Aluminum doped zinc oxide nanoparticles (AZO) with different doping concentrations were prepared by Nd-YAG laser ablation of target in deionized water. The characterization of these nanoparticles was performed using Fourier transform infrared (FTIR) spectroscopy, scanning electron microscopy (SEM) and photoluminance spectroscopy (PL). FTIR spectra confirmed the formation of vibrational bonds for ZnO NPs and AZO NPs. SEM images illustrated that the size and shape of the NPs changed with changing the number of laser pulses. Photoluminescence peaks exhibited two emission peaks, one at the UV region and the second in the visible region, which were modified as the number of laser pulses and doping concentration were changed.
The current work is characterized by simplicity, accuracy and high sensitivity Dispersive liquid - Liquid Micro Extraction (DLLME). The method was developed to determine Telmesartan (TEL) and Irbesartan (IRB) in the standard and pharmaceutical composition. Telmesartan and Irbesartan are separated prior to treatment with Eriochrom black T as a reagent and formation ion pair reaction dye. The analytical results of DLLME method for linearity range (0.2- 6.0) mg /L for both drugs, molar absorptivity were (1.67 × 105- 5.6 × 105) L/ mole. cm, limit of detection were (0.0242and0.0238), Limit of quantification were (0.0821and0.0711), the Distribution coefficient were
... Show MoreGraphene-carbon nitride can be synthesized from thiourea in a single step at a temperature of four hours at a rate of 2.3 ℃/min. Graphene-carbon nitride was characterized by Fourier-transform infrared spectroscopy (FTIR), energy dispersive X-ray analysis (EDX), scanning electron microscopy, and spectrophotometry (UV-VIS). Graphene-carbon nitride was found to consist of triazine and heptazine structures, carbon, and nitrogen. The weight percentage of carbon and the atomic percentage of carbon are 40.08%, and the weight percentage of nitrogen and the atomic percentage of nitrogen are 40.08%. Therefore, the ratio and the dimensions of the graphene-carbon nitride were characterized by scanning electron microscopy, and it was found that the
... Show MoreThis work aims to fabricate two types of plasmonic nanostructures by electrical exploding wire (EEW) technique and study the effects of the different morphologies of these nanostructures on the absorption spectra and Surface-Enhanced Raman Scattering (SERS) activities, using Rhodamine 6G as a probe molecule. The structural properties of these nanostructures were examined using X-Ray diffraction (XRD). The morphological properties were examined using field emission scanning electron microscopy (FESEM) and scanning transmission electron microscopy (STEM). The absorption spectra of the mixed R6G laser dye (concentration 1×10-6 M) with prepared nanostructures were examined by double beam UV-Vis Spectrophotometer. The Raman spe
... Show MoreThe size and the concentration of the gold nanoparticles (GNPs)
synthesized in double distilled deionized water (DDDW) have been
found to be affected by the laser energy and the number of pulses.
The absorption spectra of the nanoparticles DDDW, and the
surface plasmon resonance (SPR) peaks were measured, and found to
be located between (509 and 524)nm using the UV- Vis
spectrophotometer. SPR calculations, images of transmission
electron microscope, and dynamic light scattering (DLS) method
were used to determine the size of GNPs, which found to be ranged
between (3.5 and 27) nm. The concentrations of GNPs in colloidal
solutions found to be ranged between (37 and 142) ppm, and
measured by atomic absorptio
In this work, calcium ions were determined by the addition to the allyl chloride monomer resulting from bulk polymerization formation. To acquire the highest adsorption capacity, molar ratios of the template, monomer, and cross-linking agent, as well as solvents and multiple monomers were investigated. Scanning Electron Microscopy (SEM) and Fourier Transform Infrared Spectroscopy (FTIR) were used to analyze the calcium ion polymer. The elution of calcium had a small effect on the surfaces of the three-dimensional network structure. Calcium (II) ions were successfully eluted using a mixture of methanol and acetic acid. The calcium adsorption capacities were 3.8145 and 9.01773 mol/g (Qmax), respectively. A Langmuir isot
... Show MoreBromelain is a proteolytic enzyme rich in cysteine proteases, extracted from the stem and fruit of pineapple (Ananas comosus). There are several therapeutic applications of the bromelain enzyme, where it has anti-inflammatory, anti-cancer, and antimicrobial activity, reduces joint pain, and accelerates wound healing. In the current study, bromelain enzyme was loaded on silver nanoparticles (Br-AgNPs) prepared using the citrate-reduction Turkevich method. Different characterization analyses were performed, including UV-Vis spectrophotometers, FTIR, SEM, and XRD analyses. Moreover, the antioxidant activity of prepared Br-AgNPs was evaluated by DPPH assay. The results of UV-Vis showed a peak at 434 nm, which referred to the AgNPs f
... Show MoreLarge quantities of contaminated carwash wastewater are produced per day from carwash places. Extensively it contains large quantities of chemicals from detergents, oil, grease, heavy metals, suspended solids, types of hydrocarbons, and biological contents. A novel electrocoagulation treatment by foil electrodes was conducted to remove COD, turbidity, Total Dissolved Solids (TDS) from contaminated carwash wastewater and decrease its Electrical Conductivity (EC). A thin layer of aluminum foil is used as an electrode in this treatment process. The effects of different voltage and treatment times were studied. The best result was found at a voltage of 30 volts and treatment time 90 minute where the removal efficiency of COD
... Show MoreIn this study we using zirconium sulfate, Punica granatum plant extract, and an alkaline medium, to created ZrO2 nanoparticles. They were then characterized using a variety of techniques, including FT-IR, UV-visible, atomic force microscopy, X-ray diffraction, transmission electron microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The Debye-Scherrer equation was used to calculate the crystal size in X-ray diffraction and found to be 27.82 nm. The particle size of ZrO2 nanoparticles was determined using atomic force microscopy, scanning electron microscopes, and transmission electron microscopy. Utilizing ZrO2 NPs, the metal ions M (II) = Co, Ni, and Cu were successfully a
... Show MoreManganese sulfate and Punica granatum plant extract were used to create MnO2 nanoparticles, which were then characterized using techniques like Fourier transform infrared spectroscopy, ultraviolet-visible spectroscopy, atomic force microscopy, X-ray diffraction, transmission electron microscopy, scanning electron microscopy, and energy-dispersive X-ray spectroscopy. The crystal's size was calculated to be 30.94nm by employing the Debye Scherrer equation in X-ray diffraction. MnO2 NPs were shown to be effective in adsorbing M(II) = Co, Ni, and Cu ions, proving that all three metal ions may be removed from water in one go. Ni(II) has a higher adsorption rate throughout the board. Co, Ni, and Cu ion removal efficiencies were 32.79%, 75
... Show More