Hydrothermal technology has many advantages compared to other growth methods such as the availability of their simple equipment,catalyst-free growth,Environmental friendliness, less dangerous environmental, and low costs. Combine spinning method technology with Hydrothermal could improve the structural of ZnO NS by increasing the formation of ZnO NS due to influence of heat annealed treatments on the structure of ZnO NS. ZnONano-Sheets (NS)were prepared to employ hydrothermal process utilizing zinc acetate, that has the chemical composition (Zn (CH3CO2)2.2H2O),as a precursor. After preparing the material, it is deposited in two methods, the first being distillation of the material on the glass (S1),while the second method was using the spinning technique (S2).The spinning method showed better results than the other method.The synthesized ZnO NS were analyzed byscanning electron microscopy (SEM),X-ray diffraction (XRD) analysis and their optical properties have been characterized utilizingUV- absorption spectra.
The Synthesis of yttrium oxide nanoparticles have been achieved via calcination
of yttrium hydroxide produced from the reaction of aqueous solutions of yttrium
nitrate and sodium hydroxide at pH = 13 using hydrothermal and hydrothermal
microwave methods. Effect of heat treatment of the resulted yttrium hydroxide
powder on the morphology and crystallinity of the resulting oxide was studied at
calcination 500, 700 and 1000°C to obtain. The resulted products were
characterized by means of X-ray diffraction (XRD), scanning electron microscope
(SEM), atomic force microscope (AFM), Fourier transform infrared spectrometer
(FTIR) and thermal analyses (TG).
In this work, ZnO nanostructures for powder ZnO were synthesized by Hydrothermal Method. Size and shape of ZnO nanostructureas can be controlled by change ammonia concentration. In the preparation of ZnO nanostructure, zinc nitrate hexahydrate [Zn(NO3)2·6H2O] was used as a precursor. The structure and morphology of ZnO nanostructure have been characterized by scanning electron microscopy (SEM), atomic force microscopy (AFM), X-ray diffraction (XRD). The synthesized ZnO nanostructures have a hexagonal wurtzite structure. Also using Zeta potential and Particle Size Analyzers and size distribution of the ZnO powder
Zinc oxide nanoparticles sample is prepared by the precipitation method. This method involves using zinc nitrate and urea in aqueous solution, then (AgNO3) Solution with different concentrations is added. The obtained precipitated compound is structurally characterized by X-ray diffraction (XRD), Scanning electron microscopy (SEM), Atomic force microscopy (AFM) and Fourier transform infrared spectroscopy (FTIR). The average particle size of nanoparticles is around 28nm in pure, the average particle size reaches 26nm with adding AgNO3 (0.05g in100ml =0.002 M) (0.1g in100ml=0.0058M), AgNO3 (0.2g in 100ml=0.01M) was 25nm. The FTIR result shows the existence of -CO, -CO2, -OH, and -NO2- groups in sample and oxides (ZnO, Ag2O).and used an
... Show MoreChromium oxide nanoparticles were synthesized using cauliflower extract by two methods: simple chemical method and the sol-gel method. These technologies are new, environmentally friendly and cheap. Cauliflower contains plant materials and biomolecules (chromium, phenols, alkalis, vitamins, amino acids, quinones, etc. (that convert chromium chloride hexahydrate (CrCl3.6H2O) into chromium nanoparticles. The plant extracts also act as diluents, stabilizers and anti-caking agents. X-ray diffraction (XRD) analysis showed that the size of the crystals decreased from (36.1 to 57.8) nm using the simple chemical method to (13.31 to 20.68) nm of Cr2O3 using sol-gel.
... Show MoreIn context of this paper we prepare high purity powder ZnO nanostructures by chemical method at low temperature solution and study the effect off annealing at high temperature, ZnO nanoparticles have been successfully synthesized by chemical method at 0Cᵒ solution. In this method, suddenly reaction is occurred between zinc acetate solution and sodium hydroxide solution at 0Cᵒ, annealing temperature of powder product surfactant plays an important role in morphological changes. The nanostructures have been characterized by X-ray diffraction (XRD), Scanning Electron Microscope (SEM), differential scanning calorimetry(DSC) and UV-visible .analysis Effect of annealing temperatures on the morphology , structure and optical properties is di
... Show MoreTin Selenide (SnSe) Nano crystalline thin films of thickness 400±20 nm were deposited on glass substrate by thermal evaporation technique at R.T under a vacuum of ∼ 2 × 10− 5 mbar to study the effect of annealing temperatures (as-deposited, 100, 150 and 200) °C on its structural, surface morphology and optical properties. The films structure was characterized using X-ray diffraction (XRD) which showed that all the films have polycrystalline in nature and orthorhombic structure, with the preferred orientation along the (111) plane. These films was synthesized of very fine crystallites size of (14.8-24.5) nm, the effect of annealing temperatures on the cell parameters, crystallite size and dislocation density were observed.
... Show MoreIn this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
Abstract: In this research, nanofibers have been prepared by using an electrospinning method. Three types of polymer (PVA, VC, PMMA) have been used with different concentration. The applied voltage and the gap length were changed. It was observed that VC is the best polymer than the other types of polymers.
Beryllium Zinc Oxide (BexZn1-xO) ternary nano thin films were deposited using the pulsed laser deposition (PLD) technique under a vacuum condition of 10-3 torr at room temperature on glass substrates with different films thicknesses, (300, 600 and 900 nm). UV-Vis spectra study found the optical band gap for Be0.2Zn0.8O to be (3.42, 3.51 and 3.65 eV) for the (300, 600 and 900nm) film thicknesses, respectively which is larger than the value of zinc oxide ZnO (3.36eV) and smaller than that of beryllium oxide BeO (10.6eV). While the X-ray diffraction (XRD) pattern analysis of ZnO, BeO and Be 0.2 Zn 0.8 O powder and nano-thin films indicated a hexa
... Show MoreIn this paper, ferric oxide nanoparticles) Fe2O3 NPs( were synthesized directly on a quartz substrate in vacuum by pulse laser deposition technique using Nd:YAG laser at different energies (171, 201,363 mJ/pulse). The slides were then heated to 700o C for 1 hour. The structural, optical, morphological, and electrical properties were studied. The optical properties indicated that the prepared thin films have an energy gap ranging from 2.28 to 2.04 eV. The XRD results showed no lattice impurities for other iron oxide phases, confirming that all particles were transformed into the α-Fe2O3 phase during the heating process. The AFM results indicated the dependence of nanoparticles size o