Fabrication of a Chemical Sensor Based on Surface Plasmon Resonance via Plastic Optical Fiber
...Show More Authors

In this work, a chemical optical fiber sensor based on Surface Plasmon Resonance (SPR) was designed and implemented using plastic optical fiber. The sensor is used for estimating refractive indices and concentrations of various chemical materials (methanol, distilled water, ethanol, kerosene) as well as for evaluating the performance parameters such as sensitivity, signal to noise ratio, resolution and the figure of merit of the fabricated sensor. It was found that the value of the sensitivity of the optical fiber-based SPR sensor, with 40 nm thick and 10 mm long Au metal film of exposed sensing region, was 3μm/RIU, while the SNR was 0.24, the figure of merit was 20, and the resolution was 0.00066. The sort of optical fiber utilized in this work is plastic optical fiber with a core diameter of 980 μm, a fluorinated polymer cladding of 20μm and a numerical aperture of 0.51.

Scopus Crossref
View Publication Preview PDF
Quick Preview PDF
Publication Date
Sun Jan 01 2017
Journal Name
International Journal Of Latest Trends In Engineering And Technology
Study the effect of number of nozzle on optical and structural properties of sno2 films grown by (apcvd)
...Show More Authors

View Publication Preview PDF
Crossref
Publication Date
Fri Jan 11 2019
Journal Name
Iraqi Journal Of Physics
Effect of thickness on the optical properties of ZnO thin films prepared by pulsed laser deposition technique (PLD)
...Show More Authors

Zinc Oxide (ZnO) thin films of different thickness were prepared
on ultrasonically cleaned corning glass substrate, by pulsed laser
deposition technique (PLD) at room temperature. Since most
application of ZnO thin film are certainly related to its optical
properties, so the optical properties of ZnO thin film in the
wavelength range (300-1100) nm were studied, it was observed that
all ZnO films have high transmittance (˃ 80 %) in the wavelength
region (400-1100) nm and it increase as the film thickness increase,
using the optical transmittance to calculate optical energy gap (Eg
opt)
show that (Eg
opt) of a direct allowed transition and its value nearly
constant (~ 3.2 eV) for all film thickness (150

... Show More
View Publication Preview PDF
Crossref (3)
Crossref
Publication Date
Sun May 22 2022
Journal Name
International Journal Of Early Childhood Special Education
A training program based on integrating futuristic thinking skills with classroom interaction patterns and its effect on the academic self- efficacy of mathematics teachers
...Show More Authors

The research aims to identify the effect of the training program that is based on integrating futuristic thinking skills with classroom interaction patterns on mathematics teachers in order to provide their students with creative solution skills. The research sample consisted of 31teachers (15 teachers for the experimental group and 16 for the control groups). The researcher developed a measure for the academic self-efficacy consisting of (39) items. Its validity, reliability, coefficient of difficulty and discriminatory power were estimated. To analyze the findings, the researcher adopted the Mann-Whitney (U) test and the effect size, and the findings were as follows: There is a statistically significant difference at the significance leve

... Show More
Publication Date
Sun Jan 12 2020
Journal Name
Technologies And Materials For Renewable Energy, Environment And Sustainability
The effect of doping process on the structural and optical properties of Ag2Se thin films.
...Show More Authors

Preview PDF
Publication Date
Tue Jul 14 2015
Journal Name
Ibn Al-haitham J. For Pure & Appl. Sci.
Effect of Annealing Temperature and Thickness on the Structural and Optical Properties of CdSeThin Films
...Show More Authors

CdSe alloy has been prepared successfully from its high purity elements. Thin films of this alloy with different thicknesses (300,700)nm have been grown on glass substrates at room temperature under very low pressure (10-5)Torr with rate of deposition (1.7)nm/sec by thermal evaporation technique, after that these thin films have been heat treated under low pressure (10-2)Torr at (473,673)K for one hour. X-ray patterns showed that both CdSe alloy and thin films are polycrystalline and have the hexagonal structure with preferential orientation in the [100] and [002] direction respectively. The optical measurements indicated that CdSe thin films have allowed direct optical energy band gap, and it increases from (1.77- 1.84) eV and from

