing water under air pressure 30 Pascal for 15 minutes at
different temperature: 40C, 60C, and 80C (10 specimens for each groups). All specimens were tested for hardness test
by shore D device.
Results: Result showed that cold cured acrylic type PAN (polymerized by elevated temperature 80˚C) show the
maximum value of hardness (88.696) followed by cold cured acrylic type vertex polymerized at 60˚C (88.471). While,
control group type PAN (polymerized at air bench) recorded the minimum value of hardness (81.83). All groups that
polymerized at high temperature: 40C, 60C, and 80C show the higher value of hardness in comparison to those
processed by conventional methods (at air bench) with significant and highly significant differences.
Recommendations: Studies need to study the effect of increasing time and pressure of curing process on the hardness
of cold cure acrylic material, also to study the effect of increasing temperature of curing on the other properties of
cold cure acrylic material.
This investigation aimed to explain the mechanism of MFCA by applying this method on air-cooled engine factory which was suffering from high production cost. The results of this study revealed that MFCA is a useful tool to identify losses and inefficiencies of the production process. It is found that the factory is suffering from high losses due to material energy and system losses. In conclusion, it is calculated that system losses are the highest among all the losses due to inefficient use of available production capacity.
Introduction: This study aimed to assess the color change of human teeth with artificial enamel white spot lesions (WSLs) after sandblasting with bioactive glass, resin infiltration, and microabrasion and to test color stability after pH cycling. Methods: Fifty extracted human mandibular first molars were randomly assigned into five groups: Sound, WSLs (untreated), and WSLs sandblasted with bioactive glass (Sylc), WSLs treated by resin infiltration (ICON), and WSLs treated by microabrasion (Opalustre), respectively. All specimens underwent a pH cycling procedure. The color parameters for each specimen were assessed using an Easyshade dental spectrophotometer at different time stages then the color changes (ΔE) were calculated. Results: The
... Show MoreBackground: This in vitro study measure and compare the effect of light curing tip distance on the depth of cure by measuring vickers microhardness value on two recently launched bulk fill resin based composites Tetric EvoCeram Bulk Fill and Surefil SDR Flow with 4 mm thickness in comparison to Filtek Z250 Universal Restorative with 2 mm thickness. In addition, measure and compare the bottom to top microhardness ratio with different light curing tip distances. Materials and Method: One hundred fifty composite specimens were obtained from two cylindrical plastic molds the first one for bulk fill composites (Tetric EvoCeram Bulk Fill and Surefil SDR Flow) with 4 mm diameter and 4 mm depth, the second one for Filtek Z250 Universal Restorative
... Show MoreBackground: White spot lesions (WSLs) are subsurface enamel demineralization manifested as white opacities which had an esthetic problem. The purpose of this in-vitro study was to evaluate the lesion depth improvement of WSLs following application of fluoride varnish, tooth mousse and resin infiltration (ICON). Materials and methods: Artificial WSLs were created on 120 premolar teeth using demineralization solution with pH (4-4.5). Samples randomly allocated into four groups; fluoride varnish, tooth mousse, ICON and untreated group. Groups were discolored in Cola and orange juice for 24 hours. Teeth were ground sectioned by longitudinal cutting then these sections examined and photographed under stereomicroscope at 12X magnification then an
... Show MoreBackground: The anterior loop of mental nerve is commonly described as that part of the neurovascular bundle that transverses anterior and inferior to the mental foramen only to loop back to exit the mental foramen. The aim of the study is to evaluate the incidence and extension of anterior loop of mental nerve by using digital panoramic imaging system to avoid nerve damage during different surgical procedures in dentistry. Materials and Method: Panoramic image was taken for all 400 patients and stored in the computer. Then Horizontal and Vertical for the anterior loop extension when exist was measured and recorded in a special case sheet prepared for each subject. Results: Results indicated that out of 400 patients there were only 25 pat
... Show MoreABSTRACT Background: One of the major problems of all ceramic restorations is their probable fracture against the occlusal forces. The objective of this in vitro study was to evaluate the effect of two gingival finishing lines (90°shoulder and deep chamfer) on the fracture resistance of full contour CAD/CAM and heat press all-ceramic crowns. Materials and Methods: Thirty two maxillary first premolars were prepared to receive full contour CAD/CAM (zolid) and heat press (Cergo Kiss) ceramic crowns using a special paralleling device (Parallel-A-Prep). The teeth were divided into four groups according to the type of finishing line prepared. Each crown was cemented to its corresponding tooth using self-etch, self-adhesive dual cure resin ceme
... Show MoreBackground: The excessive use and abuse of antibiotics contribute to bacterial resistance, raising the risk of complications and treatment failures. This study investigates adherence to antibiotic prescriptions among Iraqi dental patients, highlighting implications for antimicrobial resistance.Objective: To assess adherence levels and identify factors influencing antibiotic therapy compliance among dental patients.Methods: A cross-sectional survey was conducted in which adult dental patients aged 18 and older, who had been prescribed antibiotics within the past year, participated. The modified Morisky Medication Adherence Scale-8 items was used to evaluate adherence, and data were analyzed with IBM SPSS Statistics software V26.Results: Amon
... Show MoreCastellated columns are structural members that are created by breaking a rolled column along the center-line by flame after that rejoining the equivalent halves by welding such that for better structural strength against axial loading, the total column depth is increased by around 50 percent. The implementation of these institutional members will also contribute to significant economies of material value. The main objectives of this study are to study the enhancement of the load-carrying capacity of castellated columns with encasement of the columns by Reactive Powder Concrete (RPC) and lacing reinforcement, and serviceability of the confined castellated columns. The Castellated columns with RPC and Lacing Reinforcement improve com
... Show MoreThe removal of heavy metal ions from wastewater by ion exchange resins ( zeolite and purolite C105), was investigated. The adsorption process, which is pH dependent, shows maximum removal of metal ions at pH 6 and 7 for zeolite and purolite C105 for initial metal ion
concentrations of 50-250 mg/l, with resin dose of 0.25-3 g. The maximum ion exchange capacity was found to be 9.74, 9.23 and 9.71 mg/g for Cu2+, Pb2+, and Ni2+ on zeolite respectively, while on purolite C105 the maximum ion exchange capacity was found to be 9.64 ,8.73 and 9.39 for Cu2+, Pb2+, and Ni2+ respectively. The maximum removal was 97-98% for Cu2+ and Ni2+ and 92- 93% for Pb2+ on zeolite, while it was 93-94% for Cu2+, 96-97% for Ni2+, and 87-88% for Pb2+ on puroli
Background: Polymethylmethacrylate (PMMA) has relatively unsatisfactory mechanical properties such as low flexural strength and impact strength also dimensional instability. Material and method: Zirconium silicate nanoparticles were coated with a layer of trimethoxysilylpropylmethacrylate (TMSPM) before sonication in monomer (MMA) with the percentages 1% and 1.5% by weight then mixed with powder using conventional procedure, (150) samples were prepared and divided into three groups, each group consisted of (50) samples, the first group prepared from PMMA without addition (control), another group with the addition of 1% wt Zrsio4 nanoparticles (experimental) and the third one with 1.5% wt Zrsio4 nanoparticles (experimental). Each group
... Show More