By extracting crystal violate dye (CV) from its aqueous solution, the photocatalytic decolorization performance of ZnO/MWCNT nanocomposite was evaluated. The nanocomposite was prepared by precipitation of ZnO and incorporates on the surface of Multi-Walled Carbon Nanotubes (MWCNT). ZnO nanoparticles were synthesized using the sol gel process with MWCNT acting as a template. They were then analyzed by XRD, SEM, and TEM, which revealed how the shape of the spherical nano ZnO interacts with the point of zero charge (pzc), which allows us to see the physical attributes. In the dipping photoreactor, which included a slurry of dye solution and ZnO/MWCNT nanocomposite, the effectiveness of decolorization was assessed. The photodecolorization was studied for CV dye in aqueous solution at different conditions: The effect of time, weight of catalyst, concentration of dye, temperature, the initial pH of dye solution and addition of S2O82- to show the optimum condition of this process. The main results were the synthesis of incorporated ZnO on MWCNT surface with 10-20 nm with high photodecolorization against CV dye. Full decolorization reached at 90 min and 89.8% decolorization at the half time of reaction. ZnO/MWCNT weight of 0.06 gm per 100 mL was optimum for photodecolorization. The photocatalytic reaction was more efficient in the deceasing of CV concentration and obeys the Langmuir-Hinshelwood kinetic, while the photodecolorization was not less than 95% in pH range 6-10.Also, the photocatalytic reaction was effected in the presence of S2O82-, where the photodecolorization was more efficient.
Application of a Fe-bentonite nano clay (Fe-BNC) as modified clay has been investigated for the removal of birlliant green (BG) from aqueous solutions. Atomic force microscope measurements give a detailed information on pore shape and pore size distribution about the clay. These measurements show that the average diameter of the improved clay is 346.84 nm. Batch adsorption experiments were carried out for the removal of (BG) from aqueous solutions onto Fe-BNC. Equilibrium data were fitted to Freundlich and Langmuir isotherm equations and the isotherm constants were determined. Thermodynamic parameters such as free energy, entropy and enthalpy, have been calculated. &n
... Show MoreIn the present study, advanced oxidation treatment, the TiO2 /UV/H2O2 process was applied to decolorisation of the reactive yellow dyes in aqueous solution. The UV radiation was carried out with a 6 W low-pressure mercury lamp. The rate of color removal was studied by measuring the absorbency at a characteristic wavelength. The effects of H2O2 dosage, dye initial concentration and pH on decolorisation kinetics in the batch photoreactor were investigated. The highest decolorisation rates were observed (98.8) at pH range between 3 and 7. The optimal levels of H2O2 needed for the process were examined. It appears that high levels of H2O2 could reduce decolori
... Show MoreOne of the significant environmental problems is the pollution of water by dyes;. Biological treatment method was used, which is one of the effective ways to reduce this sort of pollution as it is environment friendly, economic and does not require any expertise. Under controlled conditions, this study estimated the efficacy of dry biomass for Bacillus cereus to reduce Direct Blue 2 dye from the aqueous solution. The optimum conditions such as pH values, contact time and concentration of dyes, were used in this research. The end results showed that the adsorption efficiency, when using a weight of bacterial biomass 0.2 g/50mL, reached 69.2% at a concentration of 10 ppm after one hour at 40°C and pH5. While it reached 5
... Show MoreThe degradation of Toluidine Blue dye in aqueous solution under UV irradiation is investigated by using photo-Fenton oxidation (UV/H2O2/Fe+). The effect of initial dye concentration, initial ferrous ion concentration, pH, initial hydrogen peroxide dosage, and irradiation time are studied. It is found put that the removal rate increases as the initial concentration of H2O2 and ferrous ion increase to optimum value ,where in we get more than 99% removal efficiency of dye at pH = 4 when the [H2O2] = 500mg / L, [Fe + 2 = 150mg / L]. Complete degradation was achieved in the relatively short time of 75 minutes. Faster decolonization is achieved at low pH, with the optimal value at pH 4 .The concentrations of degradation dye are detected by spectr
... Show MoreIn this work, ZnO quantum dots (Q.dots) and nanorods were prepared. ZnO quantum dots were prepared by self-assembly method of zinc acetate solution with KOH solution, while ZnO nanorods were prepared by hydrothermal method of zinc nitrate hexahydrate Zn (NO3)2.6H2O with hexamethy lenetetramin (HMT) C6H12N4. The optical , structural and spectroscopic properties of the product quantum dot were studied. The results show the dependence of the optical properties on the crystal dimension and the formation of the trap states in the energy band gap. The deep levels emission was studied for n-ZnO and p-ZnO. The preparation ZnO nanorods show semiconductor behavior of p-type, which is a difficult process by doping because native defects.
Kinetic experiments were performed to induce of the green methyl dye adsorption from aqueous solution on the bauxite clay. This study includes determination of the adsorption capacity of bauxite clay to methyl green dye adsorption and study the effect of some parameters ( temperature , time ) on the kinetic of the adsorption process of the dye were studied. Quantity of dye adsorbed was increased when the temperature increases from 298 to 318K which indicates that methyl green adsorption processes are endothermic nature . In order to describe the kinetic data and the rate adsorption constants of the pseudo-first-order and second-order kinetics were used . The kinetics data were applied well
... Show MoreMagnetized iron oxide nanoparticles (NPs) were prepared using Eucalyptus leaf extract and then coated with CTAB (Cetrimonium bromide) to increase efficiency. The prepared and modified (NPs) were characterized using AFM, FTIR, and X-ray techniques. The adsorption of the dye reactive blue RB 238 on coated (NPs) was investigated. The effect of various experimental factors, such as the initial concentration of the dye, the amount of adsorbent, pH and temperature on the removal of RB238 was studied. The best conditions for dye removal were found to be 298 K in an acidic medium of pH = 3 and an appropriate dose of the adsorbent of 0.15 g per 25 mg/L to achieve the best color removal of 90% within 60 minutes. The pseudo-second-order re
... Show MoreIn this study, the zinc oxide NPs have been synthesized from the fresh pomegranate peels extract using the precipitation method. The ZnO nanoparticles were produced from the reaction of fresh peels extract with zinc acetate salt which was used as zinc source in the presence of 2 M NaOH. The green synthesized nanoparticles were characterized through X-ray diffraction (XRD), UV-Vis diffuse reflection spectroscopy, Fourier transform infrared spectroscopy (FTIR), and Atomic force microscopy (AFM). The XRD patterns confirm the formation of hexagonal wurtzite phase structure for ZnO synthesized using pomegranate peels extract with average crystalline size of 28 nm. FTIR spectra identify the presence of many active functional groups for the pom
... Show MoreThe current study used extracts from the aloe vera (AV) plant and the hibiscus sabdariffa flower to make Ag-ZnO nanoparticles (NPs) and Ag-ZnO nanocomposites (NCs). Ag/ZnO NCs were compared to Ag NPs and ZnO NPs. They exhibited unique properties against bacteria and fungi that aren't present in either of the individual parts. The Ag-ZnO NCs from AV showed the best performance against E. coli, with an inhibition zone of up to 27 mm, compared to the other samples. The maximum absorbance peaks were observed at 431 nm and 410 nm for Ag NPs, at 374 nm and 377 nm for ZnO NPs and at 384 nm and 391 nm for Ag-ZnO NCs using AV leaf extract and hibiscus sabdariffa flower extract, respectively. Using field emission-scanning electron microscopes (FE-
... Show More