... Show More
Publication Date
Mon Jun 10 2013
Journal Name
International Journal Of Application Or Innovation In Engineering & Management (ijaiem)
The Effect of Annealing Temperature on the Optical Properties of CdS and CdS:Al Thin Films
...Show More Authors

Cadmium sulfide and Aluminum doped CdS thin films were prepared by thermal evaporation technique in vacuum on a heated glass substrates at 373K. A comparison between the optical properties of the pure and doped films was made through measuring and analyzing the transmittance curves, and the effect of the annealing temperature on these properties were estimated. All the films were found to exhibit high transmittance in the visible/ near infrared region from 500nm to 1100nm.The optical band gap energy was found to be in the range 2.68-2.60 eV and 2.65-2.44 eV for CdS and CdS:Al respectively , with changing the annealing temperature from room temperature to 423K.Optical constants such as refractive index, extinction coefficient, and complex di

... Show More
Publication Date
Mon Sep 20 2021
Journal Name
Key Engineering Materials
The Effect of Quantum Confinement on Optical Properties of CdSe Quantum Dots at Room Temperature
...Show More Authors

CdSe quantum dots possess a tuning energy gap which can control gap values according to the size of the quantum dots, this is made the material able to absorb the wavelengths within visible light. A simple model is provided for the absorption coefficient, optical properties, and optical constants for CdSe quantum dots from the size 10nm to 1nm with the range of visible region between (300-730) nm at room temperature. It turns out that there is an absorption threshold for each wavelength, CdSe quantum dots begin to absorb the visible spectrum of 1.4 nm at room temperature for a wavelength of 300 nm. It has been noted that; when the wavelength is increased, the absorption threshold also increases. This applies to the optical propertie

... Show More
View Publication
Crossref
Publication Date
Sun Jun 01 2008
Journal Name
Baghdad Science Journal
Study the Effect of thickness on the Optical Properties Performance of active polymeric laser media
...Show More Authors

The paper include study the effect thickness of the polymeric sample which is manufactured by thermo press way. The sample was used as an active tunable R6G laser media. The remarks show that, when the thickness of the samples is increased, with the same concentration, the spectrum will shift towards the short wavelength, & the quantum fluorescence yield will increased. The best result we obtained for the quantum fluorescence yield is (0.68) at the sample, with thickness (0.304mm) in Ethanol solvent, while when we used the Pure Water as a solvent, we found that the best quantum fluorescence yield is (0.63) at (0.18mm) thickness of the sample.

View Publication Preview PDF
Crossref
Publication Date
Sat Jan 01 2011
Journal Name
Iraqi Journal Of Physics
Study of annealing effect on some Optical Properties of CuIn(SexTe1-x)2 Thin Films
...Show More Authors

The optical properties for the components CuIn(SexTe1-x)2 thin films with both values of selenium content (x) [0.4 and 0.6] are studied. The films have been prepared by the vacuum thermal evaporation method with thickness of (250±5nm) on glass substrates. From the transmittance and absorbance spectra within the range of wavelength (400-900)nm, we determined the forbidden optical energy gap (Egopt) and the constant (B). From the studyingthe relation between absorption coefficient (α) photon energy, we determined the tails width inside the energy gap.
The results showed that the optical transition is direct; we also found that the optical energy gap increases with annealing temperature and selenium content (x). However, the width of l

... Show More
View Publication Preview PDF
Publication Date
Mon Feb 18 2019
Journal Name
Iraqi Journal Of Physics
Effect of annealed temperature on some structural, optical and mechanical properties of selenium thin film
...Show More Authors

In this paper a thin films of selenium was prepare on substrates of n-Si by evaporation in a vacuum technique with thickness about 0.5μm. And then an annealing process was done on samples at two temperature (100 and 200) C ° in a vacuum furnace (10-3 torr).
Some structural, optical and mechanical properties of prepared thin films were measured. Results showed that the prepared film was the crystallization, optical transmittance and micro hardness of the prepared thin films increased significantly after annealing.