In the present investigation, (NiO:WO3 ) thin films were deposited at RT onto glass substrates using PLD technique employing focused Nd:YAG laser beam at 600 mJ with a frequency second radiation at 1064 nm (pulse width 9 ns) repetition frequency (6 Hz), for 400 laser pulses incident on the target surface .The structural, morphological and optical properties of the films doped with different concentration of Au content (0.03, 0.05, and 0.07) were examined with X-ray diffractometer(XRD), Atomic Force Microscope(AFM) , UV–Vis spectrophotometer . The results show that the films were amorphous with small peaks appearing when doped with AuNPs . The XRD peaks of the deposited NiO:WO3 were enhanced with increasing the Au content . The crystalline size of the deposited thin films was calculated using Debye Scherer formula and found to decrease from 6.6 nm for undoped NiO:WO3 to 3.4 nm for doped (NiO:WO3) with the increase of Au content from x=0 to x=0.07 at preferred orientation of (200). All the samples have a cubic structure. Also, the results showed that Au content of the films affects the surface morphology. From the results of AFM analysis, it was found that the roughness and average diameter change when adding Au to the structure, with the highest value occurring at Au ratio 0.03 equal to 7.58 and 81.02 nm, respectively. UV–Vis spectrophotometer was used to investigate the optical transmission. It was found that when Au content of films increased, the transmittance of films decreased.
In this work, the effect of Zn dopant on structural and optical properties of cadmium oxides, CdO, thin film were studied prepared by pulse laser deposition on glass substrate then annealed at 250 ᵒC in air. All films were examined by X-ray diffraction and UV- visible spectrometer. The XRD analysis shows appearance of new phase identical with hexagonal ZnO additional with cubic phase at high Zn content, which effected on the optical properties. The optical energy gap increase from 2.45 eV to 2.70 eV with increasing Zn content from 0 to 40 %.
Cadmium sulfide (CdS) thin films with n-type semiconductor characteristics were prepared by flash evaporating method on glass substrates. Some films were annealed at 250 oC for 1hr in air. The thicknesses of the films was estimated to be 0.5µ by the spectrometer measurement. Structural, morphological, electrical, optical and photoconductivity properties of CdS films have been investigated by X-ray diffraction, AFM, the Hall effect, optical transmittance spectra and photoconductivity analysis, respectively. X-ray diffraction (XRD) pattern shows that CdS films are in the stable hexagonal crystalline structure. Using Debye Scherrerś formula, the average grain size for the samples was found to be 26 nm. The transmittance of the
... Show MoreUndoped and Al-doped CdO thin films have been prepared by vacuum thermal evaporation on glass substrate at room temperature for various Al doping ratios (0.5, 1 and 2)wt.% . The films are characterized by XRD and AFM surface morphology properties. XRD analysis showed that CdO:Al films are highly polycrystalline and exhibit cubic crystal structure of lattice constant averaged to 0.4696 nm with (111) preferred orientation. However, intensity of all peaks rapidly decreases which indicates that the crystallinity decreases with the increase of Al dopant. The grain size decreases with Al content (from 60.81 to 48.03 nm). SEM and AFM were applied to study the morphology an
... Show MoreThe structural, optical properties of copper oxide thin films ( CuO) thin films which have been prepared by thermal oxidation with exist air once and oxygen another have been studied. Structural analysis results of Cu thin films demonstrate that the single phase of Cu with high a crystalline structure with a preferred orientation (111). X-ray diffraction results confirm the formation of pure (CuO) phase in both methods of preparation. The optical constant are investigated and calculated such as absorption coefficient, refractive index, extinction coefficient and the dielectric constants for the wavelengths in the range (300-1100) nm.
In this work, nanostructured TiO2 thin films were grown by pulsed laser deposition (PLD) technique on glass substrates. TiO2 thin films then were annealed at 400-600 °C in air for a period of 2 hours. Effect of annealing on the structural and morphological were studied. Many growth parameters have been considered to specify the optimum conditions, namely substrate temperature (300 °C), oxygen pressure (10-2 Torr), laser fluence energy density (0.4 J/cm2), using double frequency Q-switching Nd:YAG laser beam (wavelength 532nm), repetition rate (1-6 Hz) and the pulse duration of 10 ns. The results of the X-ray test show that all nanostructures tetragonal are polycrystalline. These results show that grain size increase fr
... Show MoreThe structural, optical and electrical properties of ZnS films prepared by vacuum
evaporation technique on glass substrate at room temperature and treated at different
annealing temperatures (323, 373, 423)K of thickness (0.5)µm have been studied. The
structure of these films is determined by X-ray diffraction (XRD). The X-ray diffraction
studies show that the structure is polycrystalline with cubic structure, and there are strong
peaks at the direction (111).
The optical properties investigated which include the absorbance and transmittance
spectra, energy band gab, absorption coefficient, and other optical constants. The results
showed that films have direct optical transition. The optical band gab was
Thin films of tin disulphide SnS2 with different thicknesses (2500,4000,5000)A0 have been prepared by chemical spray pyrolises technique on substrate of glass with temperature (603)K . The effect of thickness on the optical properties of SnS2 has been studied.the optical study that includes the absorptance and transmittance spectra in the wavelength range (300900)nm demonstrated that the value of absorption coefficient (α) ) was greater than (104 cm-1) the electronic transitions at the fundamental absorption edge were of the indirect kind whether allowed and forbidden . Absorption edge shift slightly towards higher wave length.The value of energy gaps (Eg) for all the films prepared are decreased with inc
... Show MoreThin films of tin sulfide (SnS) were prepared by thermal evaporation technique on glass substrates, with thickness in the range of 100, 200 and 300nm and their physical properties were studied with appropriate techniques. The phase of the synthesized thin films was confirmed by X-ray diffraction analysis. Further, the crystallite size was calculated by Scherer formula and found to increase from 58 to 79 nm with increase of thickness. The obtained results were discussed in view of testing the suitability of SnS film as an absorber for the fabrication of low-cost and non toxic solar cell. For thickness, t=300nm, the films showed orthorhombic OR phase with a strong (111) preferred orientation. The films deposited with thickness < 200nm deviate
... Show MoreThin films of (CuO)x(ZnO)1-x composite were prepared by pulsed laser deposition technique and x ratio of 0≤ x ≤ 0.8 on clean corning glass substrate at room temperatures (RT) and annealed at 373 and 473K. The X-ray diffraction (XRD) analysis indicated that all prepared films have polycrystalline nature and the phase change from ZnO hexagonal wurtzite to CuO monoclinic structure with increasing x ratio. The deposited films were optically characterized by UV-VIS spectroscopy. The optical measurements showed that (CuO)x(ZnO)1-x films have direct energy gap. The energy band gaps of prepared thin films
In this research the effect of laser energy by using argon gas on the some physical properties of semiconductor film of TiO2, was studied used Q-Switch Nd:YAG laser in different energies (600-1000) mJ with temperature 100 0C for glass substrate under vacuum nearly 10-3 - - , and by AFM test the roughness of films increased when the energy of laser increased too. The values of roughness between (6.77-13) nm, therefore the thicknesses increased to change from (34.88 - 165.48) nm, so the absorption of film increased because of the thickness of the film increased and we can get the optical energy gap between (3.6-3.9) eV.