Cadmium sulfide (CdS) nanocrystalline thin films are prepared onto ITO-glass and Si(111) substrates by chemical bath deposition method. The scanning electron microscope images showed that the CdS thin film onto Si substrate is more homogenous without vacancies. The XRD patterns of the CdS nanocrystalline thin film confirm that they have polycrystalline with cubic phase. Room temperature photoluminescence (PL) spectrum of the CdS nanocrystalline thin films shows emission band located at 502nm for CdS/Si sample while the CdS/ITO-glass thin films shows a broad emission band peaked at 505nm. The Raman spectra of CdS nanocrystalline thin films prepared onto Si and ITO-glass substrates contain two main peaks which are corresponding to the first and second-order longitudinal optical (LO) phonon modes.
The compound 3-[4Ì„-(4Ë-methoxy benzoyloxy) benzylideneamino]-2-thioxo-imidazolidine-4-one [III] was prepared from the cyclization of thiosemicarbazone [II] with
ethyl α -chloroacetate in the presence of fused sodium acetate. Treatment the later compound
with acetic anhydride yielded the corresponding 1-Acetyl-3-[ 4Ì„- (4Ë- methoxy benzoyloxy)
benzylideneamino] – 2 – thioxo -imidazolidine-4-one [IV]. 1,3-Oxazepine derivatives [V]a-d
and [VI]a-d are obtained from the reaction of compounds[III] and [IV] with different acid
anhydrides, in dry benzene. The FTIR and
1
HNMR spectroscopy are indicated a good
evidence for the formation of the synthesized compounds. Some of the synthesized
Spin coating technique has been applied in this work to prepared Xerogel films doped with Rhodamine 6G laser dyes. The solid host of laser dye modifies its spectroscopic properties with respect to liquid host. During the spin coating process the dye molecules suffer from changing their environment. The effects of three parameters were studied here: the spinning speed, multilayer coating and formaldehyde addition
Acetophenone sulfamethoxazole and 3-Nitrobenzophenone sulfamethoxazole were prepared from the reaction of sulfamethoxazole with two ketones. The prepared ligands were identified by (C.H.N) analysis and UV-VIS, FT-IR spectroscopic techniques. Metal complexes of the two ligands were prepared in an aqueous alcohol with Zn (II), Mn (II) and Cu (II) ions with a molar ratio1:1. The proposed general formula for the resulting complexes was [ML.CL2.H2O]H2O .The complexes were characterized by (C.H.N) technique , spectroscopic methods ,conductivity, atomic absorption ,magnetic susceptibility measurements and melting point. According to the results obtained, the suggested geometry is to be octahedral for all the complexes.
The purpose of this study is to determine the useful of Schiff bases derivatives containing (oxazepine, tetrazole) rings with biological activity which can be used as drug and antimicrobial, the present work is started from [Binary (2,5(4,'4-diaminophenyl) – 1,3,4 – oxadiazole]. A variety of Schiff bases and heterocyclic (oxazepine, tetrazole) have been synthesis, and confirm that structures by physical properties , FTIR , 1H-NMR, 13C-NMR, elemental analysis, [Microbial study against three type of bacteria (staphylococcus aurea and klebsiella pneumonia) and (Canadida albncans) fungi].All analyzation performed in center of consulatation University of Jordan.
In this study a new composite nano material was prepared and characterized through the polymerization of inter attuplgie layered m-phenylendiamine with p-kresol. The results indicated that the propagated polymer separated the clay aluminosilicate layers as a two dimensional nano-sheets soaked in the prepared polymer matrix with losing the original fibrous structure of Attuplgite clay.
Silver selenide telluride Semiconducting (Ag2Se0.8Te0.2) thin films were by thermal evaporation at RT with thickness350 nm at annealing temperatures (300, 348, 398, and 448) °K for 1 hour on glass substrates .using X-ray diffraction, the structural characteristics were calculated as a function of annealing temperatures with no preferential orientation along any plane. Atomic force microscopy (AFM) and X-ray techniques are used to analyze the Ag2SeTe thin films' physical makeup and properties. AFM techniques were used to analyze the surface morphology of the Ag2SeTe films, and the results showed that the values for average diameter, surface roughness, and grain size mutation increased with annealing temperature (116.36-171.02) nm The transm
... Show MoreSilver selenide telluride Semiconducting (Ag2Se0.8Te0.2) thin films were by thermal evaporation at RT with thickness350 nm at annealing temperatures (300, 348, 398, and 448) °K for 1 hour on glass substrates .using X-ray diffraction, the structural characteristics were calculated as a function of annealing temperatures with no preferential orientation along any plane. Atomic force microscopy (AFM) and X-ray techniques are used to analyze the Ag2SeTe thin films' physical makeup and properties. AFM techniques were used to analyze the surface morphology of the Ag2SeTe films, and the results showed that the values for average diameter, surface roughness, and grain size mutation increased with annealing temperature (116.36-171.02) nm The transm
... Show MoreIn this work, (CdO)1-x (CoO)x thin films were prepared on glass slides by laser-induced plasma using Nd:YAG laser with (λ=1064 nm) and duration (9 ns) at different laser energies (200-500 mJ) with ratio (x=0.5), The influence of laser energy on structural and optical properties has been studied. XRD patterns show the films have a structure of polycrystalline wurtzite. As for AFM tests results for the topography of the surface of the film, where the results showed that the grain size and the average roughness increase with increasing laser energy. The optical properties of all films were also studied and the results showed that the absorption coefficient for within the wavelength range (280-1100 nm), The value of the optical power gap fo
... Show More