This study was conducted to investigate the antibacterial activity of green synthesized copper oxide nanoparticles (CuO NPs) using Aloe vera. Initially, bacteria were collected from clinical samples of patients having otitis media infection and the isolates were identified at the species level following biochemical tests. Copper oxide nanoparticles were prepared by green synthesis using Aloe vera leaves and characterized using UV- visible spectroscopy at 260 nm peak. The shape and size were determined by using transmission electron microscopy (TEM) and the dimensions of the particles were more precisely determined by using scanning electron microscopy (SEM) and x-ray diffraction (XRD). Different concentrations of nanoparticles (25-50-75-100 µg/ml) were tested for antibacterial activity by using the well diffusion method. The results showed that the shape of CuO NPs was spherical with a size range of 40-10 0nm. The TEM images revealed average of dimensions of 32.34, 35.63, 51.85, 74.71 and 100 nm. The antibacterial activity results of the nanoparticles showed the following growth zone inhibition values for the different bacterial species used: Staphylococci aureus 17.1 mm, Pseudomonas aeruginosa 17 mm, Escherichia coli 16.8mm, Staphylococci epidermidis 16.4mm, Pseudomonas oryzihabitans 15.3mm, Klebsiella pneumonia 13.5mm, Citrobacter freundii 12.7mm, Enterobacter Cloacae 12.2 mm, Proteus vulgaris 8mm, Concerning the virulence factor production, the nanoparticle inhibited the production of biofilm and urease more than other virulence factors, such as gelatinase, hemolysin, protease and lecithinase, by some Gram negative and positive bacterial isolates.
Nd:YAG laser pulses of 9 nanosecond pulse duration and operating wavelength at 1.06 μm, were utilized to drill high thermal conductivity and high reflectivity aluminum and copper foils. The results showed a dependence of drilled holes characteristics on laser power density and the number of laser pulses used. Drilled depth of 74 ϻm was obtained in aluminum at 11.036×108 W/cm2 of laser power density. Due to its higher melting point, copper required higher laser power density and/or larger number of laser pulses to melt, and a maximum depth of 25 μm was reached at 13.46×108 W/cm2 using single laser pulse.
Copper Telluride Thin films of thickness 700nm and 900nm, prepared thin films using thermal evaporation on cleaned Si substrates kept at 300K under the vacuum about (4x10-5 ) mbar. The XRD analysis and (AFM) measurements use to study structure properties. The sensitivity (S) of the fabricated sensors to NO2 and H2 was measured at room temperature. The experimental relationship between S and thickness of the sensitive film was investigated, and higher S values were recorded for thicker sensors. Results showed that the best sensitivity was attributed to the Cu2Te film of 900 nm thickness at the H2 gas.
Objective: The aim of this study to detect the correlation between trace elements such as zinc, copper and
spermatogenesis, sperm viability and motility.
Methodology: Serum and semen samples were collected from one hundred twenty patients with age ranged (20-
50 years) attending the high institute for Embryo Research and Infertility Treatment/ Baghdad University, in
addition to thirty fertile males their age comparable to that of patients. The period of this study was from June
2004 until the end of October 2004.
Results: The result of routine seminal fluid analysis of all infertile males was divided according to WHO, (1999) limit
into four groups: Asthenospermia(A), Asthenoteratospermia(AT), Oligoasthenoteratospermi
Zinc oxide (ZnO) nanoparticles were synthesized using a modified hydrothermal approach at different reaction temperatures and growth times. Moreover, a thorough morphological, structural and optical investigation was demonstrated using scanning electron microscopy (SEM), x-ray diffraction (XRD), ultra-violate visible light spectroscopy (UV-Vis.), and photoluminescence (PL) techniques. Notably, SEM analysis revealed the occurrence of nanorods-shaped surface morphology with a wide range of length and diameter. Meanwhile, a hexagonal crystal structure of the ZnO nanoparticles was perceived using XRD analysis and crystallite size ranging from 14.7 to 23.8 nm at 7 and 8 ℎ𝑟𝑠., respectively. The prepared ZnO samples showed good abso
... Show MoreLead-free ferroelectric nano ceramics of BaZrxTi1-xO3 (x=0.1, 0.2 and 0.3) were prepared by means of microwave assisted chemical route. The structural, dielectric and electrical properties were examined. The crystalline structure of the specimens was studied by X-ray diffraction patterns. All the samples showed pure single phase of perovskite structure with space group of I4/mcm. X-ray diffraction data illustrated that there is no secondary phases exist. Structural and electrical properties of barium titanate ceramics are influenced significantly by small additions of Zr. The electrical conductivity showed higher values at x=0.2 and decreased at higher Zr content. The Hall charge mobility is found
... Show MoreThis study includes the preparation of the ferrite nano ferrite CuxAl0.3-XNi0.7Fe2O4 (where: x = 0, 0.05, 0.1, 0.15, 0.2, 0.25, 0.3) M using the auto combustion method (sol-gel), and citric acid was used as fuel for auto combustion. The ferrite samples were checked by X-ray diffraction (XRD), Field Emission Scanning Electron Microscopes (FE-SEM), and energy dispersive X-ray analyzer (EDX). They showed that the prepared compound has a face-centered cubic structure (FCC). The lattice constant increases with an increase in the percentage of doping of the copper ions, and a decrease for the aluminum ion and that the compound is porous and its grains are spherical, and there are no other
... Show MoreZnO nanostructures were synthesized by hydrothermal method at different temperatures and growth times. The effect of increasing the temperature on structural and optical properties of ZnO were analyzed and discussed. The prepared ZnO nanostructures were characterized by X-ray diffraction (XRD), UV–Vis. absorption spectroscopy (UV–Vis.), Photoluminescence (PL), and scanning electron microscopy (SEM). In this work, hexagonal crystal structure prepared ZnO nanostructures was observed using X-ray diffraction (XRD) and the average crystallite size equal 14.7 and 23.8 nm for samples synthesized at growth time 7 and 8 hours respectively. A nanotubes-shaped surface morphology was found using scanning electron microscopy (SEM). The optic
... Show MoreThis paper presents the ability to use cheap adsorbent (corn leaf) for the removal of Malachite Green (MG) dye from its aqueous solution. A batch mode was used to study several factors, dye concentration (50-150) ppm, adsorbent dosage (0.5-2.5) g/L, contact time (1-4) day, pH (2-10), and temperature (30-60) The results indicated that the removal efficiency increases with the increase of adsorbent dosage and contact time, while inversely proportional to the increase in pH and temperature. An SEM device characterized the adsorbent corn leaves. The adsorption's resulting data were in agreement with Freundlich isotherm according to the regression analysis, and the kinetics data followed pseudo-first-or
... Show MoreHybrid architecture of ZnO nanorods/graphene oxide ZnO-NRs@GO synthesized by electrostatic self-assembly methods. The morphological, optical and luminescence characteristics of ZnO-NRs@GO and ZnO-NRs thin films have been described by FESEM, TEM, HRTEM, and AFM, which refers to graphene oxide have been coated ZnO-NRs with five layers. Here we synthesis ZnO-NRs@GO by simple, cheap and environmentally friendly method, which made it favorable for huge -scale preparation in many applications such as photocatalyst. ZnO-NRs@GO was applied as a photocatalyst Rodamin 6 G (R6G) dye from water using 532 nm diode laser-induced photocatalytic process. Overall degradation of R6G/ ZnO-NRs@GO was achieved after 90 minutes of laser irradiation while it ne