In this paper, the productions of gallium oxide (Ga2O3) nanoparticles were achieved via using the Nd: YAG laser deposition method with a fundamental wavelength (1064 nm). These nanoparticles were characterized by using different methods such as X-ray diffractometer (XRD), atomic force microscopy (AFM) and Ultraviolet–visible (UV–vis) spectroscopy. To examine the effects of laser energy on the properties of nanoparticles, the experimental results and theoretical considerations were prepared by the effective method of pulse laser deposition. The synthesis of Ga2O3NPs) was achieved with different ranges of energies (500 to 900 mJ). Average crystallite sizes of the synthesized nanoparticles were found to be in the range of 15-37 nm. On the other hand, the AFM images showed that the size is ranging between 60 and 85 nm. Optical parameters of the samples showed a strong dependence on average crystallite size.
Nanoparticles (NPs) have unique capabilities that make them an eye-opener opportunity for the upstream oil industry. Their nano-size allows them to flow within reservoir rocks without the fear of retention between micro-sized pores. Incorporating NPs with drilling and completion fluids has proved to be an effective additive that improves various properties such as mud rheology, filtration, thermal conductivity, and wellbore stability. However, the biodegradability of drilling fluid chemicals is becoming a global issue as the discharged wetted cuttings raise toxicity concerns and environmental hazards. Therefore, it is urged to utilize chemicals that tend to break down and susceptible to biodegradation. This research presents the pra
... Show MoreMagnetized iron oxide nanoparticles (NPs) were prepared using Eucalyptus leaf extract and then coated with CTAB (Cetrimonium bromide) to increase efficiency. The prepared and modified (NPs) were characterized using AFM, FTIR, and X-ray techniques. The adsorption of the dye reactive blue RB 238 on coated (NPs) was investigated. The effect of various experimental factors, such as the initial concentration of the dye, the amount of adsorbent, pH and temperature on the removal of RB238 was studied. The best conditions for dye removal were found to be 298 K in an acidic medium of pH = 3 and an appropriate dose of the adsorbent of 0.15 g per 25 mg/L to achieve the best color removal of 90% within 60 minutes. The pseudo-second-order re
... Show MoreBackground: Surface treatment of machined dental zirconia for enhancement of the adhesion to resin cement, using Er,Cr:YSGG Laser. Materials and Methods: Total number of 42 zirconia disc specimens (9 mm diameter, and 2 mm height) was sintered according to the manufacturer instruction. They are divided into six groups, each group of seven samples. Laser groups (Experiment parameters) were depend on laser total irradiation time, pulse duration, and power. Group (A): 20 sec., 60 µs pulse duration. Group (B): 30 sec., 60 µs pulse duration. Group (C): 40 sec., 60 µs pulse duration. Group (D): 20 sec., 700 µs pulse duration. Group (E): 30 sec., 700 µs pulse duration, with different powers used (1, 1
... Show MoreA simple, inexpensive, and home–built electrostatic spray deposition (ESD) system with stable cone-jet mode was used to obtain nickel oxide (NiO) thin films on glass substrates kept at temperature of 400°C. The primary precursor solution of 0.1 M concentration hydrated nickel chloride dissolved in isopropyl alcohol. The structural, optical and electrical parameters were studied. The optical absorbance spectra for the studied samples showed its maximum around 280 nm. On the other hand, thickness interferometry measurements on the tested samples showed that film thickness was around 400 nm. The optical energy gap of the prepared NiO samples was determined to be 3.75 eV and the maximum value of refractive index was determined to be 2.1 a
... Show MoreOil well drilling fluid rheology, lubricity, swelling, and fluid loss control are all critical factors to take into account before beginning the hole's construction. Drilling fluids can be made smoother, more cost-effective, and more efficient by investigating and evaluating the effects of various nanoparticles including aluminum oxide (Al2O3) and iron oxide (Fe2O3) on their performance. A drilling fluid's performance can be assessed by comparing its baseline characteristics to those of nanoparticle (NPs) enhanced fluids. It was found that the drilling mud contained NPs in concentrations of 0,0.25, 0. 5, 0.75 and 1 g. According to the results, when drilling fluid was used without NPs, the coeff
... Show MoreThe Synthesis of yttrium oxide nanoparticles have been achieved via calcination
of yttrium hydroxide produced from the reaction of aqueous solutions of yttrium
nitrate and sodium hydroxide at pH = 13 using hydrothermal and hydrothermal
microwave methods. Effect of heat treatment of the resulted yttrium hydroxide
powder on the morphology and crystallinity of the resulting oxide was studied at
calcination 500, 700 and 1000°C to obtain. The resulted products were
characterized by means of X-ray diffraction (XRD), scanning electron microscope
(SEM), atomic force microscope (AFM), Fourier transform infrared spectrometer
(FTIR) and thermal analyses (TG).
The Catharanthus roseus plant was extracted and converted to nanoparticles in this work. The Soxhlet method extracted alkaloid compounds from the plant Catharanthus roseus and converted them to the nanoscale. Chitosan polymer was used as a linking material and converted to Chitosan nanoparticles using Sodium TriPolyPhosphate (STPP). The extracted alkaloids were linked with Chitosan nanoparticles CSNPs by maleic anhydride to get the final product (CSNPs- Linker- alkaloids). The synthesized (CSNPs- Linker- alkaloids) was characterized using SEM spectroscopy UV–Vis., Zeta Potential, and HPLC High-Performance Liquid Chromatography. Scanning electron microscope (SEM) analysis shows that the Chitosan nanoparticles (CSNPs) have small dim
... Show MoreIn this research, the results of x-ray diffraction method were used to determine the uniform stress deformation and microstructure parameters of CuO nanoparticles to determine the lattice strain obtained and crystallite size and then to compare the results obtained by two model Halder Wagner and Size Strain Plot with the results of these methods of the same powder using equations during which the calculation of the size of the crystallite size and lattice strain, It was found that the results obtained the values of the crystallite size (19.81nm) and the lattice strain (0.004065) of the Halder-wagner model respectively and for the ssp method were the results of the crystallite size (17.20nm) and lattice strain (0.000305) respectively. The sa
... Show MoreIn this study, a double frequency Q-switching Nd:YAG laser beam (1064 nm and λ= 532 nm, repetition rate 6 Hz and the pulse duration 10ns) have been used, to deposit TiO2 pure and nanocomposites thin films with noble metal (Ag) at various concentration ratios of (0, 10, 20, 30, 40 and 50 wt.%) on glass and p-Si wafer (111) substrates using Pulse Laser Deposition (PLD) technique. Many growth parameters have been considered to specify the optimum condition, namely substrate temperature (300˚C), oxygen pressure (2.8×10-4 mbar), laser energy (700) mJ and the number of laser shots was 400 pulses with thickness of about 170 nm. The surface morphology of the thin films has been studied by using atomic force microscopes (AFM). The Root Mean Sq
... Show More