In this work, has been a studied the effect of thermal treatment using different annealing temperatures (373, 423 and 473) K in vacuum on structural and morphological properties of organic semiconductor Alq3:C60 thin films which are prepared by the spin coating on a glass, silicon and porous silicon. These films have been coated on substrates with speed of 2000 rpm. The structure properties of Tris(8-hydroxyquinoline) aluminum (III) (Alq3) and fullerene (C60) (100:1) and (100:10) blend as-deposited and treated have been studied by X-ray diffraction (XRD) for glass only and morphological properties by Atomic Force Microscope (AFM) for silicon and porous silicon substrates. The results of XRD pattern shows that the structure of (Alq3:C60) as-deposited and annealed thin films are polycrystalline in nature for both mixed weight ratio. The result of AFM measurements show that grain size increase is due to the increases of surface energy at high temperature. Surface roughness increasing and decreased randomly with the temperature can be attributed to the random distributions of the grains and also due to the phase change.
The study effect irradiation on optical properties of film (PVA: CuCL2) prepared by casting method, with thickness of (30±1) μm. And used Cs137 to obtained Gamma ray with energy (662)keV and time irradiation(5,6 and 7) weeks and affectivity (4.3) ci. The spectra absorbance and transmittance register in range (300-1100) nm .
Results show that the optical band gap for (PVA: CuCl2) decreasing after irradiation with gamma ray from (3.2,3.1,3 and 2.7)eV, urbach energy values increase with the increasing time radiation. And the absorption constants (α,k,n,) and the optical conductivity are changing after irradiated with gamma ray .
The influence of annealing on quaternary compound Ag0.9Cu0.1InSe2 (ACIS) thin film is considered a striking semiconductor for second-generation solar cells. The film deposited by thermal evaporation with a thickness of about 700 nm at R.T and vacuum annealing at temperatures (373,473) K for 1 hour. It was deposited in a vacuum of 4.5*10-5 Torr on a glass substrate. From XRD and AFM analysis, it is evident that Ag0.9Cu0.1InSe2 films are polycrystalline in nature, having ideal stoichiometric composition. Structural analysis indicated that annealing the films following the deposition resulted in the increasing polycrystalline phase with the preferred orientation along (112) direction. , increasing crystallite size and average grain size
... Show MoreIron–phthalocyanine (FePc) organic photoconductive detector was fabricated using pulsed laser deposition (PLD) technique to work in ultraviolet (UV) and visible regions. The organic semiconductor material (iron phthalocyanine) was deposited on n-type silicon wafer (Si) substrates at different thicknesses (100, 200 and 300) nm. FePc organic photoconductive detector has been improved by two methods: the first is to manufacture the detector on PSi substrates, and the second is by coating the detector with polyamide–nylon polymer to enhance the photoconductivity of the FePc detector. The current–voltage (I–V) characteristics, responsivity, photocurrent gain, response time and the quantum efficiency of the fabricated photoconduc
... Show MoreTin oxide films (SnO2) of thickness (1 ?m) are prepared on glass substrate by post oxidation of metal films technique. Films were irradiated with Nd:YAG double frequency laser of wavelength (532 nm) pulses of three energies (100, 500, 1000) mJ. The optical absorption, transmission, reflectance, refractive index and optical conductivity of these films are investigated in the UV-Vis region (200-900) nm. It was found that the average transmittance of the films is around (80%) at wavelength (550 nm) and showed high transmission (? 90 %) in the visible and near infrared region. The absorption edge shifts towards higher energies, which is due to the Moss-Burstien effect and it lies at (4 eV). The optical band gap increased with increasing of ene
... Show MoreIn this paper, Zinc oxide were deposited on a glass substrate at room temperature (RT) and two annealing temperatures 350ºC and 500ºC using laser induced plasma technique. ZnO nanofilms of 200nm thickness have been deposited on glass substrate. X-RAY diffraction (XRD), atomic force microscopy and UV-visible spectrophotometer were used to analyze the results. XRD forms of ZnO nanostructure display hexagonal structure with three recognized peaks (100), (002), and (101) orientations at 500ºC annealing temperature. The optical properties of ZnO nanostructure were determined spectra. The energy gap was 3.1 eV at 300 oC and 3.25eV at 500ºC annealing temperature.
The existing investigation explains the consequence of irradiation of violet laser on the optic properties of (CoO2) films. The film was equipped by the utilization of semi-computerized spray pyrolysis technique (SCSPT), it is the first time that this technique is used in the preparation and irradiation using a laser in this technique. From the XRD analysis, the crystalline existence with trigonal crystal system was when the received films were processed by continuous violet laser (405 nm) with power (1W) for different laser irradiation time using different number of times a laser scan (0, 6, 9, 12, 15 and 18 times) with total irradiation time(0,30,45,60,75,90 min
In this research we prepared thin films from pure polymer (polyvinyl alcohol PVA )and doped with CuO with concentration 8% ,and Fe2Cl3 at different concentrations (1,5,8)%.This films were prepared by casting method and placed in Britidish (4cm diameter )with thickness(200±5)μm.Through the investigation of(X-ray )diffraction it is found all that the samples have polycrystalline structure .Also we measurement the optical properties from this films such as absorption ,transmittion spectra ,absorption coefficient ,energy gap ,extinction coefficient ,refraction index ,finesse coefficient ,the dielectric constant with two parts the real and the imaginary and the optical conductivity .
A hybrid nanoparticles light emitting diode (NPs-LED) was fabricated as layers of ITO/TPD:PMMA/ Eu2O3 / Alq3 / Al, by phase segregation method using spin coating technique. The NPs-LED hybrid device emitted light and consisted of three layers in a definite order placed on the transparent conducting oxide as an ITO substrate; the first layer was made of (N, N'-bis (3-methylphenyl) -N, N'-bis (phenyl) benzidine) (TPD) and polymethyl methacrylate (PMMA) polymers combined together. The second layer consisted of Europium (III) oxide (Eu2O3), while the third layer was Alq3, one of the most frequently-used electron transport layers.
The electroluminescence (EL) of N