In this paper, the effect of films thickness on the structural and optical properties of gold (Au) thin films prepared by the DC sputtering method was studied. At three different deposition times, three samples of gold thin films of three different thicknesses (200,400, and 600 nm) were prepared. X-ray diffraction patterns, scanning electron microscopy (SEM), and atomic force microscopy (AFM) images, as well as optical spectroscopy, were used to characterize thin films. The crystalline structure of gold thin films was determined by the XRD pattern which showed to be cubic phase and polycrystalline in nature. The preferred orientation was (111) at 2Ѳ equal 37.4. The effect of deposition time on the morphology of the deposited films was visualized with a scanning electron microscope (SEM) which showed a homogenous surface with nanoparticles with a diameter size of 50-100 nm. Changes in deposition time caused variations in roughness, thickness, and surface quality, as shown by AFM results. UV-Vis reflection spectroscopy was also used to investigate the optical properties of thin films.
Thin filis have been prepared from the tin disulphide (SnS2 ), the pure and the doped with copper (SnS2:Cu) with a percentages (1,2,3,4)% by using ahemical spray pyrolysis techniqee on substrate of glass heated up to(603K)and sith thicknesses (0.7±0.02)?m ,after that the films were treated thermally with a low pressure (10-3mb) and at a temperature of (473K) for one hour. The influence of both doping with copper and the thermal treatment on some of the physical characteristics of the prepared films(structural and optical) was studied. The X-ray analysis showed that the prepared films were polycrystalline Hexagonal type. The optical study that included the absorptance and transmitance spectra in the weavelength range (300-900)nm
... Show MoreBaTiO3 thin films have been deposited on Si (111) and glass substrates by using pulsed laser deposition technique. The films were characterized by using X-ray diffraction, atomic force microscope and optical transmission spectra. The films growth on Si after annealing at 873K showed a polycrystalline nature, and exhibited tetragonal structure, while on glass substrate no growth was noticed at that temperature. UV-VIS transmittance measurements showed that the films are highly transparent in the visible wavelength region and near-infrared region for sample annealing on glass substrate. The optical gap of the film were calculated from the curve of absorption coefficient (αhν) 2 vs. hν and was found tobe 3.6 eV at substrate temperature 5
... Show MoreX-ray diffraction pattern reveled the tetragonal crystal system of SnO2 Thin films of SnO2 were prepared on glass substrates using Spray Pyrolysis Technique. The absorption and transmition spectra were recorded in the rang of 300-900nm, the spectral dependences of absorption coefficient were calculated from transmission spectra. The direct and allowed optical energy gap has been evaluated from plots of (αhυ)² vs. (hυ) . The energy gap was found to be 2.4-2.6eV. The optical constant such as extinction coefficient( k ) and absorption coefficient ( α) have been evaluated.
CdS and CdS:Sn thin films were successfully deposited on glass
substrates by spray pyrolysis method. The films were grown at
substrate temperatures 300 C°. The effects of Sn concentration on the
structural and optical properties were studied.
The XRD profiles showed that the films are polycrystalline with
hexagonal structure grown preferentially along the (002) axis. The
optical studies exhibit direct allowed transition. Energy band gap
vary from 3.2 to 2.7 eV.
In this work, the optical properties of Cu2S with different thickness
(1400, 2400, 4400) Ǻ have been prepared by chemical spray pyrolys
is method onto clean glass substrate heated at 283 oC ±2. The effect
of thickness on the optical properties of Cu2S has been studied. It
was found that the optical properties of the electronic transitions on
fundamental absorption edge were direct allowed and the value of the
optical energy gap of Cu2S (Eg) for direct transition decreased from
(2.4-2.1) eV with increasing of the thickness from (1400 - 4400)Ǻ
respectively. Also it was found that the absorption coefficient is
increased with increasing of thicknesses. The optical constants such<
This work describes, selenium (Se) films were deposited on clean glass substrates by dc planar magnetron sputtering technique.The dependence of sputtering deposition rate of Se film deposited on pressure and DC power has been studied. The optimum argon pressure has range (4x10-1 -8x10-2 )mbar. The optical properties such as absorption coefficient (α) was determined using the absorbance and transmission measurement from UnicoUV-2102 PC spectrophotometer, at normal incidence of light in the wavelength range of 200-850 nm. And also we calculated optical constants(refractive index (n), dielectric constant (εi,r), and Extinction coefficient (κ) for selenium films.
In this research, the study effect of irradiation on structural and optical properties of thin film (CdO) by spray pyrolysis method, which deposited on glasses substrates at a thickness of (350±20)nm , The flow rate of solution was 5 ml/min and the substrate temperature was held constant at 400˚C.The investigation of (XRD) indicates that the (CdO) films are polycrystalline and type of cubic. The results of the measuring of each sample from grain size, micro strain, dislocation density and number of crystals the grain size decreasing after irradiation with gamma ray from(27.41, 26.29 ,23.63)nm . The absorbance and transmittance spectra have been recorded in the wavelength range (300-1100) nm in order to study the optical properties.
... Show MoreAntimony (Sb) films are fabricated by depositing (Sb) on glass substrates at room
temperature by the method of vacuum evaporation with thickness (0.25 and 0.51m),
with rate of deposition equal to (2.77Å/sec), the two samples are annealed in a
vacuum for one hour at 473K. The optical constants which are represented by the
refractive index (n), extinction coefficient (k) were determined from transmittance
spectram in the near Infrared(2500-3500 )nm regions. The tests have been shown
that the optical energy gap increases with increasing of annealing temperature for
the two samples.
In the present work, We study the structural and optical properties of (ZnO), which are prepared by thermal evaporation technique, where deposit (Zn) on glass substrates at different thicknesses (150,250,350)nm, deposited on glass substrate at R.T. with rate (5 nm sec-1). And then we make oxidation for (Zn) films at temperature (500) and using the air for one hour, and last annealing samples at temperature (400,500) for one hour. The investigation of (XRD) indicates that the (ZnO) films are polycrystalline type of hexagonal with a preferred orientation along (002) to all samples and analysis reveals that the intensity of this orientation increases with the increase of the thickness and annealing temperature.  
... Show MoreIn this work, the effect of Zn dopant on structural and optical properties of cadmium oxides, CdO, thin film were studied prepared by pulse laser deposition on glass substrate then annealed at 250 ᵒC in air. All films were examined by X-ray diffraction and UV- visible spectrometer. The XRD analysis shows appearance of new phase identical with hexagonal ZnO additional with cubic phase at high Zn content, which effected on the optical properties. The optical energy gap increase from 2.45 eV to 2.70 eV with increasing Zn content from 0 to 40 %.