The objective of this work is to study the influence of α-amylase enzymatic solution immersion, soil burial and water immersion on the biodegradability behavior of polyvinyl alcohol (PVA) /Corn Starch (CS) blend films Polyvinyl alcohol (PVA) /Corn Starch (CS) blend films were prepared by solution casting method with different weight percentages of PVA(0%,10%,30%,50%,70% and 90%) . The biodegradability of the films has been investigated by determination the weight loss of the tested films. It was noticed that the films containing corn starch were highly biodegraded under above influences. The weight loss of the tested films decreased with increasing PVA content and increased with immersion time in enzymatic solution and water and soil burial time
In this study, gamma-ray spectrometry with an HPGe detector was used to measure the specific activity concentrations of 226Ra, 232Th, and 40K in soil samples collected from IT1 oil reservoirs in Kirkuk city, northeast Iraq. The “spectral line Gp” gamma analysis software package was used to analyze the spectral data. 226Ra specific activity varies from 9 0.34 Bq.kg-1 to 17 0.47 Bq.kg-1. 232Th specific activity varies from 6.2 0.08 Bq.kg-1 to 18 0.2 Bq.kg-1. 40K specific activity varies from 25 0.19 Bq.kg-1 to 118 0.41 Bq.kg-1. The radiological hazard due to the radiation emitted from natural r
... Show MoreCuAlTe2 thin films were evaporation on glass substrates using the technique of thermal evaporation at different range of thickness (200,300,400and500) ±2nm. The structures of these films were investigated by X-ray diffraction method; showing that films possess a good crystalline in tetragonal structure. AFM showed that the grain size increased from (70.55-99.40) nm and the roughness increased from (2.08-3.65) nm by increasing the thickness from (200-500) nm. The optical properties measurements, such as absorbance, transmtance, reflectance, and optical constant as a function of wavelength showed that the direct energy gap decreased from (2.4-2.34) eV by the gain of the thickness.
In this work the effect of annealing temperature on the structure and the electrical properties of Bi thin films was studied, the Bi films were deposited on glass substrates at room temperature by thermal evaporation technique with thickness (0.4 µm) and rate of deposition equal to 6.66Å/sec, all samples are annealed in a vacuum for one hour. The X-ray diffraction analysis shows that the prepared samples are polycrystalline and it exhibits hexagonal structure. The electrical properties of these films were studied with different annealing temperatures, the d.c conductivity for films decreases from 16.42 ? 10-2 at 343K to 10.11?10-2 (?.cm)-1 at 363K. The electrical activation energies Ea1 and Ea2 increase from 0.031 to 0.049eV and
... Show MoreIn this study, tin oxide (SnO2) and mixed with cadmium oxide (CdO) with concentration ratio of (5, 10, 15, 20)% films were deposited by spray pyrolysis technique onto glass substrates at 300ºC temperature. The structure of the SnO2:CdO mixed films have polycrystalline structure with (110) and (101) preferential orientations. Atomic force microscopy (AFM) show the films are displayed granular structure. It was found that the grain size increases with increasing of mixed concentration ratio. The transmittance in visible and NIR region was estimated for SnO2:CdO mixed films. Direct optical band gap was estimated for SnO2 and SnO2 mixed CdO and show a decrease in the energy gap with increasing mixing ratio. From Hall measurement, it was fou
... Show MoreIn the present article, Nano crystalline SnS and SnS:3% Bi thin films were fabricated using thermal
evaporation with 400±20 nm thickness at room temperature at a rate deposition rate of 0.5 ±0.01nm
/sec then annealing for one hour at 573 K for photovoltaic application. The prepared samples were
characterized in order to investigate the structural, electrical, morphological, and optical properties
using diverse techniques. XRD and SEM were recorded to investigate the effect of doping and
annealing on structural and morphological possessions, respectively. XRD showed an SnS phase
with polycrystalline and appeared to form an orthorhombic structure, with the distinguish trend
along the (111) grade,
SnO2 thin films of different two thicknesses were prepared an glass substrate by DC magnetron sputtering. The crystal structure and orientation of the films were investigated by XRD patterns. All the deposited films are polycrystalline. The grain size was calculated as 25.35, 28.8 nm. Morphological and compositions of the films were performed by SEM and EDX analyses respectively. The films appeared compact and rougher surface in nature. The allowed direct band gap was evaluated as 3.85 eV, and other optical constants such as refractive index, extinction coefficient, real and imaginary parts of dielectric constants were determined from transmittance spectrum in the wavelength range (300-900) nm and also analyzed.
A simple, inexpensive, and home–built electrostatic spray deposition (ESD) system with stable cone-jet mode was used to obtain nickel oxide (NiO) thin films on glass substrates kept at temperature of 400°C. The primary precursor solution of 0.1 M concentration hydrated nickel chloride dissolved in isopropyl alcohol. The structural, optical and electrical parameters were studied. The optical absorbance spectra for the studied samples showed its maximum around 280 nm. On the other hand, thickness interferometry measurements on the tested samples showed that film thickness was around 400 nm. The optical energy gap of the prepared NiO samples was determined to be 3.75 eV and the maximum value of refractive index was determined to be 2.1 a
... Show MoreCadmium sulfide (CdS) nanocrystalline thin films are prepared onto ITO-glass and Si(111) substrates by chemical bath deposition method. The scanning electron microscope images showed that the CdS thin film onto Si substrate is more homogenous without vacancies. The XRD patterns of the CdS nanocrystalline thin film confirm that they have polycrystalline with cubic phase. Room temperature photoluminescence (PL) spectrum of the CdS nanocrystalline thin films shows emission band located at 502nm for CdS/Si sample while the CdS/ITO-glass thin films shows a broad emission band peaked at 505nm. The Raman spectra of CdS nanocrystalline thin films prepared onto Si and ITO-glass substrates contain two main peaks which are corresponding to the firs
... Show More(Sb2S3)1-xSnx thin films with different concentrations (0, 0.05 and
0.15) and thicknesses (300,500 and 700nm) have been deposited by
single source vacuum thermal evaporation onto glass substrates at
ambient temperature to study the effect of tin content, thickness and
on its structural morphology, and electrical properties. AFM study
revealed that microstructure parameters such as crystallite size, and
roughness found to depend upon deposition conditions. The DC
conductivity of the vacuum evaporated (Sb2S3)1-x Snx thin films was
measured in the temperature range (293-473)K and was found to
increase on order of magnitude with