Polymer concrete were prepared by mixing epoxy resin with sand particles in three different grain size (150-300) , (300-600 ) and (600- 1200) μm respectively. The percentage of epoxy was 15%, 20 %, 25% and 30% wt of the total weight. Compression strength and flexural strength tests were carried out for the prepared samples.
The percentages of epoxy resin at 20% wt and 25% wt showed best mechanical properties for all grain sizes. These percentages were adopted to fill the voids between particles sand have two different size ranges (150-600) μm and {(150-300) & (600-1200)} μm respectively to obtain more dense material. The results showed that the strength of polymer composite at 20% resin is higher than 25% resin.
In this article four samples of HgBa2Ca2Cu2.4Ag0.6O8+δ were prepared and irradiated with different doses of gamma radiation 6, 8 and 10 Mrad. The effects of gamma irradiation on structure of HgBa2Ca2Cu2.4Ag0.6O8+δ samples were characterized using X-ray diffraction. It was concluded that there effect on structure by gamma irradiation. Scherrer, crystallization, and Williamson equations were applied based on the X-ray diffraction diagram and for all gamma doses, to calculate crystal size, strain, and degree of crystallinity. I
... Show